| 用剩余强度法测定钴在铜中的扩散系数 |
| 钱知强;高树浚;张沛霖 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| DIFFUSION OF COBALT IN COPPER SINGLE CRYSTALS |
| TSIEN CHIH-CHIANG;KAO SHU-CHUN;CHANG PEI-LIN Institute of Metal Research; Academia Sinica |
引用本文:
钱知强;高树浚;张沛霖. 用剩余强度法测定钴在铜中的扩散系数[J]. 金属学报, 1965, 8(3): 319-325.
,
,
.
DIFFUSION OF COBALT IN COPPER SINGLE CRYSTALS[J]. Acta Metall Sin, 1965, 8(3): 319-325.
[1] Tomizuka, C. T.: Methods of Bxperimental Physics, ed. K. Lark-Horovitz, (Academic, 1959) , vol. 6, pt. A, p. 364. [2] #12. [3] Mortlock, A. J., Tomlin, D. H.: Proc. Phys. Soc., 1956, B69, 250. [4] Smith, R. L., Jaumot, F. E., Arne, L. A.: Phys. Rev., 1954, 94, 1407. [5] #12. [6] Letaw, H., Slifkin, L. M., Portnoy, W. M.: Rev. Sci. Instr., 1954, 25, 865. [7] Messner, A., Benson, R., Dorn, J. E.: Trans. Am. Soc., Metals, 1961, 53, 227. [8] Peart, R. F., Tomlin, D. H.: Acta Met., 1962, 10, 123. [9] Peart, R. F., Graham, D., Tomlin, D. H.: Acta Met., 1962, 10, 519. [10] Mackliet, C. A.: Phys. Rev., 1958, 109, 1964. [11] Sakamoto, M.: J. Phys. Soc. Japan, 1958, 13, 845. [12] Styris, D. L., Tomizuka, C. T.: J. Appl. Phys., 1963, 34, 1001. [13] Schamp, H. W., Oakes, D. A., Reed, N. M.: Rev. Sci. Instr., 1959, 30, 1028. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|