Mechanical Properties and Electrical Conductivity of α + β Titanium Alloy Sheet Regulated by Heat Treatment
ZHANG Shuqian, MA Yingjie, WANG Qian, QI Min, HUANG Sensen, LEI Jiafeng, YANG Rui
Acta Metall Sin . 2024, (12): 1622 -1636 .  DOI: 10.11900/0412.1961.2022.00490