| 关于异种钢焊接接头的碳迁移问题 |
| 倪瑞澄;朱逢吾 |
| 北京钢铁学院金属物理教研组;北京钢铁学院金属物理教研组 |
|
| CARBON MIGRATION THROUGH THE WELDING JOINTS OF DISSIMILAR STEELS |
| Ni Rui-cheng Zhu Feng-wu (Bei]ing Institute of Iron and Steel Technology) |
引用本文:
倪瑞澄;朱逢吾. 关于异种钢焊接接头的碳迁移问题[J]. 金属学报, 1978, 14(1): 96-106.
,
.
CARBON MIGRATION THROUGH THE WELDING JOINTS OF DISSIMILAR STEELS[J]. Acta Metall Sin, 1978, 14(1): 96-106.
[1] Zuzn, H. and Morach, E., Z. Werkstofftech., 3 (1974) , 146. [2] 熊谷,金属材料,13(1973) ,29. [3] 渡辺正纪,向井喜彦,鋼溶接,日刊工業新聞社,东京,1971. [4] 根本正,佐佐木良一,溶接学会誌,32(1963) ,205. [5] 渡辺竹春,本間浩夫,金属材料,13(1973) ,No.12,10. [6] Kauczor, E., Prakt. Metallogr., 4 (1967) , 593. [7] Darken, L. S., Trans. AIME, 180 (1949) , 430. [8] Thielsch, H., Weld. J. (New York), 31 (1952) , No. 1, 37-S. [9] Christoffel, R. J. and Curran, R. M., Weld. J. (New York), 35 (1956) , No. 9, 457-S. [10] Eckel, J. F., Weld. J. (New York), 43 (1964) , No. 4, 170-S. [11] #12 [12] 新 成夫,溶接学会誌,45(1976) ,437. [13] Bodsworth, C. and Bell, H. B., Physical Chemistry of Iron & Steel Manufacture, 3rd Ed., Longman, London, 1972. [14] Argent, B. B. et al., J. Iron Steel Inst., 208 (1970) , 830. [15] Mehl, R. F. and Wells, C., Trans. AIME, 125 (1937) , 429. [16] Smith, R. P., J. Amer, Chem. Soc., 68(1946) , 1163. [17] 新 成夫,溶接冶金学,丸善株式会社,1972,p.220. [18] 邦武立郎,日本金属学会会報,3(1964) ,466. [19] Metal Reference Book, Vol. Ⅱ, 3rd Ed., by C. J. Smithells, Butterworths, London, 1962, p. 594. [20] Andrews, K. W., J. Iron Steel Inst., 203 (1965) , 721. [21] 有川正康,溶接学会誌,40(1971) ,No.2,20. [22] Iwamoto, N. et al., Trans. Jap. Weld. Res. Inst., 4 (1975) , 49. [23] Stickels, C. A., Met. Trans., 5 (1974) , 865. [24] #12 [25] 新成夫,金属材料,13(1973) ,No.12,20. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|