| 低铝钛35Ni-15Cr型铁基高温合金的高温长期性能和组织稳定性的研究 |
| 郭建亭;徐嘉勋;安万远 |
| 中国科学院金属研究所;哈尔滨汽轮机厂;哈尔滨汽轮机厂 |
|
| AN EVALUATION OF LONG-TERM PERFORMANCE AND MICROSTRUCTURAL STABILITY OF A 35Ni-15Cr TYPE IRON-BASE SUPERALLOY WITH REDUCED Al+Ti CONTENT |
| Guo Jianting;Xu Jiaxun;An Wangyuan Institute of Metal Research; Academia Sinica Harbin Turbine Works |
引用本文:
郭建亭;徐嘉勋;安万远. 低铝钛35Ni-15Cr型铁基高温合金的高温长期性能和组织稳定性的研究[J]. 金属学报, 1980, 16(4): 386-492.
,
,
.
AN EVALUATION OF LONG-TERM PERFORMANCE AND MICROSTRUCTURAL STABILITY OF A 35Ni-15Cr TYPE IRON-BASE SUPERALLOY WITH REDUCED Al+Ti CONTENT[J]. Acta Metall Sin, 1980, 16(4): 386-492.
[1] 铁基高温合金研究组,金属学报,14(1978) ,227. [2] #12 [3] #12 [4] Betteridge, W. and Heslop, J., The Nimonic Alloys and Other Nickel-Base High-Temperature Alloys, Edward Arnold, 1974, p. 243. [5] #12 [6] 铁基高温合金研究组,金属学报,14(1978) ,348. [7] Susukida, H., Sunamoto, D. and Sakumoto, Y., ASME Gas Turbine Conference and Products Show. 69-GT-12. 2--4. [8] 郭建亭,朱耀霄,师昌绪,金属学报,10(1974) ,74. [9] Webster, G. A. and Piearcey, B. J., Metal Sci. J., 1 (1967) , 97. [10] Sullivan, C. P., Webster, G. A. and Piearcey, B. J., J. Inst. Metals, 96 (1968) , 274. [11] Tien, J. K. and Copley, S. M., Met. Trans., 2 (1971) , 215. [12] Tien, J. K. and Copley, S. M., Met. Trans., 2 (1971) , 543. [13] 郭建亭,金属学报,16(1980) ,30. [14] Tien, J. K. and Gamble. R. P., Met. Trans.. 2 (1971) . 1663. [15] 西羲澈,特殊钢,17(1968) ,№5,59 |
|