| 纯铜表面张力的温度系数 |
| 严铄 |
| 中国科学院金属研究所 |
|
| THE TEMPERATURE COEFFICIENT OF SURFACE TENSION OF PURE COPPER |
| YEN SHUO Institute of Metal Research; Academia Sinica |
引用本文:
严铄. 纯铜表面张力的温度系数[J]. 金属学报, 1965, 8(2): 251-258.
.
THE TEMPERATURE COEFFICIENT OF SURFACE TENSION OF PURE COPPER[J]. Acta Metall Sin, 1965, 8(2): 251-258.
[1] Turnbull, D.: J. Chem. Phys., 1950, 18, 769. [2] Залетаева, Р. П., Крещановский, Н. С., Кунин, Л. Л.: 1951, (2) , 26. [3] Bailey, G. L. J., Watkins, H. C.: j. Inst. Metals, 1951, 80, 57. [4] Humenik, Jr. M., Parikh, N. M.: J. Am. Ceram. Soc., 1956, 39, 60. [5] Kingery, W. D.: Am. Ceram. Soc. Bull., 1956, 35, 108. [6] Уманский,Я.С,Финкельштейн,Б.Н.,Влантер,М.Е.著,中国科学院金属研究所译:金属学物理基础,(科学出版社,1958年),200页. [7] Самарин,А.М.著,邹元爔等译:钢脱氧的物理化学基础,(科学出版社,1958年),139页. [8] 陈念贻、张桂成:科学通报,1963,(3) ,68. [9] #12 [10] Quincke, G.: Ann. Phys., 1869, 138, 141. [11] Herzfeld, R.: Ann. Phys., 1897, 62, 450. [12] Holman, E. J. L.: J. Iron Steel Inst. (London), 1923, 107, 517. [13] Libman, E. E.: Phys. Rev., 1927, 29, 911. [14] Smith, S. W.: J. Inst. Metals 1914, 12, 168. [15] #12 [16] Drath, G., Sauerwald, F.: Z. Anorg. Allgem. Chem., 1927, 162, 301. [17] Krause, W., Sauerwald, F.: Z. Anorg. Allgem. Chem., 1929, 181, 353. [18] #12 [19] #12 [20] #12 [21] Becker, G., Harders, F., Kornfeld, H.: Arch. Eisenhuttenw., 1949, 363. [22] Baes, C. F., Kellogg, H. H.: Trans. AIME, 1953, 197, 643. [23] Kozakevitch, P., Chatel, S. Urbain, G. et al.: Rev. Met., 1955, 52, 139. [24] Allen, B. C., Kingery, W. D.: Trans. AIME, 1959, 215, 30. [25] #12 [26] 门间改三、须藤一:日本金属学会志,1960, 24, 374. [27] Whalen, T. J., Humenik, M. Jr.: Trans. AIME, 1960, 218, 952. [28] #12 [29] Metzger, G.: Z. Phys. Chem., 1959, 211, 1. [30] Pawlek, F., Thielsch, W., Wuth, W.: Metall, 1961, 15, 1076. [31] Gans, W., Pawlek, F., von Ropenack, A.: Z. Metallk., 1963, 54, 147. [32] Bashforth, F., Adams, S. C.: An Attempt to test the theories of capillary action (Cambridge, 1883) . [33] Urbain, G., Lucas, L. D.: The Physical Chemistry of Metallic Solutions and Intermetallic Compounds, National Physical Laboratory Symposium, (H. M. Stationery Office, 1959) , vol. 2, No. 9, 4E. [34] Hartmann, R., Schneider, R.: Z. Anorg. Allgem. Chem., 1929, 180. 275. [35] #12 [36] White, D. W. G.: Trans. Am. Soc. Metals, 1962, 55, 757. [37] Kozakevitch, P.: The Physical Chemistry of Metallic Solutions and Intermetallic Compounds, National Physical Laboratory Symposium (H. M. Stationery Office, 1959) , vol. 1, No. 9, 1E. [38] Kurkjian, C. R., Kingery, W. D.: J. Phys. Chem., 1956, 60, 961. [39] Kingery, W. D., Humenik, M. Jr.: J. Phys. Chem., 1953, 57, 359. [40] Cahill, J. A., Kirshenbaum, A. D.: J. Phys. Chem., 1962, 66. 1080. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|