| 二元相图相界的计算方法 |
| 王明贤;雷琼芝 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| A CALCULATIONAL METHOD FOR DETERMINING PHASE BOUNDARY IN BINARY SYSTEM PHASE DIAGRAM |
| Wang Mingxian; Lei Qiongzhi (Institute of Metal Research; Academia Sinica; Shenyang) |
引用本文:
王明贤;雷琼芝. 二元相图相界的计算方法[J]. 金属学报, 1982, 18(5): 627-630.
,
.
A CALCULATIONAL METHOD FOR DETERMINING PHASE BOUNDARY IN BINARY SYSTEM PHASE DIAGRAM[J]. Acta Metall Sin, 1982, 18(5): 627-630.
1 Kubaschewski, O.; Chart, T. G., J. Inst. Met., 93(1964-1965) , 329. 2 Kubaschewski, O,; Alcock, C. B., Metallurgical Thermochemistry, 5th ed., Oxford, Pergamon Press, 1979, p. 234. 3 Kaufman, L.; Bernstein, M., Computer Calculation of Phase Diagrams, Academic Press, New York, 1970, p. 265. 4 长谷川光弘,西沢泰二,日本金属学会会报,11(1972) ,12,879. 5 Gaye, H.; Lupis, C. H. P., Metall. Trans., 6A(1975) , 1049, 6 Ansara, I., Int. Met. Rev., 24(1979) , 23. 7 Balakrishna, S. S.; Mallik, A. K., Applications of Phase Diagrams in Metallurgy and Ceramics, Ed. G. C. Carter, NBS, U. S., 1978, p. 1210. 8 Hultgren, R.; Desai, P. D., Selected Values of the Thermodynamic Properties of Binary Alloys, ASM, Metals, Park, Ohio, 1973, p. 1278. 9 Hultgren, R.; Desai, P. D., ibid., p. 696. 10 Hultgren, R.; Desai, P. D., ibid., p. 27. 11 Hultgren, R.; Desai, P. D., ibid., p. 260. 12 Hultgren, R.; Desai, P. D., ibid., p. 46. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|