| 锰在镁-钍合金中引起的挤压强化 |
| 王干;胡素辉;陈朝荣 |
| 中国科学院冶金研究听;中国科学院冶金研究听;中国科学院冶金研究听 |
|
| ПРЕССОВАНОЕ УПРОЧНЕНИЕ МАРΓАНЦЕМ В мg-Th СПЛАВАХ |
| Ван-гань;Ху Су-хэй;Чэнь Чжо-жунь Научно-цссде(?)овамедьскц(?) цнсмцмум по мемаддурецц АН КНР |
引用本文:
王干;胡素辉;陈朝荣. 锰在镁-钍合金中引起的挤压强化[J]. 金属学报, 1963, 6(1): 65-73.
,
,
.
ПРЕССОВАНОЕ УПРОЧНЕНИЕ МАРΓАНЦЕМ В мg-Th СПЛАВАХ[J]. Acta Metall Sin, 1963, 6(1): 65-73.
[1] #12 [2] #12 [3] #12 [4] #12 [5] #12 [6] Pfann,W.G.:J.Metals,1952,4,747. [7] Tiller,W.A.,Jackson,K.A.,Rutter,J.W.,Chalmers,B.:Acta Met.,1953,1,428. [8] Rutter,J.W.,Chalmers,B.:Can.J.Phys.,1953,31,(1) ,15. [9] Hansen,M.P.:Constitution of Binary Alloys,(McGraw,1958) . [10] #12 [11] #12 [12] Suzuki,T.,Imura,T.:Report of the Conference on Defects in Crystalline Solids,(Physical Laboratory University of Bristal,Published by Physical Society,London,1954) ,p.347. [13] Elbaum,C.:Progress in Metal Physics,(Pergamon,1959) ,p.203. [14] Chalmers,B.:Physical Metallurgy,(Wiley,1960) ,p.328. [15] Morell,L.G.,Hanawalt,J.D.:J.Appl.Phys.,1932,3,161. [16] Raynor,G.V.:The Physical Metallurgy of Magnesium and its Alloys,(Pergamon,1959) ,p.224. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|