准解理断口的特征长度参数与断裂韧度的关系
孙福玉
冶金工业部钢铁研究总院
CORRELATION BETWEEN THE CHARACTERISTIC LENGTH PARAMETER OF THE QUASI-CLEAVAGE FRACTURE AND FRACTURE TOUGHNESS
Sun Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry
引用本文:

孙福玉. 准解理断口的特征长度参数与断裂韧度的关系[J]. 金属学报, 1980, 16(1): 59-134.
. CORRELATION BETWEEN THE CHARACTERISTIC LENGTH PARAMETER OF THE QUASI-CLEAVAGE FRACTURE AND FRACTURE TOUGHNESS[J]. Acta Metall Sin, 1980, 16(1): 59-134.

全文: PDF(1924 KB)  
摘要: 利用扫描电镜对一些断裂韧性试样的断口表面进行了观察.发现:对于遵从准解理机制开裂的材料,从预制裂纹顶端到其前缘的初始准解理开裂源的平均距离ξ是一个特征参数,它不仅与断裂韧度G_(Ic)有学,而且是塑性区应力场的一个重要参量.
Abstract:The fracture surfaces of certain fracture toughness specimens have been ex-amined by SEM. With materials fractured in quasi-cleavage mechanism, the meandistance, ξ, from the pre-crack tip to the site where the quasi-cleavage crackstarts is regarded to be a characteristic parameter. It seems that this related toG_(Ic) and can be used as an important parameter characterizing the stress field ofthe plastic zone.
收稿日期: 1980-01-18     
[1] Spitzig, W.A., Amer. Soc. Test. Mater., Spec. Tech. Publ. № 453, p. 90.
[2] Brok, D., Eng. Fract. Mech., 6 (1974) , 173.
[3] 陈篪,金属学报,13(1977) ,57.
[4] 陈篪,金属断裂研究文集,冶金工业出版社,1978年,p.30.
[5] Levy, N., Marcal, P.V., Ostergren, W.T. and Rice, J.R., Int. J. Fract. Mech., 7(1971) , 143.
[6] Riichie, R.O., Knott, J.F. and Rice, J.R., J. Mech. Phys. Solids, 21 (1973) , 395.
No related articles found!