Strengthening and Plastifying Mechanisms of a Novel High-Strength Low-Density Austenitic Steel

  • LI Fushun ,
  • LIU Zhipeng ,
  • DING Cancan ,
  • HU Bin ,
  • LUO Haiwen
Expand
  • School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
HU Bin, associate professor, Tel: (010)62332911, E-mail: hubin@ustb.edu.cn;
LUO Haiwen, professor, Tel: (010)62332911, E-mail: luohaiwen@ustb.edu.cn

Received date: 2024-03-12

  Revised date: 2024-04-28

  Online published: 2024-04-28

Supported by

Yunnan Key Research and Development Program(202403AA080013);National Natural Science Foundation of China(52233018);National Natural Science Foundation of China(51831002);Beijing Municipal Natural Science Foundation(2242048)

Abstract

High-strength low-density steels are strongly recommended in the automotive industry because they can reduce weight and CO2 emissions without affecting structural safety. In this study, a novel Cr-alloyed austenitic steel with a low density of 6.50 g/cm3 was designed. It was subjected to two types of processing routes. One includes cold rolling with a thickness reduction of 35% followed by aging at 450 oC for 1.5 h (known as 35CR-T). The other route includes cold rolling by 75%, short annealing at 925 oC for 10 s, and final aging at 450 oC for 1.5 h (known as 75CR-AT). Both resultant specimens exhibited excellent tensile properties; the specific yield strength and total elongation of the 35CR-T and 75CR-AT specimens reached 211.5 MPa·cm3/g, 15.6% and 210.0 MPa·cm3/g3, 21.5%, respectively. The microstructure of the former comprises relatively coarse austenite grains with high-density dislocations as the matrix and coarse κ-carbides, whereas that of the latter comprises fine recrystallized austenite grains and more extensive intragranular κ-carbides with a finer size. Consequently, greater dislocation strengthening contributes to the yield strength (YS) of the former, whereas more significant grain refinement and precipitation strengthening contribute to the YS of the latter. Therefore, both specimens have the same YS after considering all strengthening contributors. Moreover, the recrystallized austenite grains in 75CR-AT allow the sequential evolution of the dislocation substructure from planar-slip dislocations, Taylor lattice, and high-density dislocation wall to the microband during tensile deformation. By contrast, the dislocation microbands formed in the austenite grains of 35CR-T specimen suppress the dislocation multiplication and sequential evolution of dislocation substructures, resulting in poorer ductility compared with that of 75CR-AT specimen.

Cite this article

LI Fushun , LIU Zhipeng , DING Cancan , HU Bin , LUO Haiwen . Strengthening and Plastifying Mechanisms of a Novel High-Strength Low-Density Austenitic Steel[J]. Acta Metall Sin, 2025 , 61(6) : 909 -916 . DOI: 10.11900/0412.1961.2024.00077

References

1 Moon J, Ha H Y, Park S J, et al. Effect of Mo and Cr additions on the microstructure, mechanical properties and pitting corrosion resistance of austenitic Fe-30Mn-10.5Al-1.1C lightweight steels [J]. J. Alloys Compd., 2019, 775: 1136
2 Liu C Q, Peng Q C, Xue Z L, et al. Research situation of Fe-Mn-Al-C system low-density high-strength steel [J]. Mater. Rep., 2019, 33: 2572
  刘春泉, 彭其春, 薛正良 等. Fe-Mn-Al-C系列低密度高强钢的研究现状 [J]. 材料导报, 2019, 33: 2572
3 Chen S P, Rana R, Haldar A, et al. Current state of Fe-Mn-Al-C low density steels [J]. Prog. Mater. Sci., 2017, 89: 345
4 Huang Z Y, Hou A L, Jiang Y S, et al. Rietveld refinement, microstructure, mechanical properties and oxidation characteristics of Fe-28Mn-xAl-1C (x = 10 and 12 wt. %) low-density steels [J]. J. Iron Steel Res. Int., 2017, 24: 1190
5 Sutou Y, Kamiya N, Umino R, et al. High-strength Fe-20Mn-Al-C-based alloys with low density [J]. ISIJ Int., 2010, 50: 893
6 Chen X P, Xu Y P, Ren P, et al. Aging hardening response and β-Mn transformation behavior of high carbon high manganese austenitic low-density Fe-30Mn-10Al-2C steel [J]. Mater. Sci. Eng., 2017, A703: 167
7 Kim S H, Kim H, Kim N J. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility [J]. Nature, 2015, 518: 77
8 Yoo J D, Hwang S W, Park K T. Factors influencing the tensile behavior of a Fe-28Mn-9Al-0.8C steel [J]. Mater. Sci. Eng., 2009, A508: 234
9 Frommeyer G, Brüx U. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels [J]. Steel Res. Int., 2006, 77: 627
10 Raabe D, Springer H, Gutierrez-Urrutia I, et al. Alloy design, combinatorial synthesis, and microstructure-property relations for low-density Fe-Mn-Al-C austenitic steels [J]. JOM, 2014, 66: 1845
11 Yang F Q, Song R B, Li Y P, et al. Tensile deformation of low density duplex Fe-Mn-Al-C steel [J]. Mater. Des., 2015, 76: 32
12 Hwang S W, Ji J H, Lee E G, et al. Tensile deformation of a duplex Fe-20Mn-9Al-0.6C steel having the reduced specific weight [J]. Mater. Sci. Eng., 2011, A528: 5196
13 Ha M C, Koo J M, Lee J K, et al. Tensile deformation of a low density Fe-27Mn-12Al-0.8C duplex steel in association with ordered phases at ambient temperature [J]. Mater. Sci. Eng., 2013, A586: 276
14 Ren P, Chen X P, Cao Z X, et al. Synergistic strengthening effect induced ultrahigh yield strength in lightweight Fe-30Mn-11Al-1.2C steel [J]. Mater. Sci. Eng., 2019, A752: 160
15 Yoo J D, Park K T. Microband-induced plasticity in a high Mn-Al-C light steel [J]. Mater. Sci. Eng., 2008, A496: 417
16 Gutierrez-Urrutia I, Raabe D. Influence of Al content and precipitation state on the mechanical behavior of austenitic high-Mn low-density steels [J]. Scr. Mater., 2013, 68: 343
17 Lee J, Park S, Kim H, et al. Simulation of κ-carbide precipitation kinetics in aged low-density Fe-Mn-Al-C steels and its effects on strengthening [J]. Met. Mater. Int., 2018, 24: 702
18 Wu Z Q, Ding H, An X H, et al. Influence of Al content on the strain-hardening behavior of aged low density Fe-Mn-Al-C steels with high Al content [J]. Mater. Sci. Eng., 2015, A639: 187
19 Jiang Z H, Jin J J, Wang X Z, et al. Microstructure and properties of a low-density steel with high strength of 1350 MPa [J]. J. Aeronaut. Mater., 2018, 38(5): 67
  江志华, 金建军, 王晓震 等. 一种1350 MPa级低密度高强度钢的组织性能 [J]. 航空材料学报, 2018, 38(5): 67
20 Seward G G E, Celotto S, Prior D J, et al. In situ SEM-EBSD observations of the hcp to bcc phase transformation in commercially pure titanium [J]. Acta Mater., 2004, 52: 821
21 Humphreys F J. Review Grain and subgrain characterisation by electron backscatter diffraction [J]. J. Mater. Sci., 2001, 36: 3833
22 Wang Y J, Sun J J, Jiang T, et al. A low-alloy high-carbon martensite steel with 2.6?GPa tensile strength and good ductility [J]. Acta Mater., 2018, 158: 247
23 He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029
24 Wang Z W, Lu W J, Zhao H, et al. Ultrastrong lightweight compositionally complex steels via dual-nanoprecipitation [J]. Sci. Adv., 2020, 6: eaba9543
25 Ardell A J. Precipitation hardening [J]. Metall. Trans., 1985, 16A: 2131
26 Zhao Y L, Li Y R, Yeli G M, et al. Anomalous precipitate-size-dependent ductility in multicomponent high-entropy alloys with dense nanoscale precipitates [J]. Acta Mater., 2022, 223: 117480
27 Yang T, Zhao Y L, Tong Y, et al. Multicomponent intermetallic nanoparticles and superb mechanical behaviors of complex alloys [J]. Science, 2018, 362: 933
28 Wang Z W, Lu W J, Zhao H, et al. Formation mechanism of κ- carbides and deformation behavior in Si-alloyed FeMnAlC lightweight steels [J]. Acta Mater., 2020, 198: 258
29 Zhang J L, Raabe D, Tasan C C. Designing duplex, ultrafine-grained Fe-Mn-Al-C steels by tuning phase transformation and recrystallization kinetics [J]. Acta Mater., 2017, 141: 374
30 Yoo J D, Hwang S W, Park K T. Origin of extended tensile ductility of a Fe-28Mn-10Al-1C steel [J]. Metall. Mater. Trans., 2009, 40A: 1520
Outlines

/