Y(Mn_(1-x)Fe_x)_(12)的结构和磁性 |
杨应昌 |
北京大学物理系 |
|
STRUCTURAL AND MAGNETIC PROPERTIES OF Y (Mn_(1—x)Fe_x)_(12) |
by Yang Yingchang (Dept. of Physics; Beijing University) |
引用本文:
杨应昌. Y(Mn_(1-x)Fe_x)_(12)的结构和磁性[J]. 金属学报, 1981, 17(3): 355-358.
.
STRUCTURAL AND MAGNETIC PROPERTIES OF Y (Mn_(1—x)Fe_x)_(12)[J]. Acta Metall Sin, 1981, 17(3): 355-358.