| 镍铁合金中八面体蝕坑 |
| 何开元;桂蓉麗 |
| 冶金工业部钢铁研究院;冶金工业部钢铁研究院 |
|
| THE OCTAHEDRAL ETCH PITS IN NICKEL-IRON ALLOYS |
| HO KAY-YUAN; KUEY YUNG-LEE(Iron and Steel Research Institute; The Ministry of Metallurgical Industry) |
引用本文:
何开元;桂蓉麗. 镍铁合金中八面体蝕坑[J]. 金属学报, 1964, 7(1): 104-108.
,
.
THE OCTAHEDRAL ETCH PITS IN NICKEL-IRON ALLOYS[J]. Acta Metall Sin, 1964, 7(1): 104-108.
[1] Barrett, C. S.: Structure of Metals, (McGraw-Hill, 1952) , p. 192-195. [2] Smith, D. W., Mehl, R. F.: Metals Alloys, 1933, 4, (1) , 31. [3] Lacombe, P., Beaujard, L.: J. Inst. Metals, 1947-48, 74, 1. [4] Tucker, G. E. G., Murphy, P. C.: J. Inst. Metals, 1952-53, 81, 235. [5] Seymour, W. E., Harker, D.: Trans. AIME, 1950, 188, 1001. [6] #12Z |
|