| 关于弥散强化奥氏体耐热钢的一些实验 |
| 刘民治;白福山 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| SOME EXPERIMENTS ON THE DISPERSION-STRENGTHENING AUSTENITIC HEAT-RESISTING STEEL |
| LIU MIN-CHIH;PAI FU-SHAN Institute of Metal Research;Academia Sinica |
引用本文:
刘民治;白福山. 关于弥散强化奥氏体耐热钢的一些实验[J]. 金属学报, 1963, 6(1): 59-64.
,
.
SOME EXPERIMENTS ON THE DISPERSION-STRENGTHENING AUSTENITIC HEAT-RESISTING STEEL[J]. Acta Metall Sin, 1963, 6(1): 59-64.
[1] Irmann,R.:Rev.Aluminium,1951,28,(179) ,269. [2] Bruckart,W.L.,Jaffee,R.I.:Symposium on Metallic Materials for Service at Temperatures above 1600°F.(ASM,1955) ,p.111. Robert,I.J.:The Metal Molybdenum,(ASM,1958) ,p.354-364. [3] Gatti,A.:Trans.AIME,1960,218,437. [4] Gregory,E.,Goetzel,G.:Trans.AIME,1958,212,868. [5] Blainey,A.:Metal Progr.,1958,74,(3) ,95. [6] Adkins,E.F.,Sims,C.T.,Jaffee,R.I.:Trans.AIME,1959,215,344. [7] Gatti,A.:Trans.AIME,1959,215,753. [8] Yunoshin,I.,Hiroshi,H.:Sci.Rept.Res.Inst.Tohoku Univ.,1960,A12,168. [9] Orowan,E.:Symposium on Internal Stresses in Metals and Alloys,(L M.,London,1947) ,p.451. [10] Coulomb,P.,Friedel,J.:Dislocations and Mechanical Properties of Crystals,(Wiley,1957) ,p.555. [11] Ansell,G.S.:Trans.AIME,1959,215,294. [12] Towner,R.J.:Metal Progr.,1958,73,(5) ,70. [13] Sugarman,B.:Symposium on Powder Metallurgy,(ISI,1954) ,p.175. [14] #12 [15] 刘民治等:“表面活性介质在机械加工过程中的作用”,未发表. [16] #12 [17] Ball,C.J.:Dislocations and Mechanical Properties of Crystals,(Wiley,1957) ,p.353. [18] Hart,E.W.:Relation of Properties to Microstructure,(ASM,1954) ,p.95. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|