| 硅酸盐熔体聚合度的确定及其应用 |
| 窦士学;刘化坤 |
| 东北工学院;东北工学院 |
|
| DETERMINATION OF EQUILIBRIUM CONSTANT FOR SILICATE MELT POLYMERIZATION AND ITS APPLICATION |
| by Dou Shixue and Liu Huakun (Northeast Institute of Technology) |
引用本文:
窦士学;刘化坤. 硅酸盐熔体聚合度的确定及其应用[J]. 金属学报, 1981, 17(4): 454-460.
,
.
DETERMINATION OF EQUILIBRIUM CONSTANT FOR SILICATE MELT POLYMERIZATION AND ITS APPLICATION[J]. Acta Metall Sin, 1981, 17(4): 454-460.
[1] Flory, P. J., Principles of Polymer Chemistry, Cornell University Press, New York, 1953. [2] Frincham, C. J. B. and Richardson, F. D., Proc, R. Soc., 223 (1954) , 40, [3] Toop, G. W. and Samis, C. S., Trans. Metall. Soc. AIME 224 (1962) , 878. [4] Masson, C. R., Canada, N. S., Proc. R. Soc., Ser. A, 287 (1965) 201. [5] Whiteway, S. G., Smith, I. B. and Masson, C. R., Can. J. Chem., 48 (1970) , 33. [6] Masson, C. R., Smith, I. B. and Whiteway, S. G., Can. J. Chem., 48 (1970) , 201. [7] Ibid, 45 (1970) , 1457. [8] Yokokawa, T. and Niwa, K., Trans. Jpn. Inst. Met., 10 (1969) , 3. [9] Von Kapoor, M. L. and Frohberg, M. G., Arch. Eisenhuettenwes., 41 (1970) , 1035. [10] Gaskell, D. R., Metall. Trans., 8B (1977) , 131. [11] Masson, C. R., J. Iron Steel Inst., 210 (1972) , 89. [12] Balta, P. and Balta, F., Roum. Chim. 16 (1971) , 1537. [13] Allred, A. L. and Rochow, E. G., J. Inorg. Nucl. Chem., 5 (1958) , 264. [14] Sakawa, M. and Masson, C. R., Trans. Iron Steel Inst. Jpn., 18 (1978) , 173. [15] Richardson, F. D. and Webb, L. E., Bull Inst. Min. Metall., (1955) , № 583 529. [16] Morgan, R. A. and Hummel, F. A., J. Am. Ceram. Soc., 32 (1949) , 250.z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|