Overview

Progress on Materials Design and Multiscale Simulations for Phase-Change Memory

  • SHEN Xueyang ,
  • CHU Ruixuan ,
  • JIANG Yihui ,
  • ZHANG Wei
Expand
  • Center for Alloy Innovation and Design (CAID), State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China
ZHANG Wei, professor, Tel: (029)82664839, E-mail: wzhang0@mail.xjtu.edu.cn

Received date: 2024-06-03

  Revised date: 2024-07-05

  Online published: 2024-08-23

Supported by

National Key Research and Development Program of China(2023YFB4404500);National Natural Science Foundation of China(62374131)

Abstract

In the era of big data, the demand for data storage and processing is increasing because of advanced technologies such as artificial intelligence (AI), 5G, and cloud computing. Emerging non-volatile memory materials and devices present remarkable opportunities to enhance computing capacity. Concurrently, the AI-driven scientific research paradigm introduces a new mode for improving device performance. This review focuses on recent advances in phase-change memory materials and devices, emphasizing computational- and data-driven methodologies. Phase-change materials (PCMs) operate based on rapid and reversible phase transitions between amorphous and crystalline states, where differences in electrical and optical properties are used to encode digital information. These materials typically consist of multicomponent alloys, with phase transitions involving melting, quenching, crystallization, glass relaxation, and crystal-crystal structural changes. To achieve a detailed atomistic understanding of PCMs, large-scale density functional theory (DFT) and DFT-based ab initio molecular dynamics (AIMD) simulations are essential. Comparisons between DFT/AIMD simulations and experimental results have clarified many fundamental aspects of PCM. The first part of this review provides an overview of the history and progress in large-scale ab initio simulations of PCMs. With atomic-scale knowledge, rational materials design becomes feasible. The second part explores methods for developing new PCMs with specific properties, such as accelerating crystallization at elevated temperatures while maintaining non-volatile characteristics at room temperature. High-throughput screening's role in discovering new phase change alloys is also discussed. In the third part, we examine multiscale and cross-scale simulations of PCM for various optical and electronic phase change applications. By computing the dielectric functions of PCM during the amorphous-to-crystalline transition, we can track changes in the refractive index and extinction coefficient across visible and infrared spectra over time. These DFT-computed parameters inform coarse-grained device simulations using finite-difference time-domain (FDTD) or finite element method (FEM). Based on these multiscale simulations, we offer optimization guidelines for non-volatile color display and photonic waveguide devices. The machine learning potentials address some performance gaps between the DFT/AIMD and FEM/FDTD calculations. Machine-learning-driven molecular dynamics (MLMD) simulations serve as cross-scale simulations, with recent developments including neural networks, graph convolutional neural networks, and Gaussian approximation potentials. We discuss the role of MLMD in enabling device-scale atomistic simulations, facilitating device design and optimization with atomic-scale information. Finally, we outline future opportunities and challenges in theoretical PCM research. With ongoing AI-driven fundamental research, we anticipate the commercialization of high-performance phase change memory, neuroinspired computing, and reconfigurable nanophotonic devices, which will, in turn, foster the development of more advanced theoretical tools for research.

Cite this article

SHEN Xueyang , CHU Ruixuan , JIANG Yihui , ZHANG Wei . Progress on Materials Design and Multiscale Simulations for Phase-Change Memory[J]. Acta Metall Sin, 2024 , 60(10) : 1362 -1378 . DOI: 10.11900/0412.1961.2024.00188

References

1 Wuttig M, Yamada N. Phase-change materials for rewriteable data storage [J]. Nat. Mater., 2007, 6: 824
2 Wong H S P, Raoux S, Kim S, et al. Phase change memory [J]. Proc. IEEE, 2010, 98: 2201
3 Zhang W, Mazzarello R, Wuttig M, et al. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing [J]. Nat. Rev. Mater., 2019, 4: 150
4 Zhou W, Shen X Y, Yang X L, et al. Fabrication and integration of photonic devices for phase-change memory and neuromorphic computing [J]. Int. J. Extrem. Manuf., 2024, 6: 022001
5 Zhang Z H, Wang Z W, Shi T, et al. Memory materials and devices: From concept to application [J]. InfoMat, 2020, 2: 261
6 Kwon D H, Kim K M, Jang J H, et al. Atomic structure of conducting nanofilaments in TiO2 resistive switching memory [J]. Nat. Nanotechnol., 2010, 5: 148
7 Prezioso M, Merrikh-Bayat F, Hoskins B D, et al. Training and operation of an integrated neuromorphic network based on metal-oxide memristors [J]. Nature, 2015, 521: 61
8 Liu S, Lu N D, Zhao X L, et al. Eliminating negative-SET behavior by suppressing nanofilament overgrowth in cation-based memory [J]. Adv. Mater., 2016, 28: 10623
9 Mangin S, Ravelosona D, Katine J A, et al. Current-induced magnetization reversal in nanopillars with perpendicular anisotropy [J]. Nat. Mater., 2006, 5: 210
10 Torrejon J, Riou M, Araujo F A, et al. Neuromorphic computing with nanoscale spintronic oscillators [J]. Nature, 2017, 547: 428
11 Park B H, Kang B S, Bu S D, et al. Lanthanum-substituted bismuth titanate for use in non-volatile memories [J]. Nature, 1999, 401: 682
12 Chanthbouala A, Garcia V, Cherifi R O, et al. A ferroelectric memristor [J]. Nat. Mater., 2012, 11: 860
13 Wong H S P, Salahuddin S. Memory leads the way to better computing [J]. Nat. Nanotechnol., 2015, 10: 191
14 Yang J J, Strukov D B, Stewart D R. Memristive devices for computing [J]. Nat. Nanotechnol., 2013, 8: 13
15 Service R F. The brain chip [J]. Science, 2014, 345: 614
16 Lanza M, Sebastian A, Lu W D, et al. Memristive technologies for data storage, computation, encryption, and radio-frequency communication [J]. Science, 2022, 376: eabj9979
17 Liu B, Wei T, Hu J, et al. Universal memory based on phase-change materials: From phase-change random access memory to optoelectronic hybrid storage [J]. Chin. Phys., 2021, 30B: 058504
18 Kau D, Tang S, Karpov I V, et al. A stackable cross point phase change memory [A]. Proceedings of 2009 IEEE International Electron Devices Meeting [C]. Baltimore: IEEE, 2009: 1
19 Cheng H Y, Carta F, Chien W C, et al. 3D cross-point phase-change memory for storage-class memory [J]. J. Phys., 2019, 52D: 473002
20 Li X, Chen H P, Xie C C, et al. Enhancing the performance of phase change memory for embedded applications [J]. Phys. Status Solidi (RRL), 2019, 13: 1800558
21 Arnaud F, Ferreira P, Piazza F, et al. High density embedded PCM cell in 28 nm FDSOI technology for automotive micro-controller applications [A]. Proceedings of 2020 IEEE International Electron Devices Meeting [C]. San Francisco: IEEE, 2020: 24.2.1
22 Cappelletti P, Annunziata R, Arnaud F, et al. Phase change memory for automotive grade embedded NVM applications [J]. J. Phys., 2020, 53D: 193002
23 Sebastian A, Le Gallo M, Khaddam-Aljameh R, et al. Memory devices and applications for in-memory computing [J]. Nat. Nanotechnol., 2020, 15: 529
24 Xu M, Mai X L, Lin J, et al. Recent advances on neuromorphic devices based on chalcogenide phase-change materials [J]. Adv. Funct. Mater., 2020, 30: 2003419
25 Shastri B J, Tait A N, Ferreira de Lima T, et al. Photonics for artificial intelligence and neuromorphic computing [J]. Nat. Photonics, 2021, 15: 102
26 Liu H L, Dong W L, Wang H, et al. Rewritable color nanoprints in antimony trisulfide films [J]. Sci. Adv., 2020, 6: eabb7171
27 Cheng Z G, Milne T, Salter P, et al. Antimony thin films demonstrate programmable optical nonlinearity [J]. Sci. Adv., 2021, 7: eabd7097
28 Ríos C, Stegmaier M, Hosseini P, et al. Integrated all-photonic non-volatile multi-level memory [J]. Nat. Photonics, 2015, 9: 725
29 Cheng Z G, Ríos C, Pernice W H P, et al. On-chip photonic synapse [J]. Sci. Adv., 2017, 3: e1700160
30 Wuttig M, Bhaskaran H, Taubner T. Phase-change materials for non-volatile photonic applications [J]. Nat. Photonics, 2017, 11: 465
31 Wu C M, Yu H S, Lee S, et al. Programmable phase-change metasurfaces on waveguides for multimode photonic convolutional neural network [J]. Nat. Commun., 2021, 12: 96
32 Ríos C, Youngblood N, Cheng Z G, et al. In-memory computing on a photonic platform [J]. Sci. Adv., 2019, 5: eaau5759
33 Feldmann J, Youngblood N, Karpov M, et al. Parallel convolutional processing using an integrated photonic tensor core [J]. Nature, 2021, 589: 52
34 Zhang W, Mazzarello R, Ma E. Phase-change materials in electronics and photonics [J]. MRS Bull., 2019, 44: 686
35 Curtarolo S, Hart G L W, Nardelli M B, et al. The high-throughput highway to computational materials design [J]. Nat. Mater., 2013, 12: 191
36 Xie J X, Su Y J, Xue D Z, et al. Machine learning for materials research and development [J]. Acta Metall. Sin., 2021, 57: 1343
  谢建新, 宿彦京, 薛德祯 等. 机器学习在材料研发中的应用 [J]. 金属学报, 2021, 57: 1343
37 Friederich P, H?se F, Proppe J, et al. Machine-learned potentials for next-generation matter simulations [J]. Nat. Mater., 2021, 20: 750
38 Li H, Xu Y, Duan W H. Ab initio artificial intelligence: Future research of Materials Genome Initiative [J]. MGE Adv., 2023, 1: e16
39 Su Y J, Fu H D, Bai Y, et al. Progress in materials genome engineering in China [J]. Acta Metall. Sin., 2020, 56: 1313
  宿彦京, 付华栋, 白 洋 等. 中国材料基因工程研究进展 [J]. 金属学报, 2020, 56: 1313
40 Xie J X. Prospects of materials genome engineering frontiers [J]. MGE Adv., 2023, 1: e17
41 Feng R, Zhang C, Gao M C, et al. High-throughput design of high-performance lightweight high-entropy alloys [J]. Nat. Commun., 2021, 12: 4329
42 Rao Z Y, Tung P Y, Xie R W, et al. Machine learning-enabled high-entropy alloy discovery [J]. Science, 2022, 378: 78
43 Xu Y F, Elcoro L, Song Z D, et al. High-throughput calculations of magnetic topological materials [J]. Nature, 2020, 586: 702
44 Choudhary K, Garrity K F, Jiang J, et al. Computational search for magnetic and non-magnetic 2D topological materials using unified spin-orbit spillage screening [J]. npj Comput. Mater., 2020, 6: 49
45 Gorai P, Stevanovi? V, Toberer E S. Computationally guided discovery of thermoelectric materials [J]. Nat. Rev. Mater., 2017, 2: 17053
46 Wang X D, Tan J L, Ouyang J, et al. Designing inorganic semiconductors with cold-rolling processability [J]. Adv. Sci., 2022, 9: 2203776
47 Gao Z Q, Wei T R, Deng T T, et al. High-throughput screening of 2D van der Waals crystals with plastic deformability [J]. Nat. Commun., 2022, 13: 7491
48 Jain A, Ong S P, Hautier G, et al. Commentary: The Materials Project: A materials genome approach to accelerating materials innovation [J]. APL Mater., 2013, 1: 011002
49 Hicks D, Toher C, Ford D C, et al. AFLOW-XtalFinder: A reliable choice to identify crystalline prototypes [J]. npj Comput. Mater., 2021, 7: 30
50 Wang G J, Li K Q, Peng L Y, et al. High-throughput automatic integrated material calculations and data management intelligent platform and the application in novel alloys [J]. Acta Metall. Sin., 2022, 58: 75
  王冠杰, 李开旗, 彭力宇 等. 高通量自动流程集成计算与数据管理智能平台及其在合金设计中的应用 [J]. 金属学报, 2022, 58: 75
51 Yamada N, Ohno E, Akahira N, et al. High speed overwritable phase change optical disk material [J]. Jpn. J. Appl. Phys., 1987, 26(s4): 61
52 Yamada N, Ohno E, Nishiuchi K, et al. Rapid-phase transitions of GeTe-Sb2Te3 pseudobinary amorphous thin films for an optical disk memory [J]. J. Appl. Phys., 1991, 69: 2849
53 Caravati S, Bernasconi M, Kühne T D, et al. Coexistence of tetrahedral- and octahedral-like sites in amorphous phase change materials [J]. Appl. Phys. Lett., 2007, 91: 171906
54 Akola J, Jones R O. Structural phase transitions on the nanoscale: The crucial pattern in the phase-change materials Ge2Sb2Te5 and GeTe [J]. Phys. Rev., 2007, 76B: 235201
55 Kohara S, Kato K, Kimura S, et al. Structural basis for the fast phase change of Ge2Sb2Te5: Ring statistics analogy between the crystal and amorphous states [J]. Appl. Phys. Lett., 2006, 89: 201910
56 Rao F, Ding K Y, Zhou Y X, et al. Reducing the stochasticity of crystal nucleation to enable subnanosecond memory writing [J]. Science, 2017, 358: 1423
57 Orava J, Greer A L, Gholipour B, et al. Characterization of supercooled liquid Ge2Sb2Te5 and its crystallization by ultrafast-heating calorimetry [J]. Nat. Mater., 2012, 11: 279
58 Jeyasingh R, Fong S W, Lee J, et al. Ultrafast characterization of phase-change material crystallization properties in the melt-quenched amorphous phase [J]. Nano Lett., 2014, 14: 3419
59 Ronneberger I, Zhang W, Eshet H, et al. Crystallization properties of the Ge2Sb2Te5 phase-change compound from advanced simulations [J]. Adv. Funct. Mater., 2015, 25: 6407
60 Ronneberger I, Zhang W, Mazzarello R. Crystal growth of Ge2Sb2Te5 at high temperatures [J]. MRS Commun., 2018, 8: 1018
61 Xu Y Z, Zhou Y X, Wang X D, et al. Unraveling crystallization mechanisms and electronic structure of phase-change materials by large-scale ab initio simulations [J]. Adv. Mater., 2022, 34: 2109139
62 ten Wolde P R, Ruiz-Montero M J, Frenkel D. Simulation of homogeneous crystal nucleation close to coexistence [J]. Faraday Discuss., 1996, 104: 93
63 Bartók A P, Csányi G. Gaussian approximation potentials: A brief tutorial introduction [J]. Int. J. Quantum Chem., 2015, 115: 1051
64 Kalikka J, Akola J, Jones R O. Crystallization processes in the phase change material Ge2Sb2Te5: Unbiased density functional/molecular dynamics simulations [J]. Phys. Rev., 2016, 94B: 134105
65 Raty J Y, Zhang W, Luckas J, et al. Aging mechanisms in amorphous phase-change materials [J]. Nat. Commun., 2015, 6: 7467
66 Li X B, Liu X Q, Liu X, et al. Role of electronic excitation in the amorphization of Ge-Sb-Te alloys [J]. Phys. Rev. Lett., 2011, 107: 015501
67 Zalden P, Quirin F, Schumacher M, et al. Femtosecond X-ray diffraction reveals a liquid-liquid phase transition in phase-change materials [J]. Science, 2019, 364: 1062
68 Kalikka J, Akola J, Larrucea J, et al. Nucleus-driven crystallization of amorphous Ge2Sb2Te5: A density functional study [J]. Phys. Rev., 2012, 86B: 144113
69 Kalikka J, Akola J, Jones R O. Simulation of crystallization in Ge2Sb2Te5: A memory effect in the canonical phase-change material [J]. Phys. Rev., 2014, 90B: 184109
70 Loke D, Lee T H, Wang W J, et al. Breaking the speed limits of phase-change memory [J]. Science, 2012, 336: 1566
71 Zhang B, Zhang W, Shen Z J, et al. Element-resolved atomic structure imaging of rocksalt Ge2Sb2Te5 phase-change material [J]. Appl. Phys. Lett., 2016, 108: 191902
72 Xu M, Zhang W, Mazzarello R, et al. Disorder control in crystalline GeSb2Te4 using high pressure [J]. Adv. Sci., 2015, 2: 1500117
73 Zheng Y H, Xia M J, Cheng Y, et al. Direct observation of metastable face-centered cubic Sb2Te3 crystal [J]. Nano Res., 2016, 9: 3453
74 Li Z, Si C, Zhou J, et al. Yttrium-doped Sb2Te3: A promising material for phase-change memory [J]. ACS Appl. Mater. Interfaces, 2016, 8: 26126
75 Liu B, Li K Q, Liu W L, et al. Multi-level phase-change memory with ultralow power consumption and resistance drift [J]. Sci. Bull., 2021, 66: 2217
76 Zhou Y X, Sun L, Zewdie G M, et al. Bonding similarities and differences between Y-Sb-Te and Sc-Sb-Te phase-change memory materials [J]. J. Mater. Chem., 2020, 8C: 3646
77 Chen B, Chen Y M, Ding K Y, et al. Kinetics features conducive to cache-type nonvolatile phase-change memory [J]. Chem. Mater., 2019, 31: 8794
78 Hu S W, Liu B, Li Z, et al. Identifying optimal dopants for Sb2Te3 phase-change material by high-throughput ab initio calculations with experiments [J]. Comput. Mater. Sci., 2019, 165: 51
79 Zewdie G M, Zhou Y X, Sun L, et al. Chemical design principles for cache-type Sc-Sb-Te phase-change memory materials [J]. Chem. Mater., 2019, 31: 4008
80 Wang X P, Li X B, Chen N K, et al. Time-dependent density-functional theory molecular-dynamics study on amorphization of Sc-Sb-Te alloy under optical excitation [J]. npj Comput. Mater., 2020, 6: 31
81 Qiao C, Guo Y R, Wang S Y, et al. Local structure origin of ultrafast crystallization driven by high-fidelity octahedral clusters in amorphous Sc0.2Sb2Te3 [J]. Appl. Phys. Lett., 2019, 114: 071901
82 Ding K Y, Chen B, Chen Y M, et al. Recipe for ultrafast and persistent phase-change memory materials [J]. NPG Asia Mater., 2020, 12: 63
83 Ding K Y, Wang J J, Zhou Y X, et al. Phase-change heterostructure enables ultralow noise and drift for memory operation [J]. Science, 2019, 366: 210
84 Yang Z, Li B W, Wang J J, et al. Designing conductive-bridge phase-change memory to enable ultralow programming power [J]. Adv. Sci., 2022, 9: 2103478
85 Wang J J, Wang X Z, Cheng Y D, et al. Tailoring the oxygen concentration in Ge-Sb-O alloys to enable femtojoule-level phase-change memory operations [J]. Mater. Futures, 2022, 1: 045302
86 Liu Y T, Li X B, Zheng H, et al. High-throughput screening for phase-change memory materials [J]. Adv. Funct. Mater., 2021, 31: 2009803
87 Zhang W, Zhang H M, Sun S Y, et al. Metavalent bonding in layered phase-change memory materials [J]. Adv. Sci., 2023, 10: 2300901
88 Wuttig M, Deringer V L, Gonze X, et al. Incipient metals: Functional materials with a unique bonding mechanism [J]. Adv. Mater., 2018, 30: 1803777
89 Wuttig M, Sch?n C F, L?tfering J, et al. Revisiting the nature of chemical bonding in chalcogenides to explain and design their properties [J]. Adv. Mater., 2023, 35: 2208485
90 Xu Y Z, Wang X D, Zhang W, et al. Materials screening for disorder-controlled chalcogenide crystals for phase-change memory applications [J]. Adv. Mater., 2021, 33: 2006221
91 Zhang W, Thiess A, Zalden P, et al. Role of vacancies in metal-insulator transitions of crystalline phase-change materials [J]. Nat. Mater., 2012, 11: 952
92 Jiang T T, Wang X D, Wang J J, et al. In situ characterization of vacancy ordering in Ge-Sb-Te phase-change memory alloys [J]. Fundam. Res., 2022, DOI: 10.1016/j.fmre.2022.09.010
93 Esser M, Deringer V L, Wuttig M, et al. Orbital mixing in solids as a descriptor for materials mapping [J]. Solid State Commun., 2015, 203: 31
94 Wang Y Z, Ning J, Lu L, et al. A scheme for simulating multi-level phase change photonics materials [J]. npj Comput. Mater., 2021, 7: 183
95 Khan A I, Daus A, Islam R, et al. Ultralow-switching current density multilevel phase-change memory on a flexible substrate [J]. Science, 2021, 373: 1243
96 Ghazi Sarwat S, Philip T M, Chen C T, et al. Projected mushroom type phase-change memory [J]. Adv. Funct. Mater., 2021, 31: 2106547
97 Deringer V L, Caro M A, Csányi G. Machine learning interatomic potentials as emerging tools for materials science [J]. Adv. Mater., 2019, 31: 1902765
98 Wang H, Zhang L F, Han J Q, et al. DeePMD-kit: A deep learning package for many-body potential energy representation and molecular dynamics [J]. Comput. Phys. Commun., 2018, 228: 178
99 Wang G J, Wang C R, Zhang X G, et al. Machine learning interatomic potential: Bridge the gap between small-scale models and realistic device-scale simulations [J]. iScience, 2024, 27: 109673
100 Zhou Y X, Zhang W, Ma E, et al. Device-scale atomistic modelling of phase-change memory materials [J]. Nat. Electron., 2023, 6: 746
101 Du K K, Li Q, Lyu Y B, et al. Control over emissivity of zero-static-power thermal emitters based on phase-changing material GST [J]. Light Sci. Appl., 2017, 6: e16194
102 Qu Y R, Li Q, Cai L, et al. Thermal camouflage based on the phase-changing material GST [J]. Light Sci. Appl., 2018, 7: 26
103 Li C L, Liu D J, Dai D X. Multimode silicon photonics [J]. Nanophotonics, 2019, 8: 227
104 Hosseini P, Wright C D, Bhaskaran H. An optoelectronic framework enabled by low-dimensional phase-change films [J]. Nature, 2014, 511: 206
105 Wang D N, Zhao L, Yu S Y, et al. Non-volatile tunable optics by design: From chalcogenide phase-change materials to device structures [J]. Mater. Today, 2023, 68: 334
106 Siegrist T, Jost P, Volker H, et al. Disorder-induced localization in crystalline phase-change materials [J]. Nat. Mater., 2011, 10: 202
107 Hu C Q, Yang Z B, Bi C B, et al. “All-crystalline” phase transition in nonmetal doped germanium-antimony-tellurium films for high-temperature non-volatile photonic applications [J]. Acta Mater., 2020, 188: 121
108 Matsunaga T, Umetani Y, Yamada N. Structural study of a Ag3.4In3.7Sb76.4Te16.5 quadruple compound utilized for phase-change optical disks [J]. Phys. Rev., 2001, 64B: 184116
109 Matsunaga T, Akola J, Kohara S, et al. From local structure to nanosecond recrystallization dynamics in AgInSbTe phase-change materials [J]. Nat. Mater., 2011, 10: 129
110 Zhang W, Ronneberger I, Zalden P, et al. How fragility makes phase-change data storage robust: Insights from ab initio simulations [J]. Sci. Rep., 2014, 4: 6529
111 Wang X D, Zhou W, Zhang H M, et al. Multiscale simulations of growth-dominated Sb2Te phase-change material for non-volatile photonic applications [J]. npj Comput. Mater., 2023, 9: 136
112 Wang V, Xu N, Liu J C, et al. VASPKIT: A user-friendly interface facilitating high-throughput computing and analysis using VASP code [J]. Comput. Phys. Commun., 2021, 267: 108033
113 IncAnsys. Lumerical FDTD solutions [EB/OL].
114 Zheng Y H, Song W X, Song Z T, et al. A complicated route from disorder to order in antimony-tellurium binary phase change materials [J]. Adv. Sci., 2024, 11: 2301021
115 Belsky A J, Hellenbrandt M, Karen V L, et al. New developments in the Inorganic Crystal Structure Database (ICSD): Accessibility in support of materials research and design [J]. Acta Crystallogr., 2002, 58B: 364
116 Pickard C J, Needs R J. Ab initio random structure searching [J]. J. Phys.: Condens. Matter, 2011, 23: 053201
117 Thompson A P, Aktulga H M, Berger R, et al. LAMMPS—A flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales [J]. Comput. Phys. Commun., 2022, 271: 108171
118 Behler J. First principles neural network potentials for reactive simulations of large molecular and condensed systems [J]. Angew. Chem. Int. Ed., 2017, 56: 12828
119 Xie T, Grossman J C. Crystal graph convolutional neural networks for an accurate and interpretable prediction of material properties [J]. Phys. Rev. Lett., 2018, 120: 145301
120 Behler J. Atom-centered symmetry functions for constructing high-dimensional neural network potentials [J]. J. Chem. Phys., 2011, 134: 074106
121 Wang G J, Sun Y Q, Zhou J, et al. PotentialMind: Graph convolutional machine learning potential for Sb-Te binary compounds of multiple stoichiometries [J]. J. Phys. Chem., 2023, 127C: 24724
122 Bartók A P, Payne M C, Kondor R, et al. Gaussian approximation potentials: The accuracy of quantum mechanics, without the electrons [J]. Phys. Rev. Lett., 2010, 104: 136403
123 Deringer V L, Bartók A P, Bernstein N, et al. Gaussian process regression for materials and molecules [J]. Chem. Rev., 2021, 121: 10073
124 Sosso G C, Miceli G, Caravati S, et al. Neural network interatomic potential for the phase change material GeTe [J]. Phys. Rev., 2012, 85B: 174103
125 Sosso G C, Miceli G, Caravati S, et al. Fast crystallization of the phase change compound GeTe by large-scale molecular dynamics simulations [J]. J. Phys. Chem. Lett., 2013, 4: 4241
126 Gabardi S, Baldi E, Bosoni E, et al. Atomistic simulations of the crystallization and aging of GeTe nanowires [J]. J. Phys. Chem., 2017, 121C: 23827
127 Abou El Kheir O, Bonati L, Parrinello M, et al. Unraveling the crystallization kinetics of the Ge2Sb2Te5 phase change compound with a machine-learned interatomic potential [J]. npj Comput. Mater., 2024, 10: 33
128 Dragoni D, Behler J, Bernasconi M. Mechanism of amorphous phase stabilization in ultrathin films of monoatomic phase change material [J]. Nanoscale, 2021, 13: 16146
129 Shi M C, Li J H, Tao M, et al. Artificial intelligence model for efficient simulation of monatomic phase change material antimony [J]. Mater. Sci. Semicond. Process., 2021, 136: 106146
130 Li K Q, Liu B, Zhou J, et al. Revealing the crystallization dynamics of Sb-Te phase change materials by large-scale simulations [J]. J. Mater. Chem., 2024, 12C: 3897
131 Mocanu F C, Konstantinou K, Lee T H, et al. Modeling the phase-change memory material, Ge2Sb2Te5, with a machine-learned interatomic potential [J]. J. Phys. Chem., 2018, 122B: 8998
132 Mocanu F C, Konstantinou K, Elliott S R. Quench-rate and size-dependent behaviour in glassy Ge2Sb2Te5 models simulated with a machine-learned Gaussian approximation potential [J]. J. Phys., 2020, 53D: 244002
133 Konstantinou K, Mocanu F C, Lee T H, et al. Revealing the intrinsic nature of the mid-gap defects in amorphous Ge2Sb2Te5 [J]. Nat. Commun., 2019, 10: 3065
134 Konstantinou K, Mocanu F C, Akola J, et al. Electric-field-induced annihilation of localized gap defect states in amorphous phase-change memory materials [J]. Acta Mater., 2022, 223: 117465
135 Zhou Y X, Zhang W, Ma E, et al. Device-scale atomistic modelling of phase-change memory materials [J]. Nat. Electron., 2023, 6: 746
136 Mo P H, Li C, Zhao D, et al. Accurate and efficient molecular dynamics based on machine learning and non von Neumann architecture [J]. npj Comput. Mater., 2022, 8: 107
137 Li H, Wang Z, Zou N L, et al. Deep-learning density functional theory Hamiltonian for efficient ab initio electronic-structure calculation [J]. Nat. Comput. Sci., 2022, 2: 367
138 Gong X X, Li H, Zou N L, et al. General framework for E(3)-equivariant neural network representation of density functional theory Hamiltonian [J]. Nat. Commun., 2023, 14: 2848
Outlines

/