| 六水合氯化钇的脫水和无水氯化钇的气相水解的研究 |
| 苏勉■;裘炳毅 |
| 北京大学;北京大学 |
|
| THE DEHYDRATION OF HEXAHYDRATED YTTRIUM CHLORIDE AND THE VAPOR PHASE HYDROLYSIS OF ANHYDROUS |
| SU MIEN-TSNG; CH'IU PING-YI (Peking University) |
引用本文:
苏勉■;裘炳毅. 六水合氯化钇的脫水和无水氯化钇的气相水解的研究[J]. 金属学报, 1966, 9(2): 142-147.
,
.
THE DEHYDRATION OF HEXAHYDRATED YTTRIUM CHLORIDE AND THE VAPOR PHASE HYDROLYSIS OF ANHYDROUS[J]. Acta Metall Sin, 1966, 9(2): 142-147.
[1] Spedding, F. H.. Daane, A. H.: The Rare Earths, (Wiley, 1961) , p. 89-99. [2] Wendlandt, W. W.: J. Inorg. Nud. Chem., 1957, 5, 118. Wendlandt, W. W.: J. Inorg. Nucl. Chem., 1959, 9, 136. [3] Wendlandt, W. W., Bear, J. L.: Anal. Chim. Acta, 1959, 21, 439. [4] Koch, C. W., Broido; A., Cunningham, B. B.: J. Am. Chem. Soc., 1952, 74, 2349. Koch, C. W., Cunningham, B. B.: J. Am. Chem. Soc., 1953, 75, 796. Koch, C. W., Cunningham, B. B.: J. Am. Chem. Soc., 1954, 76, 1471. [5] #12 [6] Kleinheksel, J. H., Kremers, H. C.: J. Am. Chem. Soc., 1928, 50, 959. [7] #12 [8] #12 [9] C1ementduval: Inorganic Thermogravimetric Analysis, (Elsevier, 1963) , p. 55. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|