| 胺类萃取Cr,Mo,W,V等过渡元素规律的研究 |
| 于淑秋;陈家镛 |
| 中国科学院化工冶金研究所;中国科学院化工冶金研究所 |
|
| SOLVATION EXTRACTION OF TRANSITIONMETALS Cr, Mo, W AND V BY AMINES |
| Yu Shuqiu;Chen Jiayong Chen Chiayung Institute of Chemical Metallurgy; Academia Sinica; Beijing |
引用本文:
于淑秋;陈家镛. 胺类萃取Cr,Mo,W,V等过渡元素规律的研究[J]. 金属学报, 1982, 18(2): 187-200.
,
.
SOLVATION EXTRACTION OF TRANSITIONMETALS Cr, Mo, W AND V BY AMINES[J]. Acta Metall Sin, 1982, 18(2): 187-200.
1 Yu,S.;Meng,S.;Chen,C.,1980 Int.Solvent Extraction Conference,Paper 80~132,Liege,Belgium. 2 于淑秋;孟祥胜;陈家镛,中国科学,(1982) ,№1. 3 Pope,M.T.;Dale,B.W.,Q.Rev.Chem.Soc.,22(1968) ,527. 4 Rieger,P.H.;Aust.J.Chem.,26(1973) ,1173. 5 Kepert,D.L.,Isopolyanions and Hcterpolyanions,in Comprehensive Inorganic Chemistry,A.F.Trotman-Dickenson,Executive Editor,Vol.4,Pergamon,Oxford,Endland,1973,p.607-672. 6 Esnault,F.;Robaglia,M.,Proc.Int.Solvent Extraction Conf.,Vol.3,Soc.Chem.Ind.,London,1974,p.2765. 7 Launay,J.-P.;Boyer,M.,J.Inorg.Nucl.Chem.,38(1976) ,243. 8 Gmelins Handbuch der Anorganischen Chimie,48:Vanadium.Teil B,Lfg.1,1967,p.132-166. 9 南京大学地质系编,地球化学,科学出版社,1979,p.136. 10 Kertes,A.S.,The Chemistry of Solvent Extraction in Recent Advances in Liquid-Liquid Extraction,Ed.Hanson,C.,Pergamon Press,Oxford,Endland,1971,p.15-72. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|