| 奥氏体低温分解形成下贝氏体中的ε-Fe_3C相的价电子结构分析 |
| 余瑞璜;张瑞林 |
| 吉林大学物理系;吉林大学物理系 |
|
| VALENCE ELECTRON STRUCTURE ANALYSIS OF ε-Fe_3C IN BAINITE FORMED BY AUSTENITE LOWTEMPERATURE DECOMPOSITION |
| Yu Ruihuang S.H.Yu Zhang Ruilin (Department of Physics; Jilin University; Changchun) (Manuscript received 16 January; 1981) |
引用本文:
余瑞璜;张瑞林. 奥氏体低温分解形成下贝氏体中的ε-Fe_3C相的价电子结构分析[J]. 金属学报, 1982, 18(4): 444-450.
,
.
VALENCE ELECTRON STRUCTURE ANALYSIS OF ε-Fe_3C IN BAINITE FORMED BY AUSTENITE LOWTEMPERATURE DECOMPOSITION[J]. Acta Metall Sin, 1982, 18(4): 444-450.
1 余瑞璜,科学通报,23(1978) ,217. 2 Jack, K.H., Acta Crystallogr., 3(1950) , 392. 3 Hehemann, R.F.; Kinsman, K.R.: Aaronson, H.I., Metall. Trans., 3(1972) , 1077. 4 Jack, K.H., Acta Crystallogr., 5(1952) ; 404. 5 Pearson, W.B., A Handbook of Lattice Spacings and Structures of Metals and Alloys, Pergamon Press, New York, 1958, p. 121. 6 Jack, K.H., J. Iron Steel Inst., 169(1951) , 26. 7 余瑞璜,待发表. 8 余瑞璜,待发表. 9 Hofer, L.J.E.; Cohn, E.M., J. Am. Chem. Soc., 81(1959) , 1576. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|