| 铜在200-900℃的氧化 |
| 李薰;骆继勋 |
|
| THE OXIDATION OF COPPER AT 200--900℃ |
| LI HSUN;LUO CHI-HSUN |
引用本文:
李薰;骆继勋. 铜在200-900℃的氧化[J]. 金属学报, 1965, 8(3): 311-420.
,
.
THE OXIDATION OF COPPER AT 200--900℃[J]. Acta Metall Sin, 1965, 8(3): 311-420.
[1] Tylecote, R. F.: J. Inst. Metals, 1950--51, 78, 259. [2] Ronnquist, A., Fischmeister, H.: J. Inst. Metals, 1960--61, 89, 65. [3] Pilling, N. B., Bedworth, R. E.: J. Inst. Metals, 1923, 29, 529. [4] Tylecote, R. F.: J. Inst. Metals, 1952--53, 81, 681. [5] Tylecote, R. F.: J. Inst. Metals 1950--51, 78, 327. [6] de Carli, F., Collari, N.: Chim. Ind. (Paris), 1951, 33, 77. [7] Bridges, D. W., Baur, J. P., Baur, G. S. et al.: J. Electrochem. Soc., 1956, 103, 475. [8] Matyas, M.: Czech. J. Phys., 1954, 4, 174. [9] Gulbransen, E. A., Copan, T. P., Anderw, K. F.: J. Electrochem. Soc., 1961, 108, 119. [10] Mott, N. F.: Trans. Faraday Soc., 1940, 36, 472. [11] Mott, N. F.: Trans. Faraday Soc., 1947, 43, 429. [12] Cabrera, N., Mott, N. F.: Rept. Progr. Phys., 1948--49, 12, 163. [13] Hauffe, K.: Oxydation von Metallen und Metallegierungen, (Springer-Verlag, Berlin, 1956) . [14] Evans, U. R.: J. Electrochem. Soc., 1947, 91, 547. [15] 李薰、郑逸苹、银耀德:金属学报,1965, 8, 221. [16] Tylecote, R. F.: J. Inst. Metals, 1950, 78, 301. [17] Castellan, G. W., Moore, W. J.: J. Chem. Phys., 1949, 17, 41. [18] Sartell, J. A., Stokes, R. J., Bendel, S. H. et al.: Trans. AIME, 1959, 215, 420. [19] Lasko, W. R., Tice, W. K.: J. Electrochem. Soc., 1962, 109, 211, [20] Takagi, R.: J. Phyt. Soc. Japan. 1957, 12, 1212. [21] Cowley, J. M.: J. Electrochem. Soc., 1954, 101, 277. [22] Von Pfefferkorn, G.: Z. Metallk., 1955, 46, 204. [23] Frank, F. C.: Phil. Mag., 1953, 44, 854. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|