| 非晶态形成的临界条件 |
| 郑兆勃 |
| 中国科学技术大学物理系 |
|
| CERTAIN CRITERION FOR THE FORMATION OF AMORPHOUS SOLIDS |
| Zheng Zhaobo Dept.of Physics; University of Science and Technology of China |
引用本文:
郑兆勃. 非晶态形成的临界条件[J]. 金属学报, 1979, 15(2): 292-295.
.
CERTAIN CRITERION FOR THE FORMATION OF AMORPHOUS SOLIDS[J]. Acta Metall Sin, 1979, 15(2): 292-295.
[1] Turnbull, D. and Cohen, M. H., J. Chem. Phys., 29 (1958) , 1049. [2] Turnbull, D., Contemp. Phys., 10 (1969) , 473. [3] Hoffman, J. D., J. Chem Phys., 29 (1958) , 1192. [4] Uhlmann, D. R., J. Non-Cryst. Solids, 7 (1972) , 337. [5] Onorato, P. I. K. and Uhlmann, D. R., J. Non-Cryst. Solids, 22 (1976) , 367 |
|