| 高炉型渣中氧化钒还原的物理化学 |
| 赵彭年;邹元爔 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| PHYSICAL CHEMISTRY OF REDUCTION OF VANADIUM OXIDE FROM LIQUID BLAST-FURNACE-TYPE SLAGS |
| CHAO PENG-NIAN;CHOU YUAN-HSI Institute of Metallurgy;Academia Sinica |
引用本文:
赵彭年;邹元爔. 高炉型渣中氧化钒还原的物理化学[J]. 金属学报, 1963, 6(1): 28-39.
,
.
PHYSICAL CHEMISTRY OF REDUCTION OF VANADIUM OXIDE FROM LIQUID BLAST-FURNACE-TYPE SLAGS[J]. Acta Metall Sin, 1963, 6(1): 28-39.
[1] #12 [2] #12 [3] #12 [4] 向山 干夫:铁(?)钢,1931,17,1005. [5] #12 [6] #12 [7] 杨振古、胡廷显:钢铁,1959,(23) ,1118. [8] Filer,E.W.,Darken,L.S.:Trans.AIME,1952,194,253. [9] McCoy,C.W.,Philbrook,W.O.:Trans.AIME,1958,212,226. [10] Philbrook,W.O.,Kirkbride,L.D.:Trans.AIME,1956,206,351. [11] Fulton,J.C.,Chipman,J.:Trans.AIME,1959,215,888. [12] Wagner,C.:The Physical Chemistry of Steelmaking,(Wiley,1958) ,p.237. [13] Machin,T.S.,Yee,T.B.:J.Am.Ceram.Soc.,1948,31,200. [14] 莫培根等:待发表. [15] #12 [16] #12 [17] Tower,H.,Chipman,J.:Trans.AIME,1953,197,1455. [18] Saito,T.,Maruya,K.:Sci.Rept.Res.Inst.Tohoku Univ.,1958,A10,306. [19] 丹羽 贵知藏,日本金属学会志 1957,21,304. [20] Saito,T.,Kawai,Y.:Sci.Rept.Res.Inst.Tohoku Univ.,1953,A5,460. [21] Fulton,J.C.,Chipman,J.:Trans.AIME,1954,200,1136. [22] #12 [23] 邹元燨:金属学报,1957,2,13. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|