| 几种合金元素对Pt高温蠕变激活能的影响 |
| 宁远涛;王永立 |
| 贵金属研究所;贵金属研究所 |
|
| INFLUENCE OF CERTAIN ALLOYING ELEMENTS ON THE CREEP ACTIVATION ENERGY OF PLATINUM |
| Ning Yuantao;Wang Yongli Institute of Noble Metals Research |
引用本文:
宁远涛;王永立. 几种合金元素对Pt高温蠕变激活能的影响[J]. 金属学报, 1979, 15(4): 548-594.
,
.
INFLUENCE OF CERTAIN ALLOYING ELEMENTS ON THE CREEP ACTIVATION ENERGY OF PLATINUM[J]. Acta Metall Sin, 1979, 15(4): 548-594.
[1] Bennett, H. E., Platinum Metals Rev., 2 (1958) , 120. [2] Bourne, A. A. and Darling, A. S., Platinum Metals Rev., 7 (1963) , 42. [3] Reinacher, G., Metall., 15 (1961) , 657; 29 (1975) , 681. [4] Sadowski, E. P., Refract. Metals Alloys, 11 (1960) , 465. [5] Darling, A. S., Platinum Metals Rev.. 17 (1973) , 130. [6] 38 (1974) , 4, 827. [7] 1977, 169. [8] 37(1974) , 1, 142. [9] Chaston, J. C., Platinum Metals Rev., 19 (1975) , 135. [10] Owens-Corning Fiberglass Corp., U. S. Pat. 3, 622, 289, 1972. [11] Owens-Corning Fiberglass Corp., Brit. Pat. 1,350, 644, 1974. [12] Conrad, H., High-Strength Materials, Ed. by V. F. Zackay, Wiley, New York, 1965, p. 445. [13] Reinacher, G., Z. Metallk., 62 (1971) , 835. [14] Selman, G. L., Day, J. G. and Bourne, A. A., Platinum Metals Rev., 18 (1974) , 42; 20 (1976) , 86.: |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|