| 稀土元素对Fe-Cr-Al合金1200℃氧化层择尤取向的影响 |
| 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸 |
|
| EFFECTS OF RARE EARTH ON PREFERRED ORIENTATION IN OXIDE SCALE O FA Fe-Cr-Al ALLOY |
| by Zhang Lixin; Luo Jixun; Yin Yaode and Li Liguang (Institute of Metal Research; Academia Sinica) Zhao Qi and Zhang Jiayun |
引用本文:
张立新;骆继勋;银耀德;李黎光;赵齐;张家芸. 稀土元素对Fe-Cr-Al合金1200℃氧化层择尤取向的影响[J]. 金属学报, 1981, 17(3): 233-242.
,
,
,
,
,
.
EFFECTS OF RARE EARTH ON PREFERRED ORIENTATION IN OXIDE SCALE O FA Fe-Cr-Al ALLOY[J]. Acta Metall Sin, 1981, 17(3): 233-242.
[1] 骆继勋、银耀德、林生昆、赵齐、王俭,金属学报,13(1977) ,263. [2] 天野忠昭,矢島聖使,斎藤安俊,日本金属学会誌,41(1977) ,1074. [3] Golightly, F. A., Sott, F. H. and Wood, G. C., Oxid. Metals, 10 (1976) , 163. [4] Kubaschewski, O. and Hopkins, B. E., Oxidation of Metals and Alloys, 2nd ed. Butterworths, London, 1962, p. 66. [5] Muller, M. H. Chernock, W. P. and Beck, P. A., Trans. AIME, 212 (1958) , 39. [6] Klug, H. P. and Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous, 2nd ed., John Wiley & Sons New York, 1974, p. 360. [7] 张立新、银耀德、李黎光、赵齐、张丙申,金属学报,16(1980) . [8] Felten, E. J. and Pettit, F. S., Oxid. Metals, 10 (1976) , 189. [9] Hirota, K. and Komatsu, W., J. Amer. Ceram. Soc., 60 (1977) , 105. [10] Sadananda, K. and Marcinkowski, M. J., J. Appl. Phys., 45 (1974) , 1521. [11] Stephens, D. L. and Alford, W. J., J. Amer. Ceram. Soc., 47 (1964) , 81. [12] Scheuplein, R. and Gibbs, P., J. Amer. Ceram. Soc., 43 (1960) , 458. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|