| 钢中白点断口的显微空隙与台阶花样 |
| 陈廉;徐永波;尹万全 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| UNHEALED POROSITIES AND CRYSTALLINE STEPS IN FLAKES |
| Chen Lian Xu Yong-bo Yin Wan-quan(Institute of Metal Research; Academia Sinica) |
引用本文:
陈廉;徐永波;尹万全. 钢中白点断口的显微空隙与台阶花样[J]. 金属学报, 1978, 14(3): 253-333.
,
,
.
UNHEALED POROSITIES AND CRYSTALLINE STEPS IN FLAKES[J]. Acta Metall Sin, 1978, 14(3): 253-333.
[1] “层次结构”断口三结合研究组,金属学报,12(1976) ,92. [2] Musatti, I. and Reggior, A., Metal Progr., 3 (1936) , 51. [3] Scott, T. E. and Troiano, A. R., J. Metals, 11 (1959) , 619. [4] Dana, A. W. et al., Trans. AIME, 7 (1955) , 895. [5] #12 [6] 下川義雄,鉄鋼,57(1971) ,1992. [7] Pittinato, G. F. et al., SEM/TEM Fractography Handbook, Metals and Ceramics Information Center, Columbus, (1975) , p. 56. [8] ASM Metals Handbook, vol. 9, Fractography and Atlas of Fractography (1974) , p. 89. [9] Engel-Klingele, Rasterelektronenmikroskopische Untersuchungen von Metallschaden, Gerling Institut fur Schadenforschung und Schadenverhutung GmbH, Koln (1974) , p. 114. [10] Phillips, A. and Kerlins, V., Metal Progr., 95 (1969) , 81. [11] Hemsworth, B. et al., Metal Constr. Brit. Weld. J., 1 (1969) , 5. [12] Ryder, D. A., Acta Met., 9 (1961) , 73. [13] 周敬等,金属学报,14(1978) .# |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|