| CaF_2-CaO-La_2O_3三元炉渣粘度的测定及物相特征的研究 |
| 彭(忄育)强;洪彦若;朱元凯 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| DETERMINATION OF VISCOSITY OF CaF_2-CaO-La_2O_3 TERNARY SLAGS AND INVESTIGATION OF PHASE CHARACTERISTICS |
| Peng Yujiang Hong Yanruo Zhu Yuankai (Beijing University of Iron and Steel Technology) (Manuscript received 13 March; 1981; revised manuscript 5 October; 1981) |
引用本文:
彭(忄育)强;洪彦若;朱元凯. CaF_2-CaO-La_2O_3三元炉渣粘度的测定及物相特征的研究[J]. 金属学报, 1982, 18(4): 456-462.
,
,
.
DETERMINATION OF VISCOSITY OF CaF_2-CaO-La_2O_3 TERNARY SLAGS AND INVESTIGATION OF PHASE CHARACTERISTICS[J]. Acta Metall Sin, 1982, 18(4): 456-462.
1 Daviec, M.W., Proceedings of the International Symposium on Metallurgical Chemical-Applications in Ferrous Metallurgy, Univ. Sheffield, 1971, Chemical Metallurgy of Iron and Steel, Publ. Iron Steel Inst., London, 1973, p. 43. 2 洪彦若;叶杏甫;郭昭信,钢铁,(1980) ,№.9,23. 3 稀土杂志社,未发表资料,1980. 4 王常珍;邹元爔,金属学报,16(1980) ,190. 5 洪彦若;白江添,金属学报,15(1979) ,51. 6 朱之凯;洪彦若;毛裕文,北京钢铁学院学报,(1979) ,№.2,99. 7 中国科学院贵阳地球化学研究所,矿物X射线粉晶鉴定手册,科学出版社,1978年,p.68. 8 中国科学院贵阳地球化学研究所,稀有元素矿物鉴定手册,科学出版社,1972,p.120. 9 Levin, E.M.; Robbins, C.R.; Mcmurdie, H.F., Phase Diagrams for Ceramists, 1969 Supplement,Amer. Ceram. Soc., 2nd ed., p. 84, 446. 10 Kozakevitch, P., Metallurgical Society Conference, Vol. 7, Physical Chemistry of Process Metal-lurgy, Part 1, Ed. George, R., Interscience Publ., New York, London., 1961, p. 97. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|