| 低合金铸钢中硼的分布 |
| 褚幼义;贺信莱;余宗森;欧宇光 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;内蒙第一机械厂 |
|
| THE DISTRIBUTION OF BORON IN LOW ALLOY CAST STEELS |
| Chu Youyi;He Xinlai;Yu Zongsen;Ou Yuguang Beijing Institute of Iron and Steel Technology and Nei Monggol №. 1 Machine Works |
引用本文:
褚幼义;贺信莱;余宗森;欧宇光. 低合金铸钢中硼的分布[J]. 金属学报, 1980, 16(4): 380-490.
,
,
,
.
THE DISTRIBUTION OF BORON IN LOW ALLOY CAST STEELS[J]. Acta Metall Sin, 1980, 16(4): 380-490.
[1] 贺信莱,褚幼义,张秀林,余宗森,李秋萍,尹熙光,金属学报,13(1977) ,235. [2] Wilson, W. G., Elec. Furnace Conf. Proc., 31 (1973) , 154.p |
|