Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys
Received date: 2024-11-04
Revised date: 2025-01-02
Online published: 2025-02-20
Supported by
Ministry of Education Yangtze River Scholar Professor Program(T2020124);National Natural Science Foundation of China(52371104);National Natural Science Foundation of China(52171126);National Natural Science Foundation of China(52202374);National Natural Science Foundation of China(52331003);Guangdong Basic and Applied Basic Research Foundation(2024A1515013052);Guangzhou Basic and Applied Basic Research Special Project(2024A04J4289);HK PolyU grant(1-YXB4)
Magnesium alloys are the lightest metallic structural materials. The density of magnesium alloys is ~1.7 g/cm3, which is ~2/3 of the aluminum alloy, ~2/5 of titanium alloys, and ~1/4 of steel. Magnesium alloys possess high specific strength, excellent casting performance, excellent biocompatibility, good electromagnetic shielding performance, remarkable damping performance, and ease of recovery. They have broad application potential in aerospace, defense, automobile transportation, biomedical, electronic 3C, construction, and energy fields. China has substantial Mg resources. The development of low-cost and high-performance magnesium alloys in the lightweight field can transform resource advantages into industrial benefits while promoting energy conservation and emission reduction in production and daily life. This is strategically significant for the enhancement of the country's technology industry and the achievement of the objectives of “carbon peak and carbon neutrality”. However, commercial magnesium alloys currently possess relatively low strength, poor ductility, and corrosion resistance compared with common metallic structural materials like steel and aluminum alloys, significantly hindering the large-scale industrial application of magnesium alloys as structural materials. Many methods exist to enhance the comprehensive mechanical properties of magnesium alloys. Conventionally, the microstructure of magnesium alloys can be modified by adding alloying elements, plastic deformation, and heat treatment. The strength of magnesium alloys can be improved through grain refinement, work hardening, solid solution strengthening, and precipitation strengthening. Nevertheless, magnesium alloys prepared through these traditional methods can achieve excellent strength but at the expense of ductility, leading to the strength-ductility tradeoff in the magnesium alloy. At present, ultrahigh-pressure (UHP) treatment technology can achieve novel phases and modified microstructures that cannot be prepared under atmospheric pressure. The pressure significantly impacts the thermodynamics and dynamic parameters of metallic materials, such as the equilibrium temperature, critical radius for nucleation, interfacial free energy, chemical potential, entropy, enthalpy and heat capacity, and nucleation rate. Thus, the solid solubility, grain size, morphologies, dislocation density and types, twin types and morphologies, as well as the distribution and morphologies of the intermetallic phases of the magnesium alloys, can be modified using UHP treatment combined with temperature. It offers significant potential for altering the microstructure of magnesium alloys, providing new paths to break the bottlenecks between the comprehensive properties. This paper summarizes the progress of the research on the UHP treatment of high-performance magnesium alloys, the fabrication technology, and the technical characteristics of the UHP treatment. Moreover, the effects of UHP treatment on the mechanical properties, corrosion resistance, and hydrogen storage properties of magnesium alloys by modifying the microstructures of magnesium alloys are emphasized. Finally, the future development directions of the UHP magnesium alloys are explored.
FU Hui , SUN Yong , ZOU Guodong , ZHANG Fan , YANG Xusheng , ZHANG Tao , PENG Qiuming . Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys[J]. Acta Metall Sin, 2025 , 61(3) : 475 -487 . DOI: 10.11900/0412.1961.2024.00366
| 1 | Peng L M, Deng Q C, Wu Y J, et al. Additive manufacturing of magnesium alloys by selective laser melting technology: A review [J]. Acta Metall. Sin., 2023, 59: 31 |
| 彭立明, 邓庆琛, 吴玉娟 等. 镁合金选区激光熔化增材制造技术研究现状与展望 [J]. 金属学报, 2023, 59: 31 | |
| 2 | Peng X, Liu W C, Wu G H. Strengthening-toughening methods and mechanisms of Mg-Li alloy: A review [J]. Rare Met., 2022, 41: 1176 |
| 3 | Nie J F, Shin K S, Zeng Z R. Microstructure, deformation, and property of wrought magnesium alloys [J]. Metall. Mater. Trans., 2020, 51A: 6045 |
| 4 | Yue Y H, Gao Y F, Hu W T, et al. Hierarchically structured diamond composite with exceptional toughness [J]. Nature, 2020, 582: 370 |
| 5 | Ge B C, Fu H, Deng K K, et al. Unique strengthening mechanisms of ultrahigh pressure Mg alloys [J]. Bioact. Mater., 2018, 3: 250 |
| 6 | Fu H, Ge B C, Xin Y C, et al. Achieving high strength and ductility in magnesium alloys via densely hierarchical double contraction nanotwins [J]. Nano Lett., 2017, 17: 6117 |
| 7 | Wang L, Lin X P, Xu C, et al. The microstructure and the mechanical property of AZ91D solidified under GPa-grade high-pressure [J]. Mater. Sci. Technol., 2019, 35: 1690 |
| 8 | Peng Q M, Sun Y, Wang J, et al. Structural characteristics of $\left\{ 10\bar{1}1 \right\}$ contraction twin-twin interaction in magnesium [J]. Acta Mater., 2020, 192: 60 |
| 9 | Zhao S S, Peng Q M, Li H, et al. Effects of super-high pressure on microstructures, nano-mechanical behaviors and corrosion properties of Mg-Al alloys [J]. J. Alloys Compd., 2014, 584: 56 |
| 10 | Fu H, Peng Q M, Guo J X, et al. High-pressure synthesis of a nanoscale YB12 strengthening precipitate in Mg-Y alloys [J]. Scr. Mater., 2014, 76: 33 |
| 11 | Feng J W, Li H N, Deng K K, et al. Unique corrosion resistance of ultrahigh pressure Mg-25Al binary alloys [J]. Corros. Sci., 2018, 143: 229 |
| 12 | Feng J W, Zhang H, Zhang L, et al. Microstructure and corrosion properties for ultrahigh-pressure Mg-Li alloys [J]. Corros. Sci., 2022, 206: 110519 |
| 13 | Yang H, Ding Z, Li Y T, et al. Recent advances in kinetic and thermodynamic regulation of magnesium hydride for hydrogen storage [J]. Rare Met., 2023, 42: 2906 |
| 14 | Ouyang L Z, Liu F, Wang H, et al. Magnesium-based hydrogen storage compounds: A review [J]. J. Alloys Compd., 2020, 832: 154865 |
| 15 | Wu C, Yang S Q, Li Y, et al. Microstructural evolution and electrochemical properties of the ultra-high pressure treated La0.70Mg0.30Ni3.3 hydrogen storage alloy [J]. J. Alloys Compd., 2016, 665: 231 |
| 16 | Pimenta Martins L G, Comin R, Matos M J S, et al. High-pressure studies of atomically thin van der Waals materials [J]. Appl. Phys. Rev., 2023, 10: 011313 |
| 17 | Tang Y, Wang H K, Ouyang X P, et al. Overcoming strength-ductility tradeoff with high pressure thermal treatment [J]. Nat. Commun., 2024, 15: 3932 |
| 18 | Bridgman P W. Recent work in the field of high pressures [J]. Rev. Mod. Phys., 1946, 18: 1 |
| 19 | Schilling J S. The use of high pressure in basic and materials science [J]. J. Phys. Chem. Solids, 1998, 59: 553 |
| 20 | Wu B L, Chen B, Wang C W, et al. Corrosion behavior of a novel Mg-13Li-X alloy with different grain sizes by rapid solidification rate [J]. Rare Met., 2022, 41: 3197 |
| 21 | Sobczak J J, Drenchev L, Asthana R. Effect of pressure on solidification of metallic materials [J]. Int. J. Cast Met. Res., 2012, 25: 1 |
| 22 | Nie J F. Precipitation and hardening in magnesium alloys [J]. Metall. Mater. Trans., 2012, 43A: 3891 |
| 23 | Lin X P, Dai P L, Xu C, et al. Solute redistribution and mechanism of structure refinement of Mg-Al alloy during solidification under high pressure [J]. J. Alloys Compd., 2022, 910: 164777 |
| 24 | Peng X, Liu W C, Wu G H, et al. Plastic deformation and heat treatment of Mg-Li alloys: A review [J]. J. Mater. Sci. Technol., 2022, 99: 193 |
| 25 | Ge B C, Yang M, Zu Q, et al. Lithium cluster segregation in coherent contraction twin boundaries of magnesium alloys [J]. Acta Mater., 2020, 201: 477 |
| 26 | Peng Q M, Ge B C, Fu H, et al. Nanoscale coherent interface strengthening of Mg alloys [J]. Nanoscale, 2018, 10: 18028 |
| 27 | Peng Q M, Sun Y, Ge B C, et al. Interactive contraction nanotwins-stacking faults strengthening mechanism of Mg alloys [J]. Acta Mater., 2019, 169: 36 |
| 28 | Zhang S, Sun Y, Wu R Z, et al. Coherent interface strengthening of ultrahigh pressure heat-treated Mg-Li-Y alloys [J]. J. Mater. Sci. Technol., 2020, 51: 79 |
| 29 | Wang D, Huang P Z, Wu R Z, et al. Synergistically improved strength and damping capacity of Mg-Li-Y-Er-Zn-Zr alloy by ultra-high pressure treatment [J]. Mater. Sci. Eng, 2024, A915: 147205 |
| 30 | Meier J M, Caris J, Luo A A. Towards high strength cast Mg-RE based alloys: Phase diagrams and strengthening mechanisms [J]. J. Magnes. Alloy., 2022, 10: 1401 |
| 31 | Zhao H G, Pan J L, Li H, et al. Spherical strengthening precipitate in a Mg-10wt%Y alloy with superhigh pressure aging [J]. Mater. Lett., 2013, 96: 16 |
| 32 | Fu H, Li H, Fang D Q, et al. High ductility of a bi-modal Mg-7wt.%Y alloy at low temperature prepared by high pressure boriding and semi-solid extrusion [J]. Mater. Des., 2016, 92: 240 |
| 33 | Fu H, Liu N, Zhang Z W, et al. Effect of super-high pressure on microstructure and mechanical properties of Mg97Zn1Y2 alloys [J]. J. Magnes. Alloy., 2016, 4: 302 |
| 34 | Matsushita M, Masuda K, Waki R, et al. Ultrafine spherulite Mg alloy with high yield strength [J]. J. Alloys Compd., 2019, 784: 1284 |
| 35 | Matsushita M, Sakata Y, Senzaki T, et al. Phase relations among D03, α-Mg, and long-period stacking orders in Mg85Zn6Y9 alloy under 3 GPa [J]. Mater. Trans., 2015, 56: 910 |
| 36 | Matsushita M, Yamamoto S, Nishiyama N, et al. D03 + hcp mixed phase with nanostructures in Mg85Zn6Y9 alloy obtained by high-pressure and high-temperature treatments [J]. Mater. Lett., 2015, 155: 11 |
| 37 | Haque N, Cochrane R F, Mullis A M. Rapid solidification morphologies in Ni3Ge: Spherulites, dendrites and dense-branched fractal structures [J]. Intermetallics, 2016, 76: 70 |
| 38 | Zhou L T, Niu T T, Zou G D, et al. High-strong-ductile magnesium alloys by interactions of nanoscale quasi-long period stacking order unit with twin [J]. J. Magnes. Alloy., 2024, 12: 4953 |
| 39 | Atrens A, Shi Z M, Mehreen S U, et al. Review of Mg alloy corrosion rates [J]. J. Magnes. Alloy., 2020, 8: 989 |
| 40 | Feng J W, Pan Y K, Yang M, et al. A lactoglobulin-composite self-healing coating for Mg alloys [J]. ACS Appl. Bio Mater., 2021, 4: 6843 |
| 41 | Zhu Q C, Li Y X, Cao F Y, et al. Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film [J]. Nat. Commun., 2022, 13: 5838 |
| 42 | Peng Q M, Zhao S S, Li H, et al. High pressure solidification: An effective approach to improve the corrosion properties of Mg-Y based implants [J]. Int. J. Electrochem. Sci., 2012, 7: 5581 |
| 43 | Yang M, Feng J W, Hu H D, et al. Microstructure and corrosion resistance of ultrahigh pressure Mg-8Li based alloys [J]. J. Alloys Compd., 2023, 966: 171543 |
| 44 | Deng M, Wang L Q, H?che D, et al. Approaching “stainless magnesium” by Ca micro-alloying [J]. Mater. Horiz., 2021, 8: 589 |
| 45 | Xu W Q, Birbilis N, Sha G, et al. A high-specific-strength and corrosion-resistant magnesium alloy [J]. Nat. Mater., 2015, 14: 1229 |
| 46 | Shang Y Y, Pistidda C, Gizer G, et al. Mg-based materials for hydrogen storage [J]. J. Magnes. Alloy., 2021, 9: 1837 |
| 47 | Chen J, Sakai T, Kitamura N, et al. High-pressure synthesis of amorphous MgNi1.02H2.2 [J]. J. Am. Chem. Soc., 2001, 123: 6193 |
| 48 | Takamura H, Kakuta H, Kamegawa A, et al. Crystal structure of novel hydrides in a Mg-Ni-H system prepared under an ultra high pressure [J]. J. Alloys Compd., 2002, 330-332: 157 |
| 49 | Kataoka R, Goto Y, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-Ni-H and Mg-Ni-Cu-H systems [J]. J. Alloys Compd., 2007, 446-447: 142 |
| 50 | Kataoka R, Kamegawa A, Takamura H, et al. High pressure synthesis of novel Mg (Ni1 - x Cu x )2 hydrides (x = 0-0.2) [J]. Mater. Trans., 2009, 50: 1179 |
| 51 | Kataoka R, Goto Y, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-Ni(-H) system [J]. Mater. Trans., 2006, 47: 1957 |
| 52 | Kamata Y, Kuriiwa T, Kamegawa A, et al. Effect of Cu or Ti substitution in MgNi on crystal structure and hydrogen absorption-desorption properties [J]. Mater. Trans., 2009, 50: 2064 |
| 53 | Peng X Y, Liu B Z, Zhao X, et al. Effects of ultra-high pressure on phase compositions, phase configurations and hydrogen storage properties of LaMg4Ni alloys [J]. Int. J. Hydrogen Energy, 2013, 38: 14661 |
| 54 | Fu H, Wu W S, Dou Y, et al. Hydrogen diffusion kinetics and structural integrity of superhigh pressure Mg-5wt%Ni alloys with dendrite interface [J]. J. Power Sources, 2016, 320: 212 |
| 55 | Sun Y, Wang D B, Wang J M, et al. Hydrogen storage properties of ultrahigh pressure Mg12NiY alloys with a superfine LPSO structure [J]. Int. J. Hydrogen Energy, 2019, 44: 23179 |
| 56 | Torres B, Martínez-Lope M J, Alonso J A, et al. Short communication: High-pressure synthesis and crystal structure of a novel Mg3CuH x ternary hydride [J]. Int. J. Hydrogen Energy, 2013, 38: 15264 |
| 57 | Kyoi D, Sato T, R?nnebro E, et al. A novel magnesium-vanadium hydride synthesized by a gigapascal-high-pressure technique [J]. J. Alloys Compd., 2004, 375: 253 |
| 58 | Moser D, Bull D J, Sato T, et al. Structure and stability of high pressure synthesized Mg-TM hydrides (TM = Ti, Zr, Hf, V, Nb and Ta) as possible new hydrogen rich hydrides for hydrogen storage [J]. J. Mater. Chem., 2009, 19: 8150 |
| 59 | Goto Y, Kakuta H, Kamegawa A, et al. High-pressure synthesis of novel hydride in Mg-M systems (M?=?Li, Pd) [J]. J. Alloys Compd., 2005, 404-406: 448 |
| 60 | Retuerto M, Sánchez-Benítez J, Rodríguez-Ca?as E, et al. High-pressure synthesis of Mg2FeH6 complex hydride [J]. Int. J. Hydrogen Energy, 2010, 35: 7835 |
| 61 | Goto Y, Kamegawa A, Takamura H, et al. Synthesis of new hydrides in Mg-Y systems by using high pressure [J]. Mater. Trans., 2002, 43: 2717 |
/
| 〈 |
|
〉 |