| 高合金钢与高温合金中的相 |
| 郭可信 |
| 中国科学院金属研究所 |
|
| PHASES IN HIGH ALLOY STEELS AND SUPERALLOYS |
| Kuo Ke-hsin (Institute of Metal Research; Academia Sinica) |
引用本文:
郭可信. 高合金钢与高温合金中的相[J]. 金属学报, 1978, 14(1): 73-95.
.
PHASES IN HIGH ALLOY STEELS AND SUPERALLOYS[J]. Acta Metall Sin, 1978, 14(1): 73-95.
[1] Sims, C. T. and Hagel, W. C., The Superalloys, Wiley, New York, 1972. [2] Sabol, G. P. and Stickler, R., Phys. Status Solidi, 35 (1969) , 11. [3] Sullivan, C. P. and Donachie, M. J. Jr., Metals Eng. Quart., 11 (1971) , No. 4, 1. [4] Banerjee, B. R., et aL, ASM Trans. Quart., 61 (1968) , 103. [5] 金子秀夫,日本金属学会誌,30(1966) ,157. [6] 郭可信(Kuo Ke-hsin), Acta Met., 1 (1953) , 301, 611. [7] Preis, G. and Lennartz, G., Arch. Eisenhuttenw., 46 (1975) , 509. [8] Piearcey, B. J. and Smashey, R. W., Trans. AIME, 239 (1967) , 451. [9] Dreshfield, R. L., ASM Trans. Quart., 61 (1968) , 352. [10] Leciejawicz, J., J. Less-Common Metals, 7 (1964) , 318. [11] Rosenbaum, B. M., NASA Tech. Note No. 1050, 1948. [12] Hagel, W. C. and Beattie, H. J. Jr., Trans. ASM, 49 (1957) , 978. [13] Anderson, T. and Lundberg, B., Met. Trans., 8A (1977) , 787. [14] Pollock, C. B. and Stadelmaier, H. H., Met. Trans., 1 (1970) , 767. [15] Fraker, A. C. and Stadelmaier, H. H., Trans. AIME, 245 (1969) , 847. [16] Ettmayer, P. and Suchentrunk, R., Monatsh. Chem., 101 (1970) , 1098. [17] Heijwegen, C. P. and Rieck, G. D., Met. Trans., 4 (1973) , 2159. [18] Elevated temperature properties as influenced by nitrogen additions to types 304 and 316 austenitic stainless steel, Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 522, 1969. [19] Hughes, H., J. Iron Steel Inst., 205 (1967) , 775. [20] Chatwin, W. H. et al., J. Iron Steel Inst., 207 (1969) , 1645. [21] Jack, D. H. and Jack, K. H., J. Iron Steel Inst., 210 (1972) , 790. [22] Ettmayer, P., Monatsh. Chem., 102 (1971) , 858. [23] 菊池 実,铁鋼,59([973) ,972. [24] 脇田三郎,铁鋼,61(1975) ,2418. [25] 郭可雠(Kuo Ke-bsin), Trans. AIME, 206 (1956) , 97. [26] Kikuchi, M. et al., Trans. Iron Steel Inst. Japan, 13 (1973) , 226. [27] Omsen, A. and Eliasson, L., J. Iron Steel Inst., 209 (1971) , 830. [28] Beattie, H. J. Jr., Acta Crystallogr., 11 (1958) , 607. [29] Coldren, A. P. et al., Trans. AIME, 230 (1964) , 1236. [30] Filippi, A. M., Met. Trans., 5 (1974) , 1423. [31] Danesi, W. P. et al., ASM Trans. Quart., 59 (1966) , 505. [32] Mihalisin, J. R. et aL, Trans. AIME, 242 (1968) , 2399. [33] Boesch, W. J. and Canada, H. B., J. Metals, 20 (1968) , No. 4, 46. [34] Sullivan, C. P., ASM Trans. Quart., 58 (1965) , 702. [35] Beattie, H. J. Jr. and Hagel, W. C., Trans. AIME, 209 (1957) , 911. [36] Brown, G. T. and Allsop, R. T., J. Iron Steel Inst., 194 (1960) , 435. [37] Hardy, J. V. and Brown, G. T., J. lron Steel Inst., 202 (1964) , 437. [38] Spiegel, F. X. et al., Trans. AIME, 227 (1963) , 575. [39] Abson, D. J. et al., J. Aust. Inst. Metals, 13 (1968) , 61. [40] Bardos, D. I. et al., Trans. AIME, 236 (1966) , 40. [41] Hughes, H., Nature, 183 (1959) , 1543. [42] Tither, S. J. and Clark, B. R., Metal Sci. J., 4 (1970) , 118. [43] Jack, D. H., Metal Sci, J., 4 (1970) , 22. [44] Frick, Von C. and Rohde, H., Arch. Eisenhuttenw., 31 (1960) , 419. [45] Kudielka, H. and Rohde, H., Z. Kristallogr. Kristallgeometrie, Kristallphys., Kristallchem., 114 (1960) , 447. [46] Casa, C. da and Nileshwar, V. B., J. Iron Steel Inst., 207 (1969) , 1003. [47] Novak, C. J. and Diran, L. M., J. Metals, 15 (1963) , 200. [48] Wallace, W. et al., Metallography, 6 (1973) , 511. [49] Donachie, M. J. Jr. and Kriege, O. H., J. Mater. 7 (1972) , 269. [50] Gemmill, M. G., et al., J. Iron Steel Inst., 184 (1956) , 122. [51] Beckmann, O. et al., Monatsh. Chem., 99 (1968) , 1580. [52] Kriege, O. H. and Baris, J. M., ASM Trans. Quart., 62 (1969) , 195. [53] 渡辺力蔵,九重常男,铁鋼,61(1975) ,2274. [54] Karg, A. V. et al., J. Inst. Metals, 99 (1971) , 301. [55] Sinha, A. K., Topologically Close-Packed Structures of Metal Alloys, Pergamon, London, 1972. [56] Pearson, W. B., A Handbook of Lattice Spacings and Structures of Metals and Alloys, Pergamon, London, 1958. [57] Cozar, R. and Pireau, A., Met. Trans., 4 (1973) , 47. [58] VerSnyder, F. L. and Beattie, H. J. Jr., Trans. ASM, 47 (1955) , 211. [59] Okubo, N. et al., J. Iron Steel Inst., 211 (1973) , 141. [60] Yagisawa, K.. and Fujita, H., Jap. J. Appl. Phys., 6 (1967) , 826. [61] Singhal, L. K. and Martin, J. W., J. Iron Steel Inst., 205 (1967) , 947. [62] 金柱,马实基,金属学报,10(1974) ,12. [63] Coutsouradis, D. et al., Cobalt, (1967) , No. 36, 144. [64] Birks, L. S. et al., Trans. AIME, 218 (1960) , 806. [65] Johnson, J. et al., J. Inst. Metals, 95 (1967) , 379. [66] McMullin, J. G. et al., Trans. ASM, 46 (1954) , 799. [67] Hughes, H. and LIewelyn, D. T., J. Iron Steel Inst., 192 (1959) , 170. [68] Beattie, H. J. Jr. and Hagel, W. C., Trans. AIME, 221 (1961) , 28. [69] Thompson, F. A. and West, D. R. F., J. Iron Steel Inst., 210 (1972) , 691. [70] Hughes, H. and Keown, S. R., J. Iron Steel Inst., 206 (1968) , 275. [71] Dyson, D. J. and Keown, S. R., Acta Met., 17 (1969) , 1095. [72] Leonard, R. B., Corrosion, 25 (1969) , 222. [73] Boesch, W. J. and Slaney, J. S., Metal Progr., 86 (1964) , No. 1, 109. [74] Woodyatt, L. R. et al., Trans. AIME, 236 (1966) , 519. [75] Rideout, S. et al., Trans. AIME, 191 (1951) , 872. [76] Sully, A. H., J. Inst. Metals, 80 (1952) , 173. [77] 郭可信 (Kuo Ke-hsin), Acta Met., 1 (1953) , 720. [78] Bergman, G. and Shoemaker, D. P., Acta Crystallogr., 7 (1954) , 857. [79] Hall, E. O. and Algie, S. H., Met. Rev., 11 (1966) , 61. [80] Barrett. C. S., J. Inst. Metals, 100 (1972) , 65. [81] 渡辺力蔵,鉄鋼,61(1975) ,2405.1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|