| 一种计算裂纹扩展的表达式 |
| 赵廷仕 |
| 华中工学院 |
|
| AN EXPRESSION FOR CALCULATING CRACK EXTENSION |
| Zhao Tingshi Central China Engineering Institute |
引用本文:
赵廷仕. 一种计算裂纹扩展的表达式[J]. 金属学报, 1979, 15(2): 296-298.
.
AN EXPRESSION FOR CALCULATING CRACK EXTENSION[J]. Acta Metall Sin, 1979, 15(2): 296-298.