| 液相烧结的30MGs·Oe稀土永磁体 |
| 肖文涛;祝景汉;孙天铎 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| 30 MGs.Oe Sm-Co PERMANENT MAGNETS PREPARED BY LIQUID PHASE SINTERING |
| by Xiao Wentao; Zhu Jinghan and Sun Tianduo (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry) |
引用本文:
肖文涛;祝景汉;孙天铎. 液相烧结的30MGs·Oe稀土永磁体[J]. 金属学报, 1981, 17(4): 424-432.
,
,
.
30 MGs.Oe Sm-Co PERMANENT MAGNETS PREPARED BY LIQUID PHASE SINTERING[J]. Acta Metall Sin, 1981, 17(4): 424-432.
[1] Ojima, T., et al., IEEE Trans. Magn. MAG-13 (1977) , 1317. [2] Livingston, J. D., J. Appl. Phys., 46 (1975) , 5259. [3] Mishra, R. K. and Thomas, G., Proc. Fourth Int. Workshop on Rare Earth-Cobelt Permanent Magnets and Their Appl ication., May 22-24, 1979, Hakone, Jap., p. 301. [4] Benz, M. G. and Martin, D. L., J. Appl. Phys., 43 (1972) , 3165. |
|