Tensile and Fracture Behaviors of Stitched Twill Carbon Fabric Structure Reinforced Aluminum Matrix Composites at Elevated Temperature
Received date: 2023-12-01
Revised date: 2024-06-06
Online published: 2024-06-28
Supported by
National Natural Science Foundation of China(52165018);Jiangxi Provincial Program for Cultivating Academic and Technical Leaders in Key Disciplines(20225BCJ22002)
Three-dimensional fabric-reinforced aluminum matrix composites with high specific strength and modulus, excellent high-temperature resistance, and impact resistance are ideal structural materials for fabricating heat-resistant components in aeronautics and aerospace engineering. However, few studies have explored the mechanical properties and fracture behaviors of these composites in high-temperature environments. This study aims to investigate the quasi-static tensile behaviors and failure mechanisms of a stitched twill carbon fabric-reinforced aluminum matrix composite at an elevated temperature of 400 oC. Based on the fabric structure and yarn microstructure, a mesoscle finite element model was established using representative unit cells at the microsale and mesoscale. The macroscopic mechanical response, damage evolution, and failure mechanism of the composite during the tensile test at an elevated temperature (400 oC) were analyzed through numerical simulations and experiments. Results show that the tested tensile modulus, strength, and fracture strain at 400 oC are 103.20 GPa, 621.60 MPa, and 0.819%, respectively. The calculated tensile stress-strain curve aligns with the experimental curves obtained from high-temperature tensile tests. The composites experience complex thermal stress at elevated temperatures, with the matrix pocket under compressive stress and the yarn structure under tensile stress. In the initial tensile stage, the matrix between interlaced weft/warp yarns is damaged, and local failure zones appear in the stitch and warp yarns; however, the composite exhibits a linear elastic response. As the tensile load increases, the degree of damage in the matrix pocket gradually increases, leading to the emergence of serious matrix damage zones and weft yarn cracking along the twill direction of the fabric. Consequently, the growth rate of tensile stress in the tensile curve declines with increasing tensile strain. In the final stage, the matrix failure zone and yarn fracture zone overlap. The axial fracture of warp yarn, in particular, leads to catastrophic fracture of the composite, resulting in a dramatic drop of the tensile stress. The stitch and weft yarns in the composites exhibit a flat fracture morphology, whereas the fractured warp yarn presents rugged fracture surfaces. A mass of fiber pull-out is observed on the microscopic fracture surface of a warp yarn, accompanied by matrix alloy tearing characteristics.
WU Zhiyong , SHAO Huifan , CAI Changchun , ZENG Min , WANG Zhenjun , WANG Yanli , CHEN Lei , XIONG Bowen . Tensile and Fracture Behaviors of Stitched Twill Carbon Fabric Structure Reinforced Aluminum Matrix Composites at Elevated Temperature[J]. Acta Metall Sin, 2025 , 61(9) : 1387 -1402 . DOI: 10.11900/0412.1961.2023.00469
| [1] | Miracle D B. Metal matrix composites—From science to technological significance [J]. Compos. Sci. Technol., 2005, 65: 2526 |
| [2] | Wenzelburger M, Silber M, Gadow R. Manufacturing of light metal matrix composites by combined thermal spray and semisolid forming process—Summary of the current state of technology [J]. Key Eng. Mater., 2010, 425: 217 |
| [3] | Wang Y, Xu X, Zhao W X, et al. Damage accumulation during high temperature fatigue of Ti/SiCf metal matrix composites under different stress amplitudes [J]. Acta Mater., 2021, 213: 116976 |
| [4] | Ma Z Y, Xiao B L, Zhang J F, et al. Overview of research and development for aluminum matrix composites driven by aerospace equipment demand [J]. Acta Metall. Sin., 2023, 59: 457 |
| 马宗义, 肖伯律, 张峻凡 等. 航天装备牵引下的铝基复合材料研究进展与展望 [J]. 金属学报, 2023, 59: 457 | |
| [5] | Kim B R, Lee H K. Elastoplastic modeling of circular fiber-reinforced ductile matrix composites considering a finite RVE [J]. Int. J. Solids Struct., 2010, 47: 827 |
| [6] | Chen Y L, Ghosh S. Micromechanical analysis of strain rate-dependent deformation and failure in composite microstructures under dynamic loading conditions [J]. Int. J. Plast., 2012, 32-33: 218 |
| [7] | Giugliano D, Barbera D, Chen H F. Effect of fiber cross section geometry on cyclic plastic behavior of continuous fiber reinforced aluminum matrix composites [J]. Eur. J. Mech., 2017, 61A: 35 |
| [8] | Giugliano D, Chen H F. Micromechanical modeling on cyclic plastic behavior of unidirectional fiber reinforced aluminum matrix composites [J]. Eur. J. Mech., 2016, 59A: 155 |
| [9] | Zhu X J, Chen X F, Zhai Z, et al. Micromechanical analysis of interfacial debonding in metal matrix composites subjected to off-axis loading [J]. Fiber Compos., 2013, 3: 53 |
| [10] | Behera N, Murari Pandey K M, Deoghare A B, et al. Modeling & simulation of interface stability in metal matrix composites subjected to off-axis loading using cohesive zone model under elevated temperature: A review [J]. Mater. Today Proc., 2018, 5: 20085 |
| [11] | Eggleston M R, Krempl E. The transverse creep and tensile behaviour of SCS-6/Ti-6Al-4V metal matrix composites at 482 oC [J]. Mech. Compos. Mater. Struct., 1994, 1: 53 |
| [12] | Aghdam M M, Morsali S R, Hosseini S M A, et al. Mechanical behavior of unidirectional SiC/Ti composites subjected to off-axis loading at elevated temperatures [J]. Mater. Sci. Eng., 2017, A688: 244 |
| [13] | Aghdam M M, Morsali S R. Damage initiation and collapse behavior of unidirectional metal matrix composites at elevated temperatures [J]. Comput. Mater. Sci., 2013, 79: 402 |
| [14] | Vassel A. Continuous fibre reinforced titanium and aluminium composites: A comparison [J]. Mater. Sci. Eng., 1999, A263: 305 |
| [15] | Zhang Y H, Yan L L, Miao M H, et al. Microstructure and mechanical properties of z-pinned carbon fiber reinforced aluminum alloy composites [J]. Mater. Des., 2015, 86: 872 |
| [16] | Zhang Y, Wu G, Chen G, et al. Microstructure and mechanical properties of 2D woven Grf/Al composite [J]. Trans. Noferrous Met. Soc. China, 2006, 16(spec. issue3) : S1509 |
| [17] | Ma Y Q, Qi L H, Zheng W Q, et al. Effect of specific pressure on fabrication of 2D-Cf/Al composite by vacuum and pressure infiltration [J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 1915 |
| [18] | Zhou J M, Zheng W Q, Qi L H, et al. Investigation on compressive failure mechanism of 2D cross-ply Cf/Al composites by extrusion directly following vacuum pressure infiltration process [J]. J. Shanghai Univ. (Nat. Sci.), 2014, 20: 75 |
| 周计明, 郑武强, 齐乐华 等. 真空吸渗挤压二维正交铺层复合材料压缩失效机制 [J]. 上海大学学报(自然科学版), 2014, 20: 75 | |
| [19] | Hufenbach W, Gude M, Czulak A. Development of textile-reinforced carbon fibre aluminium composites manufactured with gas pressure infiltration methods [J]. J. Achiev. Mater. Manuf. Eng., 2009, 2: 177 |
| [20] | Yang Q R, Liu J X, Li S K, et al. Fabrication and mechanical properties of Cu-coated woven carbon fibers reinforced aluminum alloy composite [J]. Mater. Des., 2014, 57: 442 |
| [21] | Yang Q R, Liu J X, Li S K, et al. Bending mechanical property and failure mechanisms of woven carbon fiber-reinforced aluminum alloy composite [J]. Rare Met., 2016, 35: 915 |
| [22] | Zhang J J, Liu S C, Zhang Y X, et al. Fabrication of woven carbon fibers reinforced Al-Mg (95-5wt%) matrix composites by an electromagnetic casting process [J]. J. Mater. Process. Technol., 2015, 226: 78 |
| [23] | Zhang J J, Liu S C, Lu Y P, et al. Semisolid-rolling and annealing process of woven carbon fibers reinforced Al-matrix composites [J]. J. Mater. Sci. Technol., 2017, 33: 623 |
| [24] | Lee S K, Byun J H, Hong S H. Effect of fiber geometry on the elastic constants of the plain woven fabric reinforced aluminum matrix composites [J]. Mater. Sci. Eng., 2003, A347: 346 |
| [25] | McWilliams B, Dibelka J, Yen C F. Multi scale modeling and characterization of inelastic deformation mechanisms in continuous fiber and 2D woven fabric reinforced metal matrix composites [J]. Mater. Sci. Eng., 2014, A618: 142 |
| [26] | Sheng G F, Wang Z J, Liu F H, et al. Quasi-static tensile behavior and failure mechanism of laminated puncture CF/Al composites [J]. Acta Aeronaut. Astronaut. Sin., 2021, 42(12): 345 |
| 沈高峰, 王振军, 刘丰华 等. 叠层穿刺CF/Al复合材料准静态拉伸力学行为与失效机制 [J]. 航空学报, 2021, 42(12): 345 | |
| [27] | Feng J P, Yu H, Xu Z F, et al. Bending properties and failure analysis of laminated puncture structural Cf/Al composites [J]. Chin. J. Nonferrous Met., 2020, 30: 2597 |
| 冯景鹏, 余 欢, 徐志锋 等. 叠层穿刺结构Cf/Al复合材料的弯曲性能及失效分析 [J]. 中国有色金属学报, 2020, 30: 2597 | |
| [28] | Gu S, Cai C C, Yu H, et al. Residual compression mechanical properties after low-speed impact for laminated stitched carbon fiber reinforced aluminum matrix composite [J]. J. Aeronaut. Mater., 2022, 42(3): 80 |
| 顾 姝, 蔡长春, 余 欢 等. 叠层缝合碳纤维增强铝基复合材料低速冲击及冲击后剩余压缩力学性能 [J]. 航空材料学报, 2022, 42(3): 80 | |
| [29] | Nie M M, Xu Z F, Yu H, et al. Micro-defects of 3D-Cf/Al composites by vacuum pressure infiltration [J]. Rare Met. Mater. Eng., 2018, 47: 1266 |
| 聂明明, 徐志锋, 余 欢 等. 真空气压浸渗3D-Cf/Al复合材料微观缺陷分析 [J]. 稀有金属材料与工程, 2018, 47: 1266 | |
| [30] | Wang L, Wu J Y, Chen C Y, et al. Progressive failure analysis of 2D woven composites at the meso-micro scale [J]. Compos. Struct., 2017, 178: 395 |
| [31] | Li S G. Boundary conditions for unit cells from periodic microstructures and their implications [J]. Compos. Sci. Technol., 2008, 68: 1962 |
| [32] | Xia Z H, Zhang Y F, Ellyin F. A unified periodical boundary conditions for representative volume elements of composites and applications [J]. Int. J. Solids Struct., 2003, 40: 1907 |
| [33] | Wang Z J, Zhao W H, Wang F, et al. Tensile behavior and failure mechanism of 3D woven fabric reinforced aluminum composites [J]. Int. J. Mech. Sci., 2023, 244: 108043 |
| [34] | Hidnert P. Thermal expansion of aluminum and various important aluminum alloys [J]. J. Franklin Inst., 1925, 199(4): 539 |
| [35] | ABAQUS. Version 6.12 Documentation. Dassault Systemes Simulia Corp. Providence, RI, USA, 2012 |
| [36] | Wang Z J, Wang Z Y, Xiong B W, et al. Micromechanics analysis on the microscopic damage mechanism and mechanical behavior of graphite fiber-reinforced aluminum composites under transverse tension loading [J]. J. Alloys Compd., 2020, 815: 152459 |
| [37] | Xu Q, Qu S X. Irreversible deformation of metal matrix composites: A study via the mechanism-based cohesive zone model [J]. Mech. Mater., 2015, 89: 72 |
| [38] | Lou J H, Yang Y Q, Luo X, et al. The analysis on transverse tensile behavior of SiC/Ti-6Al-4V composites by finite element method [J]. Mater. Des., 2010, 31: 3949 |
| [39] | Rupnowski P, Gentz M, Sutter J K, et al. An evaluation of the elastic properties and thermal expansion coefficients of medium and high modulus graphite fibers [J]. Composites, 2005, 3A: 327 |
| [40] | Kawabata S. Measurement of the transverse mechanical properties of high performance fibres [J]. J. Text. Inst., 1990, 81: 432 |
| [41] | Zhou Y X, Jiang D Z, Xia Y M. Tensile mechanical behavior of T300 and M40J fiber bundles at different strain rate [J]. J. Mater. Sci., 2001, 36: 919 |
| [42] | Kaddour A, Hinton M. Maturity of 3D failure criteria for fiber-reinforced composites: Comparison between theories and experiments: Part B of WWFE-II [J]. J. Compos. Mater., 2013, 47: 925 |
| [43] | He Q Q, Zhou C W, Zhou C. Micro-mechanical model of thermal expansion/contraction for damaged fiber reinforced composites [J]. Acta Mater. Compos. Sin., 2014, 31: 1077 |
| 何乾强, 周储伟, 周 灿. 纤维增强复合材料考虑损伤的温度胀缩细观力学模型 [J]. 复合材料学报, 2014, 31: 1077 | |
| [44] | Schapery R A. Thermal expansion coefficients of composite materials based on energy principles [J]. J. Compos. Mater., 1968, 2: 380 |
| [45] | Yates B, McCalla B A, Sargent J P, et al. The thermal expansion of carbon fibre reinforced plastics: Part 3 The influence of resin type [J]. J. Mater. Sci., 1978, 13: 2217 |
| [46] | Hopkins D A, Chamis C C. A unique set of micromechanics equations for high-temperature metal matrix composites [A]. The First Symposium on Testing Technology of Metal Matrix Composites [C]. Nashvilley: ASTM STP, 1985, 159 |
| [47] | Li D G, Chen G Q, Jiang L T, et al. Effect of thermal cycling on the mechanical properties of Cf/Al composites [J]. Mater. Sci. Eng., 2013, A586: 330 |
| [48] | Zhou L, Zhang P F, Wang Q Z, et al. Multi-scale study on the fracture behavior of hot compression B4C/6061Al composite [J]. Acta Metall. Sin., 2019, 55: 911 |
| 周 丽, 张鹏飞, 王全兆 等. B4C/6061Al复合材料热压缩断裂行为的多尺度研究 [J]. 金属学报, 2019, 55: 911 |
/
| 〈 |
|
〉 |