| (da)/(dN)与K_1间关系的探讨 |
| 陈篪 |
| 北京钢铁研究院 |
|
| AN INVESTIGATION OF THE RELATION BETWEEN da/dN AND K_I |
| Chen Chi (Chen Chih) (Beijing Institute of Iron and Steel Research) |
引用本文:
陈篪. (da)/(dN)与K_1间关系的探讨[J]. 金属学报, 1978, 14(2): 111-117.
.
AN INVESTIGATION OF THE RELATION BETWEEN da/dN AND K_I[J]. Acta Metall Sin, 1978, 14(2): 111-117.
[1] Cooke, R. J. and Beevers, C. J., Mater. Sci. Eng., 13 (1974) , № 3, 201. [2] 陈篪,未发表工作,(1974年)。 [3] 陈篪,力学,(1975) ,№ 3,124. [4] 陈篪等,用柔度法测定裂纹扩展速率,未发表,(1975年). [5] 陈篪等,压力容器用钢14MnMoNbB的断裂韧度及da/dN,未发表,(1976年). [6] 陈篪,裂纹扩展速率da/dN与K_1之间关系的探讨,未发表,(1977年)。 [7] Paris, P. C. et al., Amer. Soe. Test. Mater., Spec. Tech. Publ. № 513, (1972) , 141. [8] Knott, J. F., Fundamentals of Fracture Mechanics, Butterworths, London, 1973. [9] Barsom, J. M. et al., Eng. Fract. Mech., 2 (1971) , 301. [10] Richards, C. E. and Lindley, T. C., Eng. Fract. Mech., 4 (1972) , 811. [11] Clark, W. G. Jr., Met. Eng., 14 (1974) , № 3, 16. |
|