1) G. W. Elmen: Bell System Tech. J., 1936, 15, 113. 2) 见Sci. Rept. Res. Inst. Tohoku Univ., 1958, A 10, 34. 1) Sucksmith, W., Thompson, J. E.: Proc. Roy. Soc. 1954, A225, 362. 1) 参阅 Aoyagi, K.: Sci. Rept. Res. Inst. Tohoku Univ., 1961, A13, 137. [1] Kelsall, G. A.: Physics, 1934, 5, 169. [2] Dillinger, J. F., Bozorth, R. M.: Physics, 1935, 6, 279. [3] Bozorth, R. M., Dillinger, J. F.: Physics, 1935, 6, 285. [4] Bozorth, R. M.: Ferromagnetism, (Van Nostrand, 1951) , p. 119. [5] Becker, J. J.: Met. Rev., 1962, 7, 371. [6] Gould, H. L. B., Wenny, D. H.: Proceedings Conference on Magnetism and Magnetic Materials, (AIEE, 1956) , p. 675. Gould, H. L. B., Wenny, D. H.: Elec. Eng., 1957, 76, 208. [7] Burket, R. E., Stewart, D. M.: J. Appl. Phys., 1962, 33, 1224. [8] Fahlenbrach, H.: Metall, 1962, 16, 1185. [9] Bozorth, R. M.: Phys. Rev., 1934, 46, 232. [10] Becker, R., Doring, W.: Ferromagnetismus, (Verlag-Springer von Jalius, 1939) , 8. 420. [11] Dahl, O., Pawlek, F.: Z. Physik., 1935, 94, 504. [12] Bozorth, R. M.: Proceedings Conference on Magnetism and Magnetic Materials, (AIEE, 1956) , p. 69. [13] Kaya, S.: J. Fac. Sci., Hokkaido Univ., 1938, 2, 29. [14] Iida, S.: J. Phys. Soc. Japan 1952, 7, 373. [15] Kaya, S.: Rev. Mod. Phys., 1953, 25, 49. [16] Chikazumi, S.: J. Phys. Soc. Japan, 1956, 11, 551. [17] Rathenau, G. W.: 文献[15] 中的讨论, 报导了Snoek & Smit的实验. [18] Ferguson, E. T.: Compt. Rend., 1957, 244, 2363. Ferguson, E. T.: J. Appl. Phys., 1958, 29, 252. [19] Snoek, J. L.: Physica, 1939, 6, 161, 797. Snoek, J. L.: Physica, 1941, 8, 711, 734. [20] Neel, L.: J. Phys. Radium, 1951, 12, 339. Neel, L: J. Phys. Radium, 1952, 13, 249. [21] Neel, L.: J. Appl. Phys., 1959, 30, 35. [22] Chikazumi, S.: J. Phys. Soc. Japan, 1950, 5, 327, 333. [23] Neel, L.: Compt. Rend., 1953, 237, 1468. [24] Neel, L.: Compt. Rend., 1953, 237, 1613. [25] Neel, L.: J. Phys. Radium, 1954, 15, 225. [26] Taniguchi, S., Yamamoto, M.: Sci Rept. Res. Inst. Tohoku Univ., 1954, A6, 330. [27] Taniguchi, S.: Sci. Rept. Res. Inst. Tohoku Univ., 1955, A7, 269. [28] Van Vleck, J. H.: Phys. Rev., 1937, 52, 1178. [29] Takahashi, M., Kono, T.: J. Phys. Soc. Japan, 1960, 15, 936. [30] Takahashi, M., Kono, T.: J. Phys. Soc. Japan, 1961, 16, 1478. [31] Graham, C. D.: J. Phys. Soc. Japan 1961, 16, 1481. [32] Seeger, A.: Z. Metallk., 1953, 44, 247. Seeger, A.: Z. Metallk., 1956, 47, 653. [33] Sambongi, T., Mitui, T.: J. Phys. Soc. Japan, 1963, 18, 1253. [34] Heidenreich, R. D., Nesbitt, E. A.: Phys. Rev., 1957, 105. 1678. [35] Heidenreich, R. D., Nesbitt, E. A., Burbank, R. D.: J. Appl. Phys, 1959, 30, 995. [36] Nesbitt, E. A., Heidenreich, R. D.: J. Appl. Phys., 1959, 30, 1000. [37] Nesbitt, E. A., Heidenreich, R. D., Williams, A. J.: J. Appl. Phys., 1960, 31, 228S. [38] Williams, H. J., Sherwood, R. C.: J. Appl. Phys., 1957, 28, 548. [39] Graram. C. D.: Magnetic Annealing, Magnetic Properties of Metals and Alloys, (ASM, 1959) , p. 288. [40] Hart, A.: Brit. J. Appl. Phys., 1960, 11. 58. [41] Birkenbell, H. J., Cahn, R. W.: J. Appl. Phys., 1961, 32, 3638. [42] Sixtus, K.: Z. Angew. Phys., 1962, 14, 241. [43] Neurath, F. W.: J. Appl Phys., 1963, 24, 1315. [44] Takahashi, M., Sasakawa, T., Fujimori, H.: J. Appl. Phys., 1964, 35, 869. [45] Adler, E. A.: Z. Angew. Phys., 1963, 15, 250. [46] Krommuller, H., Seeger, A., Schiller, P.: Z. Naturforsch., 1960, 15a, 740. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|