Phase Stability, Magnetism, and Mechanical Properties of A2BTi: First-Principles Calculations and Experimental Studies
YANG Jinhan, YAN Haile, LIU Haoxuan, ZHAO Ying, YANG Yiqiao, ZHAO Xiang, ZUO Liang
Acta Metall Sin . 2024, (12): 1701 -1709 .  DOI: 10.11900/0412.1961.2022.00412