State-of-the-Art Progress and Outlook in Wire Arc Additive Manufacturing of Magnesium Alloys
Received date: 2024-09-06
Revised date: 2024-10-21
Online published: 2024-11-26
Supported by
National Natural Science Foundation of China(523B2049);National Natural Science Foundation of China(52275374);National Natural Science Foundation of China(52205414)
Wire arc additive manufacturing (WAAM) is a promising additive manufacturing process known for its high deposition efficiency and cost effectiveness, making it well-suited for the large-scale production of complex, lightweight magnesium alloy components. Despite these advantages, magnesium alloys present challenges owing to their low melting and boiling points and high thermal conductivity, which result in nonuniform microstructures, metallurgical defects, and residual stresses in WAAM-manufactured components. These issues notably reduce the reliability and service life of the components, making it difficult to meet the demanding requirements of high-end equipment applications. It presents a critical challenge that must be addressed. This review outlines the advantages and technical challenges of WAAM, providing a comprehensive overview of recent domestic and international research in five key areas: process types, forming quality, metallurgical defects, microstructure characteristics, and overall performance. In addition, the present study summarizes in situ modulation strategies besed on the liquid melt pool and solid interlayer, as well as heat treatment and surface strengthening methods, providing a theoretical framework for improving the quality of large and complex magnesium alloy components. Finally, this review discusses future trends and research directions in WAAM for magnesium alloys, with a focus on composition design, in situ modulation, post-treatment processes, and performance evaluation.
HUANG Ke , LI Xinzhi , FANG Xuewei , LU Bingheng . State-of-the-Art Progress and Outlook in Wire Arc Additive Manufacturing of Magnesium Alloys[J]. Acta Metall Sin, 2025 , 61(3) : 397 -419 . DOI: 10.11900/0412.1961.2024.00314
| 1 | Yang Y, Xiong X M, Chen J, et al. Research advances in magnesium and magnesium alloys worldwide in 2020 [J]. J. Magnes. Alloy., 2021, 9: 705 |
| 2 | Xu T C, Yang Y, Peng X D, et al. Overview of advancement and development trend on magnesium alloy [J]. J. Magnes. Alloy., 2019, 7: 536 |
| 3 | Sui S, Guo S, Ma D, et al. Additive manufacturing of magnesium and its alloys: Process-formability-microstructure-performance relationship and underlying mechanism [J]. Int. J. Extrem. Manuf., 2023, 5: 042009 |
| 4 | Gu D D, Shi X Y, Poprawe R, et al. Material-structure-performance integrated laser-metal additive manufacturing [J]. Science, 2021, 372: eabg1487 |
| 5 | Tang W N, Mo N, Hou J. Research progress of additively manufactured magnesium alloys: A review [J]. Acta Metall. Sin., 2023, 59: 205 |
| 唐伟能, 莫 宁, 侯 娟. 增材制造镁合金技术现状与研究进展 [J]. 金属学报, 2023, 59: 205 | |
| 6 | Peng L M, Deng Q C, Wu Y J, et al. Additive manufacturing of magnesium alloys by selective laser melting technology: A review [J]. Acta Metall. Sin., 2023, 59: 31 |
| 彭立明, 邓庆琛, 吴玉娟 等. 镁合金选区激光熔化增材制造技术研究现状与展望 [J]. 金属学报, 2023, 59: 31 | |
| 7 | Li X Z, Fang X W, Chang T X, et al. Research progress in precise fabrication of lightweight magnesium alloys by selective laser melting [J]. J. Netshape Form. Eng., 2022, 14(4): 78 |
| 李新志, 方学伟, 常天行 等. 选区激光熔化精密成形轻质镁合金的研究进展 [J]. 精密成形工程, 2022, 14(4): 78 | |
| 8 | Li K, Ji C, Bai S W, et al. Selective laser melting of magnesium alloys: Necessity, formability, performance, optimization and applications [J]. J. Mater. Sci. Technol., 2023, 154: 65 |
| 9 | Li X Z, Fang X W, Jiang X, et al. Additively manufactured high-performance AZ91D magnesium alloys with excellent strength and ductility via nanoparticles reinforcement [J]. Addit. Manuf., 2023, 69: 103550 |
| 10 | Li X Z, Fang X W, Wang S P, et al. Selective laser melted AZ91D magnesium alloy with superior balance of strength and ductility [J]. J. Magnes. Alloy., 2023, 11: 4644 |
| 11 | Zheng D D, Li Z, Jiang Y L, et al. Effect of multiple thermal cycles on the microstructure evolution of GA151K alloy fabricated by laser-directed energy deposition [J]. Addit. Manuf., 2022, 57: 102957 |
| 12 | Jiang Y L, Tang H B, Li Z, et al. Additive manufactured Mg-Gd-Y-Zr alloys: Effects of Gd content on microstructure evolution and mechanical properties [J]. Addit. Manuf., 2022, 59: 103136 |
| 13 | Yi H, Wang Q, Cao H J. Wire-arc directed energy deposition of magnesium alloys: Microstructure, properties and quality optimization strategies [J]. J. Mater. Res. Technol., 2022, 20: 627 |
| 14 | Wang Z, Fu B G, Wang Y F, et al. Research progress of additive manufacturing of magnesium alloys [J]. Chin. J. Nonferrous Met., 2021, 31: 3093 |
| 王 哲, 付彬国, 王玉凤 等. 增材制造镁合金的研究进展 [J]. 中国有色金属学报, 2021, 31: 3093 | |
| 15 | Zhao Z X, Yan P F, Wu J, et al. Research progress of additive manufacturing magnesium alloy [J]. Chin. J. Nonferrous Met., 2023, 33: 2753 |
| 赵致先, 闫鹏飞, 吴 捷 等. 增材制造镁合金的研究现状与展望 [J]. 中国有色金属学报, 2023, 33: 2753 | |
| 16 | Zhang C H, Li Z, Zhang J K, et al. Additive manufacturing of magnesium matrix composites: Comprehensive review of recent progress and research perspectives [J]. J. Magnes. Alloy., 2023, 11: 425 |
| 17 | Zeng Z R, Salehi M, Kopp A, et al. Recent progress and perspectives in additive manufacturing of magnesium alloys [J]. J. Magnes. Alloy., 2022, 10: 1511 |
| 18 | Ansari N, Alabtah F G, Albakri M I, et al. Post processing of additive manufactured Mg alloys: Current status, challenges, and opportunities [J]. J. Magnes. Alloy., 2024, 12: 1283 |
| 19 | Chen F K, Cai X Y, Dong B L, et al. Effect of process modes on microstructure and mechanical properties of CMT wire arc additive manufactured WE43 magnesium alloy [J]. J. Mater. Res. Technol., 2023, 27: 2089 |
| 20 | Cao Q H, Qi B J, Zeng C Y, et al. Achieving equiaxed microstructure and isotropic mechanical properties of additively manufactured AZ31 magnesium alloy via ultrasonic frequency pulsed arc [J]. J. Alloys Compd., 2022, 909: 164742 |
| 21 | Cao Q H, Zeng C Y, Qi B J, et al. Excellent isotropic mechanical properties of directed energy deposited Mg-Gd-Y-Zr alloys via establishing homogeneous equiaxed grains embedded with dispersed nano-precipitation [J]. Addit. Manuf., 2023, 67: 103498 |
| 22 | Li X Z, Fang X W, Zhang M G, et al. Enhanced strength-ductility synergy of magnesium alloy fabricated by ultrasound assisted directed energy deposition [J]. J. Mater. Sci. Technol., 2024, 178: 247 |
| 23 | Li X Z, Fang X W, Fang D Q, et al. On the excellent strength-ductility synergy of wire-arc directed energy deposited Mg-Gd-Y-Zn-Zr alloy via manipulating precipitates [J]. Addit. Manuf., 2023, 77: 103794 |
| 24 | Li X Z, Zhang M G, Fang X W, et al. Improved strength-ductility synergy of directed energy deposited AZ31 magnesium alloy with cryogenic cooling mode [J]. Virtual Phys. Prototyping, 2023, 18: e2170252 |
| 25 | Cao Q H, Zeng C Y, Cai X Y, et al. High-strength Mg-10Gd-3Y-1Zn-0.5Zr alloy fabricated by wire-arc directed energy deposition: Phase transformation behavior and mechanical properties [J]. Addit. Manuf., 2023, 76: 103789 |
| 26 | Li X Z, Fang X W, Zhang Z Y, et al. Revealing precipitation behavior and mechanical response of wire-arc directed energy deposited Mg-Gd-Y-Zr alloy by tailoring aging procedures [J]. Int. J. Extrem. Manuf., 2024, 6: 045001 |
| 27 | Yi H, Yang L, Jia L, et al. Porosity in wire-arc directed energy deposition of aluminum alloys: Formation mechanisms, influencing factors and inhibition strategies [J]. Addit. Manuf., 2024, 84: 104108 |
| 28 | Han S, Zielewski M, Martinez Holguin D, et al. Optimization of AZ91D process and corrosion resistance using wire arc additive manufacturing [J]. Appl. Sci., 2018, 8: 1306 |
| 29 | Takagi H, Sasahara H, Abe T, et al. Material-property evaluation of magnesium alloys fabricated using wire-and-arc-based additive manufacturing [J]. Addit. Manuf., 2018, 24: 498 |
| 30 | Yang X, Liu J R, Wang Z N, et al. Microstructure and mechanical properties of wire and arc additive manufactured AZ31 magnesium alloy using cold metal transfer process [J]. Mater. Sci. Eng., 2020, A774: 138742 |
| 31 | Wang P, Zhang H Z, Zhu H, et al. Wire-arc additive manufacturing of AZ31 magnesium alloy fabricated by cold metal transfer heat source: Processing, microstructure, and mechanical behavior [J]. J. Mater. Process. Technol., 2021, 288: 116895 |
| 32 | Guo Y Y, Quan G F, Jiang Y L, et al. Formability, microstructure evolution and mechanical properties of wire arc additively manufactured AZ80M magnesium alloy using gas tungsten arc welding [J]. J. Magnes. Alloy., 2021, 9: 192 |
| 33 | Bi J, Shen J, Hu S, et al. Microstructure and mechanical properties of AZ91 Mg alloy fabricated by cold metal transfer additive manufacturing [J]. Mater. Lett., 2020, 276: 128185 |
| 34 | Zhang H, Hu S S, Wang Z J, et al. The effect of welding speed on microstructures of cold metal transfer deposited AZ31 magnesium alloy clad [J]. Mater. Des., 2015, 86: 894 |
| 35 | Fang X W, Yang J N, Wang S P, et al. additive manufacturing of high performance AZ31 magnesium alloy with full equiaxed grains: Microstructure, mechanical property, and electromechanical corrosion performance [J]. J. Mater. Process. Technol., 2022, 300: 117430 |
| 36 | Ying T, Zhao Z X, Yan P F, et al. Effect of fabrication parameters on the microstructure and mechanical properties of wire arc additive manufactured AZ61 alloy [J]. Mater. Lett., 2022, 307: 131014 |
| 37 | Tong X, Wu G H, Easton M A, et al. Microstructural evolution and strengthening mechanism of Mg-Y-RE-Zr alloy fabricated by quasi-directed energy deposition [J]. Addit. Manuf., 2023, 67: 103487 |
| 38 | Wang Z H, Wang J F, Lin X, et al. Solidification microstructure evolution and its correlations with mechanical properties and damping capacities of Mg-Al-based alloy fabricated using wire and arc additive manufacturing [J]. J. Mater. Sci. Technol., 2023, 144: 28 |
| 39 | Ma D, Xu C J, Sui S, et al. Microstructure evolution and mechanical properties of wire arc additively manufactured Mg-Gd-Y-Zr alloy by post heat treatments [J]. Virtual Phys. Prototyping, 2023, 18: e2225492 |
| 40 | Cai X Y, Chen F K, Dong B L, et al. Microstructure and mechanical properties of GTA-based wire arc additive manufactured AZ91D magnesium alloy [J]. J. Magnes. Alloy., 2022, 12: 3180 |
| 41 | Ma D, Xu C J, Qi Y S, et al. Achieving fully equiaxed grain microstructure and isotropic mechanical properties in wire arc additive-manufactured Mg-Y-Nd-Zr alloys [J]. J. Alloys Compd., 2023, 962: 171041 |
| 42 | Wang Z H, Wang J F, Lin X, et al. Solidification texture dependence of the anisotropy of mechanical properties and damping capacities of an AZ31 Mg-based alloy fabricated via wire-arc additive manufacturing [J]. J. Mater. Res. Technol., 2023, 25: 2589 |
| 43 | Manjhi S K, Sekar P, Bontha S, et al. Effect of equiaxed grains and secondary phase particles on mechanical properties and corrosion behaviour of CMT-based wire arc additive manufactured AZ31 Mg alloy [J]. CIRP J. Manuf. Sci. Technol., 2023, 46: 48 |
| 44 | Guo Y Y, Quan G F, Celikin M, et al. Effect of heat treatment on the microstructure and mechanical properties of AZ80M magnesium alloy fabricated by wire arc additive manufacturing [J]. J. Magnes. Alloy., 2022, 10: 1930 |
| 45 | Guo Y Y, Pan H H, Ren L B, et al. Microstructure and mechanical properties of wire arc additively manufactured AZ80M magnesium alloy [J]. Mater. Lett., 2019, 247: 4 |
| 46 | Li J W, Qiu Y M, Yang J J, et al. Effect of grain refinement induced by wire and arc additive manufacture (WAAM) on the corrosion behaviors of AZ31 magnesium alloy in NaCl solution [J]. J. Magnes. Alloy., 2023, 11: 217 |
| 47 | Zhang Z, Wang L Q, Zhang R Z, et al. Effect of solution annealing on microstructures and corrosion behavior of wire and arc additive manufactured AZ91 magnesium alloy in sodium chloride solution [J]. J. Mater. Res. Technol., 2022, 18: 416 |
| 48 | Li X Z, Fang X W, Zhang M G, et al. Gradient microstructure and prominent performance of wire-arc directed energy deposited magnesium alloy via laser shock peening [J]. Int. J. Mach. Tools Manuf., 2023, 188: 104029 |
| 49 | Qiu Z J, Dong B S, Wu B T, et al. Tailoring the surface finish, dendritic microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy by magnetic arc oscillation [J]. Addit. Manuf., 2021, 48: 102397 |
| 50 | Gong M C, Meng Y F, Zhang S, et al. Laser-arc hybrid additive manufacturing of stainless steel with beam oscillation [J]. Addit. Manuf., 2020, 33: 101180 |
| 51 | Martina F, Roy M J, Szost B A, et al. Residual stress of as-deposited and rolled wire + arc additive manufacturing Ti-6Al-4V components [J]. Mater. Sci. Technol., 2016, 32: 1439 |
| 52 | Cong B Q, Cai X Y, Qi Z W, et al. The effects of ultrasonic frequency pulsed arc on wire + arc additively manufactured high strength aluminum alloys [J]. Addit. Manuf., 2022, 51: 102617 |
| 53 | Guo J, Zhou Y, Liu C M, et al. Wire Arc additive manufacturing of AZ31 magnesium alloy: Grain refinement by adjusting pulse frequency [J]. Materials, 2016, 9: 823 |
| 54 | Yi H, Wang Q, Zhang W J, et al. Wire-arc directed energy deposited Mg-Al alloy assisted by ultrasonic vibration: Improving properties via controlling grain structures [J]. J. Mater. Process. Technol., 2023, 321: 118134 |
| 55 | Ma D, Xu C J, Sui S, et al. Enhanced strength-ductility synergy in a wire and arc additively manufactured Mg alloy via tuning interlayer dwell time [J]. J. Magnes. Alloy., 2023, 11: 4696 |
| 56 | Colegrove P A, Coules H E, Fairman J, et al. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling [J]. J. Mater. Process. Technol., 2013, 213: 1782 |
| 57 | Hai-Ou Z, Wang R, Liang L Y, et al. HDMR technology for the aircraft metal part [J]. Rapid Prototyping J., 2016, 22: 857 |
| 58 | Fang X W, Yang J N, Jiang X, et al. Wire-arc directed energy deposited high-performance AZ31 magnesium alloy via a novel interlayer hammering treatment [J]. Mater. Sci. Eng., 2024, A889: 145864 |
| 59 | Zhao X H, Ren B Q, Zhang Y W, et al. Microstructural evolution and strengthening mechanisms of CMT directed energy deposition-arc with interlayer ultrasonic impact treatment manufactured AZ31 magnesium alloy [J]. Mater. Sci. Eng., 2023, A879: 145267 |
| 60 | Wei J X, He C S, Qie M F, et al. Achieving high performance of wire arc additive manufactured Mg-Y-Nd alloy assisted by interlayer friction stir processing [J]. J. Mater. Process. Technol., 2023, 311: 117809 |
| 61 | Graf G, Spoerk-Erdely P, Maawad E, et al. Effect of wire-arc directed energy deposition on the microstructural formation and age-hardening response of the Mg-9Al-1Zn (AZ91) alloy [J]. J. Magnes. Alloy., 2023, 11: 1944 |
| 62 | Chen Y F, Zhang X C, Ding D H, et al. Integration of interlayer surface enhancement technologies into metal additive manufacturing: A review [J]. J. Mater. Sci. Technol., 2023, 165: 94 |
/
| 〈 |
|
〉 |