| 高炉型渣脫硫的离子理論 |
| 魏寿崑 |
| 北京钢铁学院 |
|
| THE IONIZATION THEORY OF DESULPHURIZATION WITH THE BLAST-FURNACE-TYPE SLAGS |
| WEI SHOU-KUN (Peking Institute oF Ferrous Metallurgy) |
引用本文:
魏寿崑. 高炉型渣脫硫的离子理論[J]. 金属学报, 1966, 9(2): 127-141.
.
THE IONIZATION THEORY OF DESULPHURIZATION WITH THE BLAST-FURNACE-TYPE SLAGS[J]. Acta Metall Sin, 1966, 9(2): 127-141.
[1] 魏寿崑:金属学报,1964,7,157. [2] #12 [3] #12 [4] Hatch, G. G., Chipman, J.: Trans. AIME,, 1949, 185, 274, 831. [5] Filer, E. W., Darken, L. S.: Trans. AIME, 1952, 194, 253. [6] Grant, N. J., Kalling, U., Chipman, J.: Trans. AIME, 1951, 191, 666. [7] Grant, N. J., Troili, O., Chipman, J.: Trans. AIME, 1951, 191, 672. [8] Taylor, J., Stobo, J. J.: J. Iron Steel Inst. (London), 1954, 178, 360. [9] #12 [10] Schenck, H., Frohberg, M. G., Gammal, T. El.: Arch. Eisenhuttenw., 1960, 31, 11. [11] Schenck, H., Fohberg, M. G., Gammal, T. El.: Arch. Eisenhuttenw., 1960, 31, 471. [12] Schenck, H.. Frohberg, M. G., Gammal, T. El.: Arch. Eisenhuttenw,., 1961, 32, 63. [13] Schenck. H., Frohberg, M. G., Gammal, T. El.: Arch. E, isenhuttenw., 1962, 33, 589. [14] 邹元爔:金属学报,1956,1,127,143. [15] #12 [16] Kalyanram, M. R., MacFarlane, T. G., Bell, H. B.: J. Iron Steel Inst. (London), 1960. , 195, 58. [17] Giedroyc, V., McPhail, A. N., Mitckell, J. G.: J. Iron Steel Inst. (London), 1964, 202, 11. [18] Frohberg. M. G., Arch. Eisenhuttenw., 1961, 32, 597. [19] #12 [20] Gokcen, N. A.: Trans. AIME., 1956, 206, 1558. [21] AIME: Electric Furnace Steelmaking (Interscience, 1963) , vol. 2, p. 133-134. [22] Bockris, J. O'M.. Kitchener, J. A., Ignatowicz, S. et al.: Trans. Faraday Soc., 1952, 48, 75. [23] Bockris, J. O'M., Mackenzie, J. D., Kitchener, J. A.: Trans. Faraday Soc.. 1955, 51, 1734. [24] Bockris, J. O'M., Tomlinson, J. W., White, J. L.: Trans. Faraday Soc,, 1956, 52, 299. [25] #12 [26] Sherman, C. W., Chipman, J.: Trans. AIME, 1952, 194, 597. [27] Morris, J. P., Buehl, R. C.: Trans. AIME, 1950, 188, 317; 另见文献 [21] , vol. 2, p. 122. [28] AIME: Electric Furnace Steelmaking, (Intersscience, 1963) , Vol. 2. p. 455 (Tab. 22-12) . [29] 上海市冶金工业局中心试验室、中国科学院冶金陶瓷研究所:全国转炉会议资料汇编,(上海科技出版社,1959年),第1辑,28-78页. [30] Carter, S. F.: Trans. Am. Foundrymen's Soc., 1953, 61, 52. [31] 参阅文献[1] .x |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|