| 熔体淬火形成非晶态的判据 |
| 宁远涛;周新铭 |
| 冶金工业部贵金属研究所;冶金工业部贵金属研究所 |
|
| A CRITERION OF THE FORMATION OF AMORPHOUS STATE BY MELT QUENCHING |
| by Ning Yuantao and Zhou Xinming (Institute of Precious Metals Research) |
引用本文:
宁远涛;周新铭. 熔体淬火形成非晶态的判据[J]. 金属学报, 1981, 17(3): 278-284.
,
.
A CRITERION OF THE FORMATION OF AMORPHOUS STATE BY MELT QUENCHING[J]. Acta Metall Sin, 1981, 17(3): 278-284.
[1] Donald, I. W. and Davies, H. A., J. Non-Cryst. Solids, 30 (1978) , 77. [2] 施天生、郑如龙、陈念贻,金属学报,15(1979) ,94. [3] Anantharaman, T. R. and Suryanarayana, C., J. Mater. Sci., 6 (1971) , 1111. [4] Chen, H. S. and Jackson, K. A., Metallic Glasses, Papers Presented at a Seminar of the Materials Science Division of the ASM, Sept. 1976, ASM, Metals Park, Ohio, 1978, p. 74. [5] Sommer, F., Duddek, G. und Predel, B., Z. Metallk., 69 (1978) , 587. [6] Rapp, O., Lindberg, B., Chen, H. S. and Ran, K. V., J. Less-Common Metals, 62 (1978) , 221. [7] Duwez, P. and Johnson, W. L., J. Less-Common Metals, 62 (1978) , 215. [8] Anantharaman, T. R., Ramachandrarao, P., Suryanarayana, C., Lelc, S., Chattopadhyay, K., Sastry, G. V. S. and Davies, H. A., Rapidly Quenched Metal Ⅲ, Vol. 1, ed. by B. Cantor, London, 1978. [9] Chen, H. S. and Miller, C. E., Rev. Sci. Instrum., 41 (1970) , 1237. [10] Hansen, M., Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958. [11] Elliott, R. P., Constitution of Binary Alloys, First Suppl. McGraw-Hill, New York, 1965. [12] Hawkins, D. T. and Hultgren, R., Metals Handbook, 8th Ed., Vol. 8: Metallography Structures and Phase Diagrams, ASM, Metals Park, Ohio, 1973. [13] Takayama, S., J. Mater. Sci., 11 (1976) , 164. [14] Zielinski, P. G. and Matyja, H., Rapidly Quenched Metal Ⅱ, Section 1, ed. by N. J. Grant, B. C. Giesen, USA, MIT, 1976, p. 237. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|