| 18-8-3-1 Cr-Ni-Mo-Ti耐热钢中与δ铁素体有关的一个内耗峰 |
| 孔庆平;刘少谷 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| AN INTERNAL FRICTION PEAK RELATED TO δ-FERRITE IN A Cr-Ni-Mo-Ti HEAT-RESISTING STEEL |
| KUNG CHING-PING;LIU SHAO-KU Institute of Metal Research; Academia Sinica |
引用本文:
孔庆平;刘少谷. 18-8-3-1 Cr-Ni-Mo-Ti耐热钢中与δ铁素体有关的一个内耗峰[J]. 金属学报, 1965, 8(2): 228-231.
,
.
AN INTERNAL FRICTION PEAK RELATED TO δ-FERRITE IN A Cr-Ni-Mo-Ti HEAT-RESISTING STEEL[J]. Acta Metall Sin, 1965, 8(2): 228-231.
[1] 庄育智、李有柯:物理学报,1954,10,321. [2] 庄有智、刘嘉乐:金属学报,1956,1,337. [3] Ting-sui Ke(葛庭燧),Phys.Rev,1947,71,533. [4] Панченко,Е.В.等著,孙一唐译:金相实验室,(冶金工业出版社,1960年),456页. [5] 孔庆平:物理学报,1961,17,237. [6] Vacher, H. C., Bechtoldt, C. J.: J. Res. Natl. Bur. Std., 1954, A53, 67. [7] Zener, C.: Phys. Rev., 1947, 71, 34. [8] Li, C. Y. (李继尧), Nowick, A. S.: Acta Met., 1961, 9, 49. [9] Scraphim, D. P., Nowick, A. S.: Acta Met.. 1961, 9, 85.c |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|