Formation of γ′-Denuded Zone and Its Effect on the Mechanical Properties of Inconel 740H Welded Joint After Creep at Different Temperatures
Received date: 2023-06-09
Revised date: 2023-09-15
Online published: 2023-11-01
Supported by
National Key Research and Development Program of China(2016YFC0801904)
In recent years, advanced ultra-supercritical (A-USC) power plants have developed rapidly to increase the thermal efficiency and decrease CO2 emission. Inconel 740H (IN 740H) is one of the Ni-based superalloys with the highest creep strength and good corrosion resistance at elevated temperatures. Owing to its excellent comprehensive properties, IN 740H is considered one of the best candidate materials for superheater and reheater in A-USC power plants. Further improving the mechanical properties of IN 740H welded joint enhances the safety and economic viability of the power plants. In this study, IN 740H tubes were welded by multipass tungsten inert gas hot-wire welding followed by a post weld heat treatment (PWHT) at 800 oC for 5 h. The formation mechanism of the γ′-denuded zone in the IN 740H welded joint after creep at different temperatures was systematically investigated using OM, SEM, and TEM, and its effect on the mechanical properties was analyzed.Results show that the small rod-like γ′ phase only discontinuously precipitates at grain boundaries in the weld metal during PWHT. After creep at different temperatures, an earlier formation of a coarse rod-like γ′ phase and γ′-denuded zone is observed at grain boundaries in the weld metal than in the base metal. The formation of the coarse rod-like γ′ phase at grain boundaries in the base metal results from the discontinuous coarsening of the spherical γ′ phase near grain boundaries, whereas that in the weld metal results from the discontinuous coarsening of the discontinuously precipitated rod-like γ′ phase at the grain boundaries and spherical γ′ phase near the grain boundaries. The discontinuous coarsening of the rod-like γ′ phase and precipitation of M23C6 carbides at grain boundaries lead to the formation of the γ′-denuded zone. Increasing the creep temperature and creep time when the temperature is in the range of 700-800 oC increases the size of the rod-like γ′ phase and width of the γ′-denuded zone at grain boundaries, whereas the number of rod-like γ′ phase initially decreases and then increases with the increase of creep temperature. The spherical γ′ phase in the grain interiors plays a vital role in changing the hardness of the IN 740H welded joint. The discontinuous coarsening of the γ′ phase and the formation of the γ′-denuded zone at the grain boundaries not only decrease the hardness, but also deteriorate the creep rupture strength of the IN 740H welded joint. Controlling the discontinuous coarsening of the rod-like γ′ phase at grain boundaries, suppressing the formation of the γ′-denuded zone, and controlling the growth of the spherical γ′ phase in the grain interiors are necessary to improve the mechanical properties of the IN 740H welded joint.
Key words: Inconel 740H; creep; welded joint; microstructure; γ′ phase
ZHOU Renyuan , ZHU Lihui . Formation of γ′-Denuded Zone and Its Effect on the Mechanical Properties of Inconel 740H Welded Joint After Creep at Different Temperatures[J]. Acta Metall Sin, 2025 , 61(5) : 744 -756 . DOI: 10.11900/0412.1961.2023.00252
| 1 | Singh P, Arora N, Sharma A. Enhancing mechanical properties and creep performance of 304H and Inconel 617 superalloy dissimilar welds for advanced ultra super critical power plants [J]. Int. J. Press. Vessels Pip., 2023, 201: 104882 |
| 2 | Bechetti D H, DuPont J N, de Barbadillo J J, et al. Microstructural evolution of INCONEL? alloy 740H? fusion welds during creep [J]. Metall. Mater. Trans., 2015, 46A: 739 |
| 3 | Viswanathan R, Henry J F, Tanzosh J, et al. U.S. program on materials technology for ultra-supercritical coal power plants [J]. J. Mater. Eng. Perform., 2005, 14: 281 |
| 4 | Kim D M, Kim C, Yang C H, et al. Heat treatment design of Inconel 740H superalloy for microstructure stability and enhanced creep properties [J]. J. Alloys Compd., 2023, 946: 169341 |
| 5 | Evans N D, Maziasz P J, Swindeman R W, et al. Microstructure and phase stability in Inconel alloy 740 during creep [J]. Scr. Mater., 2004, 51: 503 |
| 6 | Shingledecker J, deBarbadillo J J, Gollihue R, et al. Development and performance of INCONEL? alloy 740H? seam-welded piping [J]. Int. J. Press. Vessels Pip., 2023, 202: 104875 |
| 7 | Render M, Santella M L, Chen X, et al. Long-term creep-rupture behavior of alloy Inconel 740/740H [J]. Metall. Mater. Trans., 2021, 52A: 2601 |
| 8 | Shin K Y, Lee J W, Han J M, et al. Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel [J]. Mater. Charact., 2018, 139: 144 |
| 9 | Shingledecker J P, Pharr G M. The role of eta phase formation on the creep strength and ductility of Inconel alloy 740 at 1023 K (750 oC) [J]. Metall. Mater. Trans., 2012, 43A: 1902 |
| 10 | Brittan A M, Mahaffey J, Anderson M, et al. Effect of supercritical CO2 on the performance of 740H fusion welds [J]. Mater. Sci. Eng., 2019, A742: 414 |
| 11 | Guo Y, Li T J, Wang C X, et al. Microstructure and phase precipitate behavior of Inconel 740H during aging [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 1598 |
| 12 | Chong Y, Liu Z D, Godfrey A, et al. Microstructure evolution and mechanical properties of Inconel 740H during aging at 750 oC [J]. Mater. Sci. Eng., 2014, A589: 153 |
| 13 | Yin H F, Gao Y M, Gu Y F. Evolution of the microstructure and microhardness of the welding joint of IN 740H alloy with IN 617 as filler metal [J]. Mater. Charact., 2017, 127: 288 |
| 14 | Bechetti D H, Dupont J N, Watanabe M, et al. Characterization of discontinuous coarsening reaction products in INCONEL? alloy 740H? fusion welds [J]. Metall. Mater. Trans., 2017, 48A: 1727 |
| 15 | Williams D B, Butler E P. Grain boundary discontinuous precipitation reactions [J]. Int. Met. Rev., 1981, 26: 153 |
| 16 | Porter D A, Easterling K E. Phase Transformations in Metals and Alloys [M]. 2nd Ed., Boca Raton: CRC Press, 1992: 322 |
| 17 | Xie X S, Zhao S Q, Dong J X, et al. Structural stability and improvement of Inconel alloy 740 for ultra supercritical power plants [J]. J. Chin. Soc. Power Eng., 2011, 31: 638 |
| 谢锡善, 赵双群, 董建新 等. 超超临界电站用Inconel 740镍基合金的组织稳定性及其改型研究 [J]. 动力工程学报, 2011, 31: 638 | |
| 18 | Skleni?ka V, Kucha?ová K, Svoboda M, et al. Creep behaviour of IN 740 alloy after HAZ thermal cycle simulations [J]. Int. J. Press. Vessels Pip., 2019, 178: 104000 |
| 19 | Gronsky R, Thomas G. Discontinuous coarsening of spinodally decomposed Cu-Ni-Fe alloys [J]. Acta Metall., 1975, 23: 1163 |
| 20 | Fournelle R A. Discontinuous coarsening of lamellar cellular precipitate in an austenitic Fe-30 wt.%Ni-6 wt.%Ti alloy-I. Morphology [J]. Acta Metall., 1979, 27: 1135 |
| 21 | Manna I, Pabi S K, Gust W. Discontinuous reactions in solids [J]. Int. Mater. Rev., 2001, 46: 53 |
| 22 | Fedoseeva A, Nikitin I, Dudova N, et al. Coarsening of Laves phase and creep behaviour of a Re-containing 10%Cr-3%Co-3%W steel [J]. Mater. Sci. Eng., 2021, A812: 141137 |
| 23 | Guo Z K, Jie J C, Liu S C, et al. Suppression of discontinuous precipitation in age-hardening Cu-15Ni-8Sn alloy by addition of V [J]. J. Alloys Compd., 2020, 813: 152229 |
| 24 | Fang J Y C, Liu W H, Luan J H, et al. Competition between continuous and discontinuous precipitation in L12-strengthened high-entropy alloys [J]. Intermetallics, 2022, 149: 107655 |
| 25 | Perez M, Dumont M, Acevedo-Reyes D. Implementation of classical nucleation and growth theories for precipitation [J]. Acta Mater., 2008, 56: 2119 |
| 26 | Funkenbusch A W. Discontinuous γ′ coarsening in a Ni-Al-Mo base superalloy [J]. Metall. Trans., 1983, 14A: 1283 |
| 27 | Manna I, Jha J N, Pabi S K. Kinetics of discontinuous precipitation in a Zn-2.5at%Cu alloy [J]. J. Mater. Sci., 1995, 30: 1449 |
| 28 | Rao K B, Seetharaman V, Mannan S L, et al. Precipitation, deformation and fracture behaviour of a thermomechanically processed Nimonic PE 16 superalloy [J]. J. Nucl. Mater., 1981, 102: 7 |
| 29 | Partridge A, Noble F W, Tatlock G J. The effects of long-term ageing on Nimonic PE16 [J]. J. Nucl. Mater., 1992, 186: 100 |
| 30 | Olalla V C, Bliznuk V, Sanchez N, et al. Analysis of the strengthening mechanisms in pipeline steels as a function of the hot rolling parameters [J]. Mater. Sci. Eng., 2014, A604: 46 |
/
| 〈 |
|
〉 |