Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors
Received date: 2025-07-15
Revised date: 2025-09-03
Online published: 2025-12-18
Supported by
Strategic Priority Research Program of Chinese Academy of Sciences(XDA0410000);LingChuang Research Project of China National Nuclear Corporation
Austenitic stainless steels are utilized in the in-core and out-of-core structural components of various Generation-IV nuclear reactors owing to their excellent comprehensive properties, mature manufacturing processes, and decades of service experience in pressurized water reactors. However, after prolonged exposure to high temperature and high-intensity irradiation, these steels gradually exhibit some performance limitations, including lower creep strength, inadequate microstructural stabilities, and higher radiation embrittlement sensitivities. Recently, alloying with Nb has been proven to effectively regulate the precipitation behavior of secondary phases and the formation and evolution of irradiation defects in austenitic stainless steels, promising simultaneous improvements in creep strength and irradiation tolerance. Therefore, Nb alloying has emerged as a key pathway for the development of next-generation austenitic stainless steels with enhanced high-temperature performance, improved irradiation resistance, and extended service life. This paper systematically reviews the research progress of Nb-stabilized austenitic stainless steels for Generation-IV nuclear power applications, including the compositional design and optimization to improve the creep properties and irradiation resistance, the effects of Nb addition on austenite stability, the formation mechanisms of primary NbC, and the precipitation behavior of Nb-bearing secondary phases. Additionally, the mechanisms by which Nb alloying influences the strength-ductility balance, creep strength, high-temperature microstructural stability, and irradiation-induced defect evolution are discussed. Finally, some future research prospects of Nb-stabilized austenitic stainless steels for Generation-IV nuclear reactors are discussed.
CHEN Shenghu , XIE Ang , YANG Binbin , LIU Yongtao , CHEN Sihan , ZHAO Mingjiu , JIANG Haichang , RONG Lijian . Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors[J]. Acta Metall Sin, 2026 , 62(7) : 1175 -1188 . DOI: 10.11900/0412.1961.2025.00203
| [1] | Buckthorpe D. Introduction to Generation IV nuclear reactors [A]. Structural Materials for Generation IV Nuclear Reactors [M]. Amsterdam: Woodhead Publishing, 2017: 1 |
| [2] | Kelly J E. Generation IV International Forum: A decade of progress through international cooperation [J]. Prog. Nucl. Energy, 2014, 77: 240 |
| [3] | Locatelli G, Mancini M, Todeschini N. Generation IV nuclear reactors: Current status and future prospects [J]. Energy Policy, 2013, 61: 1503 |
| [4] | Pioro I L, Rodriguez G H. Generation IV international forum (GIF) [A]. Handbook of Generation IV Nuclear Reactors [M]. Cambridge: Woodhead Publishing, 2023: 111 |
| [5] | China Nuclear Energy Association, Hualong Nuclear Power Technology Co., Ltd. Blue Book of China Nuclear Energy Development Report [M]. Beijing: Scientific and Technical Documentaton Press, 2025: 1 |
| 中国核能行业协会, 华龙国际核电技术有限公司. 中国核能科技创新发展报告 [M]. 北京: 科学技术文献出版社, 2025: 1 | |
| [6] | Abram T, Ion S. Generation-IV nuclear power: A review of the state of the science [J]. Energy Policy, 2008, 36: 4323 |
| [7] | Lorusso P, Bassini S, Del Nevo A, et al. GEN-IV LFR development: Status perspectives [J]. Prog. Nucl. Energy, 2018, 105: 318 |
| [8] | Magwood IV W D, Paillere H. Looking ahead at reactor development [J]. Prog. Nucl. Energy, 2018, 102: 58 |
| [9] | Serp J, Allibert M, Bene? O, et al. The molten salt reactor (MSR) in generation IV: Overview and perspectives [J]. Prog. Nucl. Energy, 2014, 77: 308 |
| [10] | Guérin Y, Was G S, Zinkle S J. Materials challenges for advanced nuclear energy systems [J]. MRS Bull., 2009, 34: 10 |
| [11] | Yvon P, Carré F. Structural materials challenges for advanced reactor systems [J]. J. Nucl. Mater., 2009, 385: 217 |
| [12] | Murty K L, Charit I. Structural materials for Gen-IV nuclear reactors: Challenges and opportunities [J]. J. Nucl. Mater., 2008, 383: 189 |
| [13] | Gong X, Short M P, Auger T, et al. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors [J]. Prog. Mater. Sci., 2022, 126: 100920 |
| [14] | Yvon P, Le Flem M, Cabet C, et al. Structural materials for next generation nuclear systems: Challenges and the path forward [J]. Nucl. Eng. Des., 2015, 294: 161 |
| [15] | Mansur L K, Rowcliffe A F, Nanstad R K, et al. Materials needs for fusion, Generation IV fission reactors and spallation neutron sources—Similarities and differences [J]. J. Nucl. Mater., 2004, 329-333: 166 |
| [16] | Samaras M, Hoffelner W, Victoria M. Modelling of advanced structural materials for GEN IV reactors [J]. J. Nucl. Mater., 2007, 371: 28 |
| [17] | Maloy S A, Natesan K, Holcomb D E, et al. Overview of reactor systems and operational environments for structural materials in gen-IV fission reactors [A]. Structural Alloys for Nuclear Energy Applications [M]. Amsterdam: Elsevier, 2019: 23 |
| [18] | Was G S, Ukai S. Austenitic stainless steels [A]. Structural Alloys for Nuclear Energy Applications [M]. Amsterdam: Elsevier, 2019: 293 |
| [19] | Cheon J S, Lee C B, Lee B O, et al. Sodium fast reactor evaluation: Core materials [J]. J. Nucl. Mater., 2009, 392: 324 |
| [20] | Klueh R L. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors [J]. Int. Mater. Rev., 2005, 50: 287 |
| [21] | Chen S H, Rong L J. Oxide scale formation on ultrafine-grained ferritic-martensitic steel during pre-oxidation and its effect on the corrosion performance in stagnant liquid Pb-Bi eutectic [J]. Acta Metall. Sin., 2021, 57: 989 |
| 陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响 [J]. 金属学报, 2021, 57: 989 | |
| [22] | Zhao Y Y, Ding S A, Du Y Y, et al. Effect of long-term thermal aging on lead-bismuth eutectic corrosion behavior of 9Cr ferritic/martensitic steel [J]. J. Mater. Sci. Technol., 2025, 210: 299 |
| [23] | Liu S J, Huang Q Y, Peng L, et al. Microstructure and its influence on mechanical properties of CLAM steel [J]. Fusion Eng. Des., 2012, 87: 1628 |
| [24] | Ma Z W, Zhou T, Jin P, et al. Influence of temperature on the microstructural evolution of SIMP and T91 steels in liquid lead-bismuth eutectic: Experiments and molecular dynamics simulations [J]. Corros. Sci., 2023, 222: 111411 |
| [25] | Yang K, Yan W, Wang Z G, et al. Development of a novel structural material (SIMP steel) for nuclear equipment with balanced resistances to high temperature, radiation and liquid metal corrosion [J]. Acta Metall. Sin., 2016, 52: 1207 |
| 杨 柯, 严 伟, 王志光 等. 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展 [J]. 金属学报, 2016, 52: 1207 | |
| [26] | Chen S H, Xie A, Lv X L, et al. Tailoring microstructure of austenitic stainless steel with improved performance for generation-IV fast reactor application: A review [J]. Crystals, 2023, 13: 268 |
| [27] | Wu X Q, Rong L J, Tan J B, et al. Research advance on liquid lead-bismuth eutectic corrosion resistant Si enhanced ferritic/martensitic and austenitic stainless steels [J]. Acta Metall. Sin., 2023, 59: 502 |
| 吴欣强, 戎利建, 谭季波 等. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展 [J]. 金属学报, 2023, 59: 502 | |
| [28] | Jayakumar T, Mathew M D, Laha K, et al. Materials development for fast reactor applications [J]. Nucl. Eng. Des., 2013, 265: 1175 |
| [29] | Maziasz P J, Busby J T. Properties of austenitic steels for nuclear reactor applications [J]. Compr. Nucl. Mater. (Second Ed.), 2020, 7: 303 |
| [30] | Maziasz P J. Overview of microstructural evolution in neutron-irradiated austenitic stainless steels [J]. J. Nucl. Mater., 1993, 205: 118 |
| [31] | Chen L L, Luo R, Gao P, et al. Dynamic recrystallization behavior and coincidence site lattice evolution in thermal deformation of 316H stainless steel used in nuclear systems [J]. J. Iron Steel Res. Int., 2023, 30: 1862 |
| [32] | Mathew M D. Evolution of creep resistant 316 stainless steel for sodium cooled fast reactor applications [J]. Trans. Indian Inst. Met., 2010, 63: 151 |
| [33] | Karthik V, Murugan S, Parameswaran P, et al. Austenitic stainless steels for fast reactors-irradiation experiments, property evaluation and microstructural studies [J]. Energy Procedia, 2011, 7: 257 |
| [34] | Lai J K L, Chastell D J, Flewitt P E J. Precipitate phases in type 316 austenitic stainless steel resulting from long-term high temperature service [J]. Mater. Sci. Eng., 1981, 49: 19 |
| [35] | Vach M, Kuníková T, Dománková M, et al. Evolution of secondary phases in austenitic stainless steels during long-term exposures at 600, 650 and 800 oC [J]. Mater. Charact., 2008, 59: 1792 |
| [36] | Lv X L, Chen S H, Rong L J. Evolution of precipitate and its effect on the degradation of impact toughness in a carbon and nitrogen-controlled 316 stainless steel during thermal aging at 650 oC [J]. J. Mater. Res. Technol., 2024, 33: 3728 |
| [37] | Xie A, Chen S H, Yin L C, et al. Microstructural evolution of the inner oxide layer of a Si-modified austenitic stainless steel exposed to oxygen-saturated lead-bismuth eutectic (LBE): Toward the origin of LBE penetration [J]. Corros. Sci., 2024, 237: 112350 |
| [38] | Padilha A F, Escriba D M, Materna-Morris E, et al. Precipitation in AISI 316L(N) during creep tests at 550 and 600 oC up to 10 years [J]. J. Nucl. Mater., 2007, 362: 132 |
| [39] | Padilha A F, Rios P R. Decomposition of austenite in austenitic stainless steels [J]. ISIJ Int., 2002, 42: 325 |
| [40] | Sourmail T. Precipitation in creep resistant austenitic stainless steels [J]. Mater. Sci. Technol., 2001, 17: 1 |
| [41] | The American Society of Mechanical Engineers. Boiler and pressure vessel code, section III: Rules for construction of nuclear power plant components, division 1, subsection NH: Class 1 components in elevated temperature service [S]. New York: ASME, 2015 |
| [42] | Zinkle S J. Radiation-induced effects on microstructure [A]. Comprehensive Nuclear Materials [M]. Amsterdam: Elsevier, 2012: 65 |
| [43] | Was G S. Irradiation-induced voids and bubbles [A]. Fundamentals of Radiation Materials Science: Metals and Alloys [M]. New York: Springer, 2017: 379 |
| [44] | Keown S R, Pickering F B. Niobium in stainless steels [A]. Proceedings of the International Symposium—Niobium 81 [C]. San Francisco, 1981: 1113 |
| [45] | Williams T M, Titchmarsh J M, Arkell D R. Void-swelling and precipitation in a neutron-irradiated, niobium-stabilised austenitic stainless steel [J]. J. Nucl. Mater., 1982, 107: 222 |
| [46] | Meng F M, Fu J Y. Modern Niobium Containing Stainless Steel [M]. Beijing: Metallurgical Industry Press, 2004: 1 |
| 孟繁茂, 付俊岩. 现代含铌不锈钢 [M]. 北京: 冶金工业出版社, 2004: 1 | |
| [47] | Wang Q Y, Chen S H, Rong L J. δ-ferrite formation and its effect on the mechanical properties of heavy-section AISI 316 stainless steel casting [J]. Metall. Mater. Trans., 2020, 51A: 2998 |
| [48] | Wang Q Y, Chen S H, Lv X L, et al. Role of δ-ferrite in fatigue crack growth of AISI 316 austenitic stainless steel [J]. J. Mater. Sci. Technol., 2022, 114: 7 |
| [49] | Chen S H, Wang Q Y, Jiang H C, et al. Effect of δ-ferrite on hot deformation and recrystallization of 316KD austenitic stainless steel for sodium-cooled fast reactor application [J]. Acta Metall. Sin., 2024, 60: 367 |
| 陈胜虎, 王琪玉, 姜海昌 等. δ-铁素体对钠冷快堆用316KD奥氏体不锈钢热变形行为和动态再结晶的影响 [J]. 金属学报, 2024, 60: 367 | |
| [50] | Xie A, Chen S H, Chen S H, et al. Austenite decomposition behavior adjacent to δ-ferrite in a Si-modified Fe-Cr-Ni austenitic stainless steel during thermal aging at 550 oC [J]. Acta Mater., 2024, 272: 119948 |
| [51] | Chen Y K, Wei S T, Wu D, et al. Mechanism of δ-ferrite decomposition in high Si-bearing austenitic stainless steel weld metal during aging at 550 oC [J]. Mater. Sci. Eng., 2023, A876: 145163 |
| [52] | Chen S H, Wang Q Y, Xie A, et al. Corrosion behavior of δ-ferrite in AISI 316 austenitic stainless steel exposed to oxygen-saturated lead-bismuth eutectic at 550 oC [J]. Mater. Charact., 2024, 211: 113930 |
| [53] | de Bellefon G M, van Duysen J C, Sridharan K. Composition-dependence of stacking fault energy in austenitic stainless steels through linear regression with random intercepts [J]. J. Nucl. Mater., 2017, 492: 227 |
| [54] | Martinez L G, Imakuma K, Padilha A F. Influence of niobium on stacking-fault energy of all-austenite stainless steels [J]. Steel Res., 1992, 63: 221 |
| [55] | Lu S, Hu Q M, Johansson B, et al. Stacking fault energies of Mn, Co and Nb alloyed austenitic stainless steels [J]. Acta Mater., 2011, 59: 5728 |
| [56] | Xie A, Chen S H, Jiang H C, et al. Effects of Nb content and homogenization treatment on the microstructure and mechanical properties of cast austenitic stainless steel [J]. Acta Metall. Sin., 2025, 61: 1035 |
| 谢 昂, 陈胜虎, 姜海昌 等. Nb含量和均质化处理对奥氏体不锈钢铸态组织和力学性能的影响 [J]. 金属学报, 2025, 61: 1035 | |
| [57] | Wang J Q, Wu J R, Yao Z Q, et al. Mechanistic insights into the dual role of NbC in strength-toughness synergy of nuclear grade Fe-Ni-based alloys [J]. J. Mater. Res. Technol., 2025, 39: 6806 |
| [58] | Zhang X, Li D Z, Li Y Y, et al. The influence of niobium on the plastic deformation behaviors of 310s austenitic stainless steel weld metals at different temperatures [J]. Mater. Sci. Eng., 2019, A743: 648 |
| [59] | Wu Y, Xie A, Chen S H, et al. Corrosion behavior of NbC and its effect on corrosion layer formation in liquid lead-bismuth eutectic of Nb-containing austenitic stainless steel [J]. Acta Metall. Sin., 2025, 61: 287 |
| 吴 炀, 谢 昂, 陈胜虎 等. 含Nb奥氏体不锈钢中NbC的液态Pb-Bi共晶腐蚀行为及其对氧化层形成的影响 [J]. 金属学报, 2025, 61: 287 | |
| [60] | Takechi H, Hasimoto S, Imagumbai M, translated by Fu J Y, Shang C J. How to Improve the Properties of Steel with Niobium: Production Technology of Niobium-Containing Steel [M]. Beijing: Metallurgical Industry Press, 2007: 1 |
| Takechi H, Hasimoto S, Imagumbai M著, 付俊岩, 尚成嘉译. 如何用铌改善钢的性能 : 含铌钢生产技术 [M]. 北京: 冶金工业出版社, 2007:1 | |
| [61] | Akahori K, Maeno S, Kodama H, et al. Prediction of the formation region of eutectic NbC in a large 12Cr-Mo-V-Nb steel ingot [J]. Tetsu-to-Hagané, 1985, 71: 78 |
| 赤堀 公彦, 前野 茂夫, 児玉 英世 等. 12Cr-Mo-V-Nb鋼大形鋼塊中の共晶NbCの発生領域の予測 [J]. 鉄と鋼, 1985, 71: 78 | |
| [62] | Xie A, Chen S H, Wu Y, et al. Homogenization temperature dependent microstructural evolution and mechanical properties in a Nb-stabilized cast austenitic stainless steel [J]. Mater. Charact., 2022, 194: 112384 |
| [63] | Nordberg H, Aronsson B. Solubility of niobium carbide in austenite [J]. J. Iron Steel Inst., 1968, 206: 1263 |
| [64] | Japan Society of Mechanical Engineers. Code for Nuclear Power Generation Facilities. Rules on Design and Construction for Nuclear Power Plants. Section II Fast Reactor Standards [S]. Tokyo: JSME, 2017 |
| 日本機械学会. 発電用原子力設備規格 設計?建設規格(2016年)第II編高速炉規格 [S]. 東京: 日本機械学会, 2017 | |
| [65] | AFCEN. Design and Construction Rules for Mechanical Components of Nuclear Installations: High temperature research and fusion reactors [S]. RCC-MRx, 2015 |
| [66] | Solenthaler C, Ramesh M, Uggowitzer P J, et al. Precipitation strengthening of Nb-stabilized TP347 austenitic steel by a dispersion of secondary Nb(C,N) formed upon a short-term hardening heat treatment [J]. Mater. Sci. Eng., 2015, A647: 294 |
| [67] | Shin J H, Kim H S, Kong B S, et al. Development of thermo-mechanical processing to form high density of uniformly distributed nanosized carbides in austenitic stainless steels [J]. Mater. Sci. Eng., 2020, A775: 138986 |
| [68] | Shin J H, Kong B S, Eom H J, et al. Dynamic evolution of nanosized NbC precipitates in austenite matrix during deformation and its contribution to strengthening [J]. Mater. Sci. Eng., 2021, A806: 140816 |
| [69] | Zhao W X, Jiang S H, Liu W H, et al. Synergistic effects of microalloying and pre-straining on enhanced nanoprecipitation and creep property of alumina-forming austenitic stainless steels [J]. Mater. Sci. Eng., 2022, A857: 143995 |
| [70] | Mu R, Wang Y J, Song R B, et al. Constructing high-density dislocations by primary (Nb,Ti)(C,N) to induce massive secondary precipitations in austenitic heat-resistant cast steel [J]. Mater. Charact., 2024, 212: 113968 |
| [71] | Ha V T, Jung W S, Suh J Y. Improved creep behavior of a high nitrogen Nb-stabilized 15Cr-15Ni austenitic stainless steel strengthened by multiple nanoprecipitates [J]. Metall. Mater. Trans., 2011, 42A: 3378 |
| [72] | Ha V T, Jung W S. Creep behavior and microstructure evolution at 750 oC in a new precipitation-strengthened heat-resistant austenitic stainless steel [J]. Mater. Sci. Eng., 2012, A558: 103 |
| [73] | Yang Y H, Zhu L H, Wang Q J, et al. Microstructural evolution and the effect on hardness and plasticity of S31042 heat-resistant steel during creep [J]. Mater. Sci. Eng., 2014, A608: 164 |
| [74] | Li Y M, Liu Y C, Liu C X, et al. Mechanism for the formation of Z-phase in 25Cr-20Ni-Nb-N austenitic stainless steel [J]. Mater. Lett., 2018, 233: 16 |
| [75] | Erneman J, Schwind M, Liu P, et al. Precipitation reactions caused by nitrogen uptake during service at high temperatures of a niobium stabilised austenitic stainless steel [J]. Acta Mater., 2004, 52: 4337 |
| [76] | Ding R G, Yan J, Li H Y, et al. Microstructural evolution of Alloy 709 during aging [J]. Mater. Charact., 2019, 154: 400 |
| [77] | Maziasz P J. Development of creep-resistant and oxidation-resistant austenitic stainless steels for high temperature applications [J]. JOM, 2018, 70: 66 |
| [78] | Zhou Y H, Liu Y C, Zhou X S, et al. Precipitation and hot deformation behavior of austenitic heat-resistant steels: A review [J]. J. Mater. Sci. Technol., 2017, 33: 1448 |
| [79] | Wang H T, Du H Y, Wei Y H, et al. Precipitation and properties at elevated temperature in austenitic heat-resistant steels—A review [J]. Steel Res. Int., 2021, 92: 2000378 |
| [80] | Dalle F, Blat-Yrieix M, Dubiez-Le Goff S, et al. Conventional austenitic steels as out-of-core materials for Generation IV nuclear reactors [A]. Structural Materials for Generation IV Nuclear Reactors [M]. Amsterdam: Woodhead Publishing, 2017: 595 |
| [81] | Powell D J, Pilkington R, Miller D A. The precipitation characteristics of 20% Cr/25% Ni-Nb stabilised stainless steel [J]. Acta Metall., 1988, 36(3): 713 |
| [82] | Vaché N, Steyer P, Duret-Thual C, et al. Microstructural study of the NbC to G-phase transformation in HP-Nb alloys [J]. Materialia, 2020, 9: 100593 |
| [83] | Zhang S Z, Shi X B, Su Y F, et al. G phase and ferrite in a high Si austenitic stainless steel during 510 oC aging [J]. Mater. Charact., 2024, 207: 113587 |
| [84] | Su Y F, Zhang S Z, Jiao S X, et al. Microstructural stability of L12-strengthened Si-modified Fe-Cr-Ni alloy during 510-600 oC thermal aging [J]. J. Mater. Sci. Technol., 2026, 244: 246 |
| [85] | Chen Y K, Wu D, Li D Z, et al. Effects of stabilization heat treatment on microstructure and mechanical properties of Si-bearing 15Cr-9Ni-Nb austenitic stainless steel weld metal [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 637 |
| [86] | Hu G D, Wang P, Li D Z, et al. Precipitate evolution in a modified 25Cr-20Ni austenitic heat resistant stainless steel during creep rupture test at 750 oC [J]. Acta Metall. Sin., 2018, 54: 1705 |
| 胡国栋, 王 培, 李殿中 等. 新型25Cr-20Ni奥氏体耐热不锈钢750 ℃持久实验过程中析出相演变 [J]. 金属学报, 2018, 54: 1705 | |
| [87] | Perron A, Toffolon-Masclet C, Ledoux X, et al. Understanding sigma-phase precipitation in a stabilized austenitic stainless steel (316Nb) through complementary CALPHAD-based and experimental investigations [J]. Acta Mater., 2014, 79: 16 |
| [88] | Séran J L, Le Flem M. Irradiation-resistant austenitic steels as core materials for Generation IV nuclear reactors [A]. Structural Materials for Generation IV Nuclear Reactors [M]. Amsterdam: Woodhead Publishing, 2017: 285 |
| [89] | Kato T, Takahashi H, Izumiya M. Grain boundary segregation under electron irradiation in austenitic stainless steels modified with oversized elements [J]. J. Nucl. Mater., 1992, 189: 167 |
| [90] | Sakaguchi N, Watanabe S, Takahashi H. Effect of additional minor element on radiation-induced grain boundary segregation in austenitic stainless steel under electron irradiation [J]. Nucl. Instrum. Methods Phys. Res., 1999, 153B: 142 |
| [91] | Hackett M J, Busby J T, Miller M K, et al. Effects of oversized solutes on radiation-induced segregation in austenitic stainless steels [J]. J. Nucl. Mater., 2009, 389: 265 |
| [92] | Kawanishi H, Nodaka M, Sekimura N, et al. Effects of C and Nb additions to Fe-16Ni-15Cr alloy on void swelling [J]. J. Nucl. Mater., 1984, 122: 284 |
| [93] | Little E A. Development of radiation resistant materials for advanced nuclear power plant [J]. Mater. Sci. Technol., 2006, 22: 491 |
| [94] | Zinkle S J, Snead L L. Designing radiation resistance in materials for fusion energy [J]. Annu. Rev. Mater. Res., 2014, 44: 241 |
| [95] | Shin J H, Kong B S, Jeong C, et al. Swelling resistance of an austenitic stainless steel with uniformly distributed nanosized NbC precipitates under heavy ion irradiation [J]. J. Nucl. Mater., 2022, 564: 153678 |
| [96] | Shin J H, Kong B S, Jeong C, et al. Evaluation of radiation resistance of an austenitic stainless steel with nanosized carbide precipitates using heavy ion irradiation at 200 dpa [J]. Nucl. Eng. Technol., 2023, 55: 555 |
| [97] | Maziasz P J. Void swelling resistance of phosphorus-modified austenitic stainless steels during HFIR irradiation at 300-500 oC to 57 dpa [J]. J. Nucl. Mater., 1993, 200: 90 |
| [98] | Tanaka M P, Hamada S, Hishinuma A, et al. Microstructural development of austenitic stainless steels irradiated in HFIR [J]. J. Nucl. Mater., 1988, 155-157: 801 |
| [99] | Bozin S N, Rodchenkov B S, Kashtanov A D, et al. Study of construction materials for a lead-cooled reactor [J]. At. Energy, 2013, 113: 320 |
| [100] | Porollo S I, Shulepin S V, Konobeev Y V, et al. Influence of silicon on swelling and microstructure in Russian austenitic stainless steel EI-847 irradiated to high neutron doses [J]. J. Nucl. Mater., 2008, 378: 17 |
| [101] | Pakhomov I. BN-600 and BN-800 operating experience [R]. Russia, 2018 |
| [102] | Ashida T, Gondai Y, Inoue M, et al. Experimental reactor Joyo [A]. Sodium-Cooled Fast Reactors [M]. London: Academic Press, 2022: 9 |
| [103] | Shibahara I, Ukai S, Onose S, et al. Irradiation performance of modified 316 stainless steel for Monju fuel [J]. J. Nucl. Mater., 1993, 204: 131 |
| [104] | Sham T L, Wang Y L, Bass R, et al. A709 qualification plan update and mechanical properties data assessment [R]. Idaho Falls: Idaho National Laboratory, 2022 |
| [105] | Rupp R E, Wang Y, Zhang X, et al. Integrated FY-21 elevated-temperature mechanical-testing results for alloy 709 code case [R]. Idaho Falls: Idaho National Laboratory, 2021 |
| [106] | Sham T L, Natesan K. Code qualification plan for an advanced austenitic stainless steel, alloy 709, for sodium fast reactor structural applications [R]. Argonne: Argonne National Laboratory, 2017 |
/
| 〈 |
|
〉 |