LaNi_5吸氢过程动力学的研究
吕曼琪;戚震中;吴平森
中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所
A STUDY OF THE KINETICS OF HYDROGEN ABSORPTION IN LaNi_5
Lu Manqi;Qi Zhenzhong;Wu Pingsen Institute of Metal Research; Academia Sinica
引用本文:

吕曼琪;戚震中;吴平森. LaNi_5吸氢过程动力学的研究[J]. 金属学报, 1980, 16(1): 65-72.
, , . A STUDY OF THE KINETICS OF HYDROGEN ABSORPTION IN LaNi_5[J]. Acta Metall Sin, 1980, 16(1): 65-72.

全文: PDF(571 KB)  
摘要: 在初始压力15—30atm、温度20—85℃的范围内研究了储氢材料LaNi_5在恒温时吸氢的动力学过程.实验结果表明:吸氢量与时间的对数呈线性关系;吸氢速率随初始压力的提高或吸氢温度的升高而改变.提出了表示吸氢速率对时间、初始压力、吸氢温度依赖性的关系式,实验结果与之一致.按这一关系式可以得到吸氢速率的限制性环节的激活能U.在吸氢量(以饱和度计)约70%以前,U约为2.0 kcal/mol H_2,吸氢量更高时约3.2 kcal/mol H_2.这些数据为进一步确定吸氢速率的限制性环节提供了重要参数.
Abstract:The kinetics of hydrogen absorption in LaNi_5 has been investigated at initialpressures of 15--30 atm and temperatures in the range of 20--85℃. LaNi_5 was pre-pared in a ZrO_2 crucible in a graphite-tube furnace under vacuum. It is shownthat a linear relationship exists between the amount of hydrogen absorbed, W,and the time of reaction on a logarithmic scale and the rate of hydrogen absorp-tion depends on the initial pressure and the test temperature. The P-X-T curves of the LaNi_5 system have been determined. For each testtemperature there is a corresponding pressure plateau P_0 and it is therefore as-sumed that for every initial pressure P_0 there is a corresponding balance temperatureT_0, and T_0-T may be taken as the driving force of hydrogen absorption processin LaNi_5 at initial pressure P_0 and test temperature T. The absorption of hydro-gen takes place in three steps: (1) surface reaction, which seems to be rather com-plicated; (2) diffusion of hydrogen atoms and (3) phase transformation f LaNi_5 toa hydride phase. All these steps are thermal activation processes, and thereforethe e~(-U/RT) can be introduce in the hydrogen absorption process. The relatioshipbetween the absorption rate, the initial pressure, the test temperature and time isgiven as follow: dW/dt=A_0(T_0-T)e~(-U/RT)·1/tThe activation energy of the rate limiting step U is about 2 or 3.2 kcal/molaccording to whether the amount of hydrogen absorbed is less or more than 70%respectively. The parameter U of the rate-limiting step during hydrogen absorptionin LaNi_5 can be obtained as shown by our experiments.
收稿日期: 1980-01-18     
[1] Zijlstra, J.H. and Westerdorp, F.F., Solid State Commun., 7 (1969) , 857.
[2] Van Vucht, J.H.N., Kuijpers, F.A. and Bruning, H.C.A.M., Philips Res. Rep., 25 (1970) , 133.
[3] Reilly, J.J. and Wiswall, R.H., Inorg. Chem., 6 (1967) , 2220.
[4] Reilly, J.J. and Wiswall, R.H., The Formation and Properties of FeTi Hydride, BNL-177711, 1973.
[5] Kuijpers, F.A., Philips Res. Rep. Suppl., 1970, № 2, p. 28.
[6] Reilly, J.J., Hoffman, K.C., Strickland, G. and Wiswall, R.H., 26th Power Sources Symp., 1974, Atlantic City, New Jersey, p. 11.
[7] Klein, M. and George, M., 26th Power Sources Symp., 1974, Atlantic City, New Jersey, p.18.
[8] Tanaka, S., Clewley, J.D. and Flaragan, T. B., J. Less-Common Metals, 56 (1977) , 137.
[9] Boser, O. and Lehrfeld, D., Record of the 10th Intersociety Energy Conversion Engineering Conference, 1975, Published by IEEE, New York, Newark Delaware, p. 1363.
[10] Lundin, C.E. and Lynch, F.E., Record of the 10th Intersociety Energy Conversion Engineering Conference, 1975, Published by IEEE, New York, Newark Delaware, p. 1380.
[11] Boser, O., J. Less-Common Metals, 46 (1976) , 91.
[12] Buschow, K.H.J. and Van Mal, H.H., J. Less-Common Metals, 29 (1972) , 203.
[13] Pryde, J.A. and Titcomb, C.G., J. Phys. C: Solid State Phys., 5 (1972) , 1293.
[14] Birnbaum, H.K. and Wert, C.A., Ber. Bunsenges. Phys. Chem., 76 (1972) , 806.
No related articles found!