| A-15型Nb_3(Al,Ge)中长程有序的讨论 |
| 姜小龙;张宏 |
| 中国科学院上海冶金研究所;中国科学院上海冶金研究所 |
|
| A DISCUSSION ON LONG-RANGE ORDER IN Nb_3 (Al,Ge) COMPOUND WITH A-15 STRUCTURE |
| Jiang Xiaolong Zhang Hong (Shanghai Intitute of Metallurgy; Academia Sinica) (Manuscript received 21 February; 1981) |
引用本文:
姜小龙;张宏. A-15型Nb_3(Al,Ge)中长程有序的讨论[J]. 金属学报, 1982, 18(4): 439-443.
,
.
A DISCUSSION ON LONG-RANGE ORDER IN Nb_3 (Al,Ge) COMPOUND WITH A-15 STRUCTURE[J]. Acta Metall Sin, 1982, 18(4): 439-443.
1 Arrehenius, G.; Corenzwit, E.; Fitzgerald, R.; Hollo, G.W., Jr., Luo, H.L.; Matthias, B.T.; Zachariasen, W.H., Proc. Nat. Acad. Sci., 61(1968) , 621. 2#12 3 Kitchingman, W. J.; Birch, A., Met. Sci. J., 7(1973) , 191. 4 张宏;姜小龙,物理,11(1982) ,44. |
|