| 铝和钛对一种35镍15铬型铁基高温合金组织结构和力学性能的影响 |
| 郭建亭 |
| 中国科学院金属研究所铁基高温合金研究组 |
|
| THE EFFECT OF ALUMINIUM AND TITANIUM ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AN IRON-BASE ALLOY |
| Res. Gp. of Iron-base Superalloy(Institute of Metal Research; Academia Sinica) |
引用本文:
郭建亭. 铝和钛对一种35镍15铬型铁基高温合金组织结构和力学性能的影响[J]. 金属学报, 1978, 14(3): 227-324.
.
THE EFFECT OF ALUMINIUM AND TITANIUM ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AN IRON-BASE ALLOY[J]. Acta Metall Sin, 1978, 14(3): 227-324.
[1] 郭建亭等,铬和硅对一种35Ni-15Cr型铁基高温合金力学性能和组织结构的影响,待发表. [2] 郭建亭等,金属学报,10(1974) ,74. [3] Raynor, D. and Silcock, J. M., Metal Sci. J., 4 (1970) , 121. [4] Brown, L. M. and Ham, R. K., Strengthening Methods in Crystals, ed. by A. Kelly and R. B. Nicholson, Elsevier, Amsterdam, (1971) , pp. 10-135. |
|