| 11立方米高爐冶炼庞家堡铁矿时的成渣过程 |
| 陈钧珊;周炘祥 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| AN INVESTIGATION OF THE SLAG-FORMING PROCESSES IN AN 11M~3 BLAST-FURNACE SMELTING PANG-CHIA-PAO IRON ORE |
| CHEN CHUIN-SHAN; CHOU SHENG-HSIANG(Institute of Metallurgy; Academia Sinica) |
引用本文:
陈钧珊;周炘祥. 11立方米高爐冶炼庞家堡铁矿时的成渣过程[J]. 金属学报, 1964, 7(3): 221-228.
,
.
AN INVESTIGATION OF THE SLAG-FORMING PROCESSES IN AN 11M~3 BLAST-FURNACE SMELTING PANG-CHIA-PAO IRON ORE[J]. Acta Metall Sin, 1964, 7(3): 221-228.
[1] #12 [2] #12 [3] #12 [4] #12 [5] 1952. [6] Bowen, N. L., Schairer, J. G., Posnjak, E.: Am. J. Sci., 1933, 26, 193. [7] Grerr, W. L. C.: Am. Mineralogist, 1932, 17, 135. [8] Ferguson, J. B., Buddigton, A. F.: Am. J. Sci., 1920, 50, 131. |
|