| Al-Si-Ge三元合金相图的研究 |
| 刘淑祺;孙国平;张启运 |
| 北京大学化学系;北京大学化学系;北京大学化学系 |
|
| THE PHASE DIAGRAM OF SYSTEM Al-Si-Ge |
| Liu Shuqi Sun Guoping Zhang Qiyun (Department of Chemistry; Beijing University) (Manuscript received 2 February; 1981; revised manuscript 13 January; 1982) |
引用本文:
刘淑祺;孙国平;张启运. Al-Si-Ge三元合金相图的研究[J]. 金属学报, 1982, 18(4): 451-523.
,
,
.
THE PHASE DIAGRAM OF SYSTEM Al-Si-Ge[J]. Acta Metall Sin, 1982, 18(4): 451-523.
| 1 Block, H.H., U.S. Pat., 2 508 008,(1950) .
2 Werner, W.J., U.S. Pat., 3 791 820,(1974) .
3 桑野明良,日本公开特许公报,52-33860,(1977) .
4 Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 133.
5 Hansen, M. ibid., p. 97.
6 Hansen, M., ibid., p. 774. |
|