金属学报  1981, Vol. 17 Issue (4): 461-466    
  论文 本期目录 | 过刊浏览 |
玻璃对金属浸润性能的键参数描述
宁远涛;王永立;袁启珑
冶金工业部贵金属研究所;冶金工业部贵金属研究所;南京玻璃纤维研究院
A BOND PARAMETER APPROACH TOW ETTABILITY OF MOLTEN GLASS ON Pt ALLOY
by Ning Yuantao; Wang Yongli(Institute of Precious Metals)and Yuan Qilong (Nanjing Institute of Glassfibre)
引用本文:

宁远涛;王永立;袁启珑. 玻璃对金属浸润性能的键参数描述[J]. 金属学报, 1981, 17(4): 461-466.
, , . A BOND PARAMETER APPROACH TOW ETTABILITY OF MOLTEN GLASS ON Pt ALLOY[J]. Acta Metall Sin, 1981, 17(4): 461-466.

全文: PDF(489 KB)  
摘要: 本工作测定了熔融玻璃与几种铂合金的接触角,讨论了浸润机理,并用键参数方法总结了玻璃对金属浸润性能的有关规律,在浸润性能与纯金属及合金元素的键参数、浸润性能与玻璃组元的键参数之间建立了定性的联系。
Abstract:The bond parameter approach to the wetting behaviour of molten glass on certain Pt alloys was attempted on the basis of their equilibrium contact angle tests. It seems to indicate that the dependence of the wetting behaviour on the bond parameters of pure metals, and Pt-alloy constituents as well as glass components itself may be qualitatively generalized.
收稿日期: 1981-04-18     
[1] Copley, G. J., Rivers, A. D. and Smith, R., J. Mater. Sci., 10 (1975) , 1285.
[2] Selman, G. L., Spender, M. R. and Darling, A. S., Platinum Met. Rev. 9 (1965) . 130.
[3] Copley, G. J. and Rivers, A. D., J. Mater. Sci., 10(1975) , 1291.
[4] Zackay, V. F., Mitchell, D. W., Mitoff, S. P. and Pask, J. A., J. Am. Ceram. Soc., 36 (1953) , 84.
[5] Fulrath, R. M., Mitoff, S. P. and Pask, J. P., J. Am. Ceram. Soc., 40 (1957) , 269; 118.
[6] Volpe, M. L., Fulrath, R. M. and Pask, J. A., J. Am. Ceram. Soc., 42 (1959) , 102.
[7] #12
[8] 陈念贻,键参数函数及其应用,科学出版社,1976,p.74.
[9] #12
No related articles found!