Microstructure and Mechanical Properties of GH4169D Superalloy Fabricated by Hybrid Arc and Micro-Rolling Additive Manufacturing
ZENG Li, WANG Guilan, ZHANG Haiou, ZHAI Wenzheng, ZHANG Yong, ZHANG Mingbo
Acta Metall Sin . 2024, (
5
): 681 -690 . DOI: 10.11900/0412.1961.2022.00264