| 金属溶剂萃取的热力学研究 |
| 滕藤;李以圭;程振华;张良平 |
| 清华大学化学化工系;清华大学化学化工系;清华大学化学化工系;清华大学化学化工系 |
|
| THERMODYNAMICAL STUDY ON SOLVENT EXTRACTION OF METALS |
| Teng Teng;Li Yigui;Cheng Zhenhua;Zhang Lianping Department of Chemistry and Chemical Engineering; Tsinghua University; Beijing |
引用本文:
滕藤;李以圭;程振华;张良平. 金属溶剂萃取的热力学研究[J]. 金属学报, 1982, 18(2): 201-210.
,
,
,
.
THERMODYNAMICAL STUDY ON SOLVENT EXTRACTION OF METALS[J]. Acta Metall Sin, 1982, 18(2): 201-210.
1 Davis,W.;Mrocheck,J.,Jr.;Judkins,R.R.,J.Inorg.Nucl.Chem.,32(1970) ,1689. 2 Watson,S.B.;Rainey,R.H.,DRNL-TM-5123,1975. 3 Homer,D.E.,ORNL-TM-2711,1970,p.27. 4 Goldberg,S.M.;Benedict,M.,Nucl.Sci Eng.,47(1972) ,169. 5 #12 6 李以圭;滕藤;张良平,清华大学学报,20(1980) ,№3,7. 7 #12 8 #12 9#12 10#12 11 Irving,H.M.N.H.,Ion Exchange and Solvent Extraction,Vol.6,Ed.Marinsky,J.A.;Marcus,Y.,Marcel Dekker,New York,1974,p.139. 12 Wingefors,S.;Liljenjin,J.O.;Saalman,E.,International Solvent Extraction Conference-80,Liege,Vol.3,1980,Report № 80-116,Association of Engineers of Univ.of Liege,Belgium. 13 Kertes,A.S.;Grauer,F.,J.Phys.Chem.,77(1973) ,3107. 14 Tsimering,L.;Kertes,A.S.,International Solvent Extraction Conference-74,Lyon,Vol.1,(1974) ,Soc.Chem.Ind.,London,p.1433. 15 Kertes,A.S.;Tsimering,L.,J.Phys.Chem.,81(1977) ,120.t |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|