Overview

Research Progress on the Preparation of Ultrafine Conductive Patterns Using Laser-Induced Transfer Technology

  • YUAN Kang ,
  • CAO Wenxin ,
  • SUN Chunqiang ,
  • WANG Zhuochao ,
  • WANG Xiaoxiao ,
  • ZHANG Yumin ,
  • ZHU Jiaqi
Expand
  • 1 Aerospace College, Harbin Institute of Technology, Harbin 150001, China
    2 Zhengzhou Research Institute, Harbin Institute of Technology, Zhengzhou 450000, China
ZHU Jiaqi, professor, Tel: (0451)86417970, E-mail: zhujq@hit.edu.cn; CAO Wenxin, professor, Tel: 15945677968, E-mail: caowenxin@hit.edu.cn

Received date: 2025-12-22

  Revised date: 2026-01-12

  Online published: 2026-06-22

Supported by

National Natural Science Foundation of China(52102039);National Natural Science Foundation of China(52032004);Aeronautical Science Foundation of China(2022Z065077001);Heilongjiang Provincial Key Research and Development Program(GA21D001);Heilongjiang Provincial Key Research and Development Program(2023T160156);Heilongjiang Provincial Key Research and Development Program(2022ZX06C05);Heilongjiang Provincial Key Research and Development Program(2024ZX12C08);Heilongjiang Provincial Key Research and Development Program(GJLX20240001)

Abstract

The fabrication of ultrafine conductive patterns serves as a core enabling technology propelling the evolution of electronic devices toward miniaturization, flexibility, and high-density integration. Driven by the rapid development of emerging fields such as Internet of Things terminals, flexible wearable electronics, and microenergy devices, the demand for electronic devices in terms of pattern linewidth precision, cross-substrate compatibility, and complex structure adaptability continues to escalate. However, traditional fabrication techniques face inherent bottlenecks in balancing precision control, flexible adaptability, and cost-effective fabrication. Laser-induced transfer (LIT) technology, leveraging its unique advantages of high precision, noncontact processing, and broad material compatibility, has remarkably improved the resolution of ultrafine patterns and expanded cross-material adaptability. This technology provides an innovative technical solution for addressing traditional process bottlenecks in this domain. In recent years, LIT-related research has achieved substantial advancements in mechanistic elucidation, process optimization, and application extension. Nevertheless, a systematic review synthesizing its key progress and evolving trends is still lacking. Accordingly, this review systematically summarizes the current research status and future development directions of LIT technology for the fabrication of ultrafine conductive patterns. First, it traces the technological evolution of LIT from conceptual initiation to multifield practical applications, elaborating on the core transfer process of LIT and its inherent advantages in ultrafine conductive pattern fabrication. It subsequently delves into two major transfer mechanisms, namely, thermally dominated and momentum-transfer-driven mechanisms and systematically discusses the regulatory effects of critical process parameters (e.g., material intrinsic properties, laser process parameters, and the donor-receiver interface distance) on the quality of ultrafine conductive patterns. On this basis, this review conducts a comparative analysis of the performance characteristics and suitable application scenarios of multiple technical implementation routes, such as single-pulse transfer, multipulse superposition transfer, and integrated composite processes. Finally, this review systematically summarizes the typical application cases of LIT-fabricated ultrafine conductive patterns in fields including microelectronic circuit repair, high-performance sensor fabrication, flexible wearable electronics, and battery manufacturing.

Cite this article

YUAN Kang , CAO Wenxin , SUN Chunqiang , WANG Zhuochao , WANG Xiaoxiao , ZHANG Yumin , ZHU Jiaqi . Research Progress on the Preparation of Ultrafine Conductive Patterns Using Laser-Induced Transfer Technology[J]. Acta Metall Sin, 2026 , 62(8) : 1357 -1375 . DOI: 10.11900/0412.1961.2025.00417

References

[1] Ko Y, Kwon G, Choi H, et al. Cutting edge use of conductive patterns in nanocellulose-based green electronics [J]. Adv. Funct. Mater., 2023, 33: 2302785
[2] Albrecht A, Rivadeneyra A, Abdellah A, et al. Inkjet printing and photonic sintering of silver and copper oxide nanoparticles for ultra-low-cost conductive patterns [J]. J. Mater. Chem., 2016, 4C: 3546
[3] Liu X, Gong Y, Jiang Z B, et al. Flexible high-density microelectrode arrays for closed-loop brain-machine interfaces: A review [J]. Front. Neurosci., 2024, 18: 1348434
[4] Liu Z Z, Ding M L, Xie J X. Advancements in digital manufacturing for metal 3D printing [J]. Acta Metall. Sin., 2024, 60: 569
  刘壮壮, 丁明路, 谢建新. 金属3D打印数字化制造研究进展 [J]. 金属学报, 2024, 60: 569
[5] Liu S L. The preparation of microwires fine conductive patterns based on microcontact printing [D]. Beijing: Beijing Institute of Graphic Communication, 2015
  刘世丽. 微接触印刷制备微米精细导电图案的研究 [D]. 北京: 北京印刷学院, 2015
[6] Sharma E, Rathi R, Misharwal J, et al. Evolution in lithography techniques: Microlithography to nanolithography [J]. Nanomaterials, 2022, 12: 2754
[7] Nomura K I, Ushijima H, Mitsui R, et al. Screen-offset printing for fine conductive patterns [J]. Microelectron. Eng., 2014, 123: 58
[8] Liu T J, Chen J L, Zhao J, et al. Research progress on the preparation of flexible high-precision conductive patterns by inkjet printing [J]. Mater. Rev., 2022, 36: 21010127
  刘泰江, 陈俊龙, 赵 杰 等. 喷墨打印制备柔性高精度导电图案研究进展 [J]. 材料导报, 2022, 36: 21010127
[9] Zhang L C. Preface to the special issue: additive manufacturing—Expanding production horizon [J]. Acta Metall. Sin. (Engl. Lett.), 2024, 37: 1
[10] Serra P, Piqué A. Laser‐induced forward transfer: Fundamentals and applications [J]. Adv. Mater. Technol., 2019, 4: 1800099
[11] Sun C Q, Wang Z C, Ji D C, et al. Research progress of laser-induced forward transfer thin films [J]. Surf. Technol., 2022, 51(8): 30
  孙春强, 王卓超, 姬栋超 等. 激光诱导向前转移薄膜材料的研究进展 [J]. 表面技术, 2022, 51(8): 30
[12] Papazoglou S, Zergioti I. Laser induced forward transfer (LIFT) of nano-micro patterns for sensor applications [J]. Microelectron. Eng., 2017, 182: 25
[13] Delaporte P, Alloncle A P. [INVITED] Laser-induced forward transfer: A high resolution additive manufacturing technology [J]. Opt. Laser Technol., 2016, 78: 33
[14] Rehman Z U, Yang F, Wang M M, et al. Fundamentals and advances in laser-induced transfer [J]. Opt. Laser Technol., 2023, 160: 109065
[15] Fernández-Pradas J M, Serra P. Laser-induced forward transfer: A method for printing functional inks [J]. Crystals, 2020, 10: 651
[16] Levene M L, Scott R D, Siryj B W. Material transfer recording [J]. Appl. Opt., 1970, 9: 2260
[17] Bohandy J, Kim B F, Adrian F J. Metal deposition from a supported metal film using an excimer laser [J]. J. Appl. Phys., 1986, 60: 1538
[18] Bohandy J, Kim B F, Adrian F J, et al. Metal deposition at 532 nm using a laser transfer technique [J]. J. Appl. Phys., 1988, 63: 1158
[19] Bonse J, Krüger J. Structuring of thin films by ultrashort laser pulses [J]. Appl. Phys., 2023, 129A: 14
[20] Shaw Stewart J, Fardel R, Nagel M, et al. The effect of laser pulse length upon laser-induced forward transfer using a triazene polymer as a dynamic release layer [J]. J. Optoelectron. Adv. Mater., 2010, 12: 605
[21] Piqué A, Chrisey D B, Auyeung R C Y, et al. A novel laser transfer process for direct writing of electronic and sensor materials [J]. Appl. Phys., 1999, 69A: S279
[22] Fernández-Pradas J M, Colina M, Serra P, et al. Laser-induced forward transfer of biomolecules [J]. Thin Solid Films, 2004, 453-454: 27
[23] Fardel R, Nagel M, Nüesch F, et al. Fabrication of organic light-emitting diode pixels by laser-assisted forward transfer [J]. Appl. Phys. Lett., 2007, 91: 061103
[24] Kattamis N T, McDaniel N D, Bernhard S, et al. Laser direct write printing of sensitive and robust light emitting organic molecules [J]. Appl. Phys. Lett., 2009, 94: 103306
[25] Zenou M, Sa'Ar A, Kotler Z. Laser jetting of femto-liter metal droplets for high resolution 3D printed structures [J]. Sci. Rep., 2015, 5: 17265
[26] Sope?a P, Serra P, Fernández-Pradas J M. Transparent and conductive silver nanowires networks printed by laser-induced forward transfer [J]. Appl. Surf. Sci., 2019, 476: 828
[27] Palla Papavlu A, Mattle T, Temmel S, et al. Highly sensitive SnO2 sensor via reactive laser-induced transfer [J]. Sci. Rep., 2016, 6: 25144
[28] Chen F R, Bian J, Hu J L, et al. Mass transfer techniques for large-scale and high-density microLED arrays [J]. Int. J. Extrem. Manuf., 2022, 4: 042005
[29] Lee C K W, Pan Y X, Yang R L, et al. Laser-induced transfer of functional materials [J]. Top. Curr. Chem., 2023, 381: 18
[30] Li R Z, Guo L J, Liu L L, et al. Laser-induced forward transfer of silver nanoparticles for a black metal absorber [J]. Front. Phys., 2022, 10: 932050
[31] Sun W G, Ji L F, Lin Z Y, et al. 20 μm micro‐LEDs mass transfer via laser‐induced in situ nanoparticles resonance enhancement [J]. Small, 2024, 20: 2309877
[32] R?der T C, K?hler J R. Physical model for the laser induced forward transfer process [J]. Appl. Phys. Lett., 2012, 100: 071603
[33] Huang Y J, Cai W L, Chen Y H, et al. Lattice Boltzmann simulation of laser-induced transfer of liquid [J]. Acta Photon. Sin., 2018, 47: 0847016
  黄亚军, 蔡文莱, 陈英怀 等. 液体激光诱导转移的格子玻尔兹曼仿真研究 [J]. 光子学报, 2018, 47: 0847016
[34] Moreno-Labella J, Munoz-Martin D, Marquez A, et al. Simulation of direct and blister-assisted laser-induced forward transfer techniques [J]. Procedia CIRP, 2020, 94: 873
[35] Jalaal M, Li S, Schaarsberg M K, et al. Destructive mechanisms in laser induced forward transfer [J]. Appl. Phys. Lett., 2019, 114: 213703
[36] Gao T Y, Zeng Q Y, Chen B, et al. Neural network molecular dynamics study of ultrafast laser-induced melting of copper nanofilms [J]. Acta Metall. Sin., 2024, 60: 1439
  高天雨, 曾启昱, 陈 博 等. 超快激光诱导Cu薄膜熔化的神经网络分子动力学研究 [J]. 金属学报, 2024, 60: 1439
[37] Li X X, Guan Y C. Theoretical fundamentals of short pulse laser-metal interaction: A review [J]. Nanotechnol. Precis. Eng., 2020, 3: 105
[38] Murzin S P. Improvement of thermochemical processes of laser-matter interaction and optical systems for wavefront shaping [J]. Appl. Sci., 2022, 12: 12133
[39] Khorasani M, Ghasemi A, Leary M, et al. A comprehensive study on meltpool depth in laser-based powder bed fusion of Inconel 718 [J]. Int. J. Adv. Manuf. Technol., 2022, 120: 2345
[40] Liu Y, Li M X, Lu X F, et al. A novel required laser energy predicting model for laser powder bed fusion [J]. Metals, 2021, 11: 1966
[41] Obilor A F, Pacella M, Wilson A, et al. Micro-texturing of polymer surfaces using lasers: A review [J]. Int. J. Adv. Manuf. Technol., 2022, 120: 103
[42] Shugaev M V, He M, Levy Y, et al. Laser-induced thermal processes: Heat transfer, generation of stresses, melting and solidification, vaporization, and phase explosion [A]. Sugioka K. Handbook of Laser Micro-and Nano-Engineering [M]. Cham: Springer, 2020: 1
[43] Harris S B, Paiste J H, Edoki J, et al. Experimentally constrained multidimensional simulation of laser-generated plasmas and its application to UV nanosecond ablation of Se and Te [J]. Plasma Sources Sci. Technol., 2021, 30: 105013
[44] Dahotre N B, Harimkar S P. Laser Fabrication and Machining of Materials [M]. New York: Springer, 2008: 34
[45] Aykac E, Turkmen M. Investigation of the biocompatibility of laser treated 316L stainless steel materials [J]. Coatings, 2022, 12: 1821
[46] Keldysh L V. Ionization in the field of a strong electromagnetic wave [J]. Sov. Phys. JETP, 1965, 20: 1307
[47] Gamaly E G, Rode A V. Transient optical properties of dielectrics and semiconductors excited by an ultrashort laser pulse [J]. J. Opt. Soc. Am., 2014, 31B: C36
[48] Amoako G. Femtosecond laser structuring of materials: A review [J]. Appl. Phys. Res., 2019, 11: 1
[49] Kuznetsov A I, Koch J, Chichkov B N. Nanostructuring of thin gold films by femtosecond lasers [J]. Appl. Phys., 2009, 94A: 221
[50] Rapp L, Cibert C, Nénon S, et al. Improvement in semiconductor laser printing using a sacrificial protecting layer for organic thin-film transistors fabrication [J]. Appl. Surf. Sci., 2011, 257: 524
[51] Fan C H, Longtin J P. Modeling optical breakdown in dielectrics during ultrafast laser processing [J]. Appl. Opt., 2001, 40: 3124
[52] Sun C Q, Wang Z C, Cao W X, et al. Preparation of brittle ITO microstructures using laser-induced forward transfer technology [J]. Chem. Eng. J., 2024, 496: 153745
[53] Kuznetsov A I, Koch J, Chichkov B N. Laser-induced backward transfer of gold nanodroplets [J]. Opt. Express, 2009, 17: 18820
[54] Gorodesky N, Sedghani-Cohen S, Fogel O, et al. Printed Cu-Ag phases using laser-induced forward transfer [J]. Adv. Eng. Mater., 2022, 24: 2100952
[55] Serra P, Colina M, Fernández-Pradas J M, et al. Preparation of functional DNA microarrays through laser-induced forward transfer [J]. Appl. Phys. Lett., 2004, 85: 1639
[56] Paris G, Heidepriem J, Tsouka A, et al. Automated laser-transfer synthesis of high-density microarrays for infectious disease screening [J]. Adv. Mater., 2022, 34: 2200359
[57] Zywietz U, Evlyukhin A B, Reinhardt C, et al. Laser printing of silicon nanoparticles with resonant optical electric and magnetic responses [J]. Nat. Commun., 2014, 5: 3402
[58] Springer M, Düsing J, Koch J, et al. Laser-induced forward transfer as a potential alternative to pick-and-place technology when assembling semiconductor components [J]. J. Laser Appl., 2021, 33: 042030
[59] Boutopoulos C, Pandis C, Giannakopoulos K, et al. Polymer/carbon nanotube composite patterns via laser induced forward transfer [J]. Appl. Phys. Lett., 2010, 96: 041104
[60] Bonciu A F, Andrei F, Palla-Papavlu A. Fabrication of hybrid electrodes by laser-induced forward transfer for the detection of Cu2? ions [J]. Materials, 2023, 16: 1744
[61] Munoz-Martin D, Brasz C F, Chen Y, et al. Laser-induced forward transfer of high-viscosity silver pastes [J]. Appl. Surf. Sci., 2016, 366: 389
[62] Sope?a P, Fernández-Pradas J M, Serra P. Laser-induced forward transfer of conductive screen-printing inks [J]. Appl. Surf. Sci., 2020, 507: 145047
[63] Visser C W, Pohl R, Sun C, et al. Toward 3D printing of pure metals by laser-induced forward transfer [J]. Adv. Mater., 2015, 27: 4087
[64] Fogel O, Cohen S S, Kotler Z, et al. Mechanical properties of 3D metallic microstructures printed by laser induced forward transfer [J]. Procedia CIRP, 2018, 74: 285
[65] Nastulyavichus A, Kudryashov S, Shelygina S, et al. One-step non-contact additive LIFT printing of silver interconnectors for flexible printed circuits [J]. Photonics, 2024, 11: 119
[66] Campagnoli M R, Galati M, Saboori A. On the processability of copper components via powder-based additive manufacturing processes: Potentials, challenges and feasible solutions [J]. J. Manuf. Processes, 2021, 72: 320
[67] Chang J L, Sun X M. Laser-induced forward transfer based laser bioprinting in biomedical applications [J]. Front. Bioeng. Biotechnol., 2023, 11: 1255782
[68] Myronyuk O, Baklan D, Rodin A M. UV resistance of super-hydrophobic stainless steel surfaces textured by femtosecond laser pulses [J]. Photonics, 2023, 10: 1005
[69] Cheng S K, Wu D, Luo G H, et al. Effect of pulse duration on laser-induced forward transfer of microdroplets [J]. Laser Optoelectron. Prog., 2023, 60: 1914001
  程帅康, 吴 迪, 罗国虎 等. 脉冲宽度对激光驱动微滴前向转移的影响 [J]. 激光与光电子学进展, 2023, 60: 1914001
[70] Link S, El-Sayed M A. Shape and size dependence of radiative, non-radiative and photothermal properties of gold nanocrystals [J]. Int. Rev. Phys. Chem., 2000, 19: 409
[71] Zhu L, Gao Y Y, Hu X Y, et al. Progress in femtosecond laser fabrication of artificial compound eye [J]. Chin. Sci. Bull., 2019, 64: 1254
  朱 琳, 高圆圆, 胡昕宇 等. 飞秒激光仿生复眼制造进展 [J]. 科学通报, 2019, 64: 1254
[72] Subhan A, Mourad A H I, Al-Douri Y. Influence of laser process parameters, liquid medium, and external field on the synthesis of colloidal metal nanoparticles using pulsed laser ablation in liquid: A review [J]. Nanomaterials, 2022, 12: 2144
[73] Zhang Y M, Tian C X, Yu Y C, et al. Morphological characteristics and printing mechanisms of grid lines by laser-induced forward transfer [J]. Metals, 2022, 12: 2090
[74] Shah A. Interference assisted laser induced forward transfer for line patterning [D]. Montreal: Concordia University, 2008
[75] Romano J M, Helbig R, Fraggelakis F, et al. Springtail-inspired triangular laser-induced surface textures on metals using MHz ultrashort pulses [J]. J. Micro Nano-Manuf., 2019, 7: 024504
[76] Schille J, Schneider L, Mueller M, et al. Highspeed laser micro processing using ultrashort laser pulses [J]. JLMN-J. Laser Micro/Nanoeng., 2014, 9: 161
[77] Yang L. Studies on depositing of metal film by femtosecond laser induce forword transfer [D]. Tianjin: Tianjin University, 2007
  杨 丽. 飞秒激光微精细加工—微量物质转移研究 [D]. 天津: 天津大学, 2007
[78] Biswas S, Karthikeyan A, Kietzig A M. Effect of repetition rate on femtosecond laser-induced homogenous microstructures [J]. Materials, 2016, 9: 1023
[79] Xu H Z, Yuan X F, Zhang Z, et al. Numerical simulation of the irradiation damage on metal films by single UV laser pulse [J]. Opt. Instrum., 2017, 39(4): 77
  徐海钊, 原晓峰, 张 哲 等. 紫外激光单脉冲辐照损伤金属薄膜的数值模拟研究 [J]. 光学仪器, 2017, 39(4): 77
[80] Wei C, Zhang Z Z, Cheng D X, et al. An overview of laser-based multiple metallic material additive manufacturing: From macro-to micro-scales [J]. Int. J. Extrem. Manuf., 2021, 3: 012003
[81] Smits E C P, Walter A, de Leeuw D M, et al. Laser induced forward transfer of graphene [J]. Appl. Phys. Lett., 2017, 111: 173101
[82] Chen Y. Desarrollo de procesos para formación de contactos con láser para módulos thin film CIGS para aplicaciones fotovoltaicas [D]. Madrid: Universidad Politécnica de Madrid, 2016
[83] Ruffino F, Grimaldi M G. Nanostructuration of thin metal films by pulsed laser irradiations: A review [J]. Nanomaterials, 2019, 9: 1133
[84] Zenou M, Kotler Z. Printing of metallic 3D micro-objects by laser induced forward transfer [J]. Opt. Express, 2016, 24: 1431
[85] Reiser A, Koch L, Dunn K A, et al. Metals by micro-scale additive manufacturing: Comparison of microstructure and mechanical properties [J]. Adv. Funct. Mater., 2020, 30: 1910491
[86] Lim J, Kim Y, Shin J, et al. Continuous-wave laser-induced transfer of metal nanoparticles to arbitrary polymer substrates [J]. Nanomaterials, 2020, 10: 701
[87] Lee B G. Improvement of conductive micro-pattern fabrication using a LIFT process [J]. J. Korea Acad.-Ind. Coop. Soc., 2017, 18: 475
[88] Kuznetsov A I, Evlyukhin A B, Gon?alves M R, et al. Laser fabrication of large-scale nanoparticle arrays for sensing applications [J]. ACS Nano, 2011, 5: 4843
[89] Orbotech, Inc. Flat Panel Display—FPD/Repair [EB/OL]. [2026-06-18]. https://www.orbotech.com/fpd/array-repair-systems.
[90] Chen X D, Liu Z B, Jiang W S, et al. The selective transfer of patterned graphene [J]. Sci. Rep., 2013, 3: 3216
[91] MODUS Research and Innovation. HiperLAM: High performance laser additive manufacturing [EB/OL]. [2026-06-18]. https://modus.ltd/our-projects/horizon-2020/hiperlam/.
[92] Touloupakis E, Boutopoulos C, Buonasera K, et al. A photosynthetic biosensor with enhanced electron transfer generation realized by laser printing technology [J]. Anal. Bioanal. Chem., 2012, 402: 3237
[93] Liang S Y, Liu Y F, Ji Z K, et al. High-resolution patterning of perovskite quantum dots via femtosecond laser-induced forward transfer [J]. Nano Lett., 2023, 23: 3769
[94] Sope?a P, Arrese J, González-Torres S, et al. Low-cost fabrication of printed electronics devices through continuous wave laser-induced forward transfer [J]. ACS Appl. Mater. Interfaces, 2017, 9: 29412
[95] Piqué A, Auyeung R C Y, Kim H, et al. Laser 3D micro-manufacturing [J]. J. Phys., 2016, 49D: 223001
[96] Heidmann B, Andree S, Levcenko S, et al. Fabrication of regularly arranged chalcopyrite micro solar cells via femtosecond laser-induced forward transfer for concentrator application [J]. ACS Appl. Energy Mater., 2018, 1: 27
[97] Guillotin B, Souquet A, Catros S, et al. Laser assisted bioprinting of engineered tissue with high cell density and microscale organization [J]. Biomaterials, 2010, 31: 7250
[98] Kaur K S, Missinne J, Van Steenberge G. Flip-chip bonding of vertical-cavity surface-emitting lasers using laser-induced forward transfer [J]. Appl. Phys. Lett., 2014, 104: 061102
[99] Luo J, Pohl R, Qi L H, et al. Printing functional 3D microdevices by laser-induced forward transfer [J]. Small, 2017, 13: 1602553
Outlines

/