| 低碳钢板材夹层的鉴定及其来源的分析 |
| 庄育智;吴昌衡 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| AN INVESTIGATION ON STRIATED INCLUSIONS IN MILD STEEL PLATES |
| CHUANG YU-CHIH AND WU CHEUNG-HANG Institute of Metal Research;Academia Sinica |
引用本文:
庄育智;吴昌衡. 低碳钢板材夹层的鉴定及其来源的分析[J]. 金属学报, 1956, 1(2): 155-164.
,
.
AN INVESTIGATION ON STRIATED INCLUSIONS IN MILD STEEL PLATES[J]. Acta Metall Sin, 1956, 1(2): 155-164.
[1] Carney,D.J.and Rudolphy,E.C.,Trans.AIME,200(1954) ,1391. [2] McCance,A.,I.& S.Inst.Special Report,No.22,1938,331. [3] Rait,J.R.and Pinder,H.W.,I.& S.Inst.,154(1946) ,371. [4] #12 [5] 庄育智,吴昌衡,高矽弹簧钢中非金夹杂物的鉴定,金属研究工作报告会会刊,1954. |
|