| 液态高炉型渣中MnO的活度及还原速率 |
| 王渭源;邹元爔 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| ACTIVITY OF MnO IN LIQUID BLAST-FURNACE-TYPE SLAGS AND ITS RATE OF REDUCTION |
| WANG WEI-YUAN;CHOU YUAN-HSI Institute of Metallurgy;Academia Sinica |
引用本文:
王渭源;邹元爔. 液态高炉型渣中MnO的活度及还原速率[J]. 金属学报, 1963, 6(1): 40-50.
,
.
ACTIVITY OF MnO IN LIQUID BLAST-FURNACE-TYPE SLAGS AND ITS RATE OF REDUCTION[J]. Acta Metall Sin, 1963, 6(1): 40-50.
[1] Chou,Y.H.(邹元燨):Doctorate Thesis,Department of Metallurgy,Carnegie Institute of Technology,1947. [2] Filer,E.W.,Darken,L.S.:Trans.AIME,1952,194,253. [3] Stukel,J.E.,Cocubinsky,J.:J.Metals,1954,6,353. [4] K(o|¨)rber,F.,Oelsen,W.:Mitt.K.W.Inst.Eisenf.,1932,14,181. [5] 三本木贡治、大谷正康:铁(?)纲,1954,40,277。 [6] 王渭源、邹元燨:科学通报,1957,(9) ,287. [7] Schenck,H.,Neumann,F.:Arch.Eisenhüttenw.,1958,263. [8] Ohtani,M.:Sci.Rept.Res.Inst.Tohoku Univ.,1957,A9,426 [9] #12 [10] Chipman,J.,Fulton,J.C.,Caskey,G.R,:Acta Met.,1954,2,439. [11] Chou,Y.H.(邹元燨):Freiberger Forschungsh.,1957,B15,18. [12] Fulton,J.C.,Chipman,J.:Trans.AIME,1954. 200,1136. [13] Schenck,H.,Neumann,F.:Arch.Eisenhüttenw.,1959,705;1960,83. [14] Abraham,K.P.,Davis,M.W.,Richardson,F.D.:J.Iron Steel Inst.,1960,196,82. [15] Chang,L.C.(张禄经),Goldman,K.M.:Trans.AIME,1948,176,309. [16] McCoy,C.W.,Philbrook,W.O.:Trans.AIME,1958,212,226. [17] Fulton,J.C.,Chipman,J.:The Physical Chemistry of Steelmaking,(Wiley,1958) ,p.113. [18] #12 [19] Philbrook,W.O.,Kirkbride,L.D.:Trans.AIME,1956,206,351. [20] Tarby,S.K.,Philbrook,W.O.:J.Metals,1961,13,442. [21] 赵彭年、邹元燨:金属学报,1963,6,28。 [22] 邹元燨、赵彭年、曹兆民:待发表. [23] Kozakevitch,P.:Rev.Met.,1954,51,559. [24] Bockris,J.O'M.,Lowe,D.C.:Proc.Roy.Soc.,1954,A226,423. [25] B(?)k,T.,(O|¨)lander,A.:Acta Chem.Scand.,1955,9,1350. [26] #12 [27] Wagner,C.:The Physical Chemistry of Steelmaking,(Wiley,1958) ,p.237. [28] 王渭源:待发表. [29] 靳树梁等:现代炼铁学,(冶金工业出版社,1959年),273页. [30] 邹元燨:金属学报,1956,1,325.x |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|